- [21] Decomposition of Chromite in Refractory Magnesite-Chrome Bricks in Lime-Burning-Kilns at 950 degree C. Berichte der Deutschen Keramischen Gesellschaft, 1977, 54 (06): : 188 - 189
- [23] REACTIONS OF MAGNESITE-CHROME REFRACTORIES WITH COAL-GASIFICATION SLAGS AMERICAN CERAMIC SOCIETY BULLETIN, 1977, 56 (03): : 369 - 369
- [25] HIGH TEMPERATURE THERMAL EXPANSION OF MAGNESITE AND CHROME-MAGNESITE BRICKS REVUE INTERNATIONALE DES HAUTES TEMPERATURES ET DES REFRACTAIRES, 1968, 5 (01): : 63 - &
- [26] The Influence of Indian Concentrate Chrome Ore on Top Quality Magnesite-chrome Brick for RH Degasser FUNDAMENTAL OF CHEMICAL ENGINEERING, PTS 1-3, 2011, 233-235 : 2654 - 2659
- [27] CHROME-MAGNESITE REFRACTORY CORROSION WITH OLIVINE SLAG OF HIGH CUPROUS OXIDE CONTENT INTERNATIONAL PEIRCE-SMITH CONVERTING CENTENNIAL, 2009, : 71 - +
- [29] INVESTIGATIONS ON PRECAUTIONS AGAINST EXPANSION IN MAGNESITE-CHROME BRICK LININGS FOR ROTARY CEMENT KILNS ZEMENT-KALK-GIPS, 1977, 30 (01): : 19 - 25