Cavitation erosion behavior of nickel-aluminum bronze weldment

被引:0
|
作者
李小亚
闫永贵
许振明
李建国
机构
[1] China
[2] College of Materials Science and Engineering
[3] Hebei University of Science and Technology
[4] Luoyang Ship Materials Research Institute
[5] Qingdao 266071
[6] Qingdao Branch
[7] Shanghai 200030
[8] Shijiazhuang 050054
[9] State Key Laboratory for Marine Corrosion and Protection
[10] State Key Laboratory of Metal Matrix Composites
[11] State Key Laboratory of Metal Matrix Composites Shanghai Jiaotong University
关键词
NAB; weldment; tungsten inert gas welding(TIG); cavitation erosion;
D O I
暂无
中图分类号
TG172.9 [其他腐蚀];
学科分类号
080503 ;
摘要
Cavitation erosion behavior of nickel-aluminum bronze(NAB) weldment in 3.5% NaCl aqueous solution was studied by magnetostrictive vibratory device for cavitation erosion. The results show that cavitation erosion resistance of the weld zone(WZ) of the weldment is superior to that of the base metal. SEM observation of eroded specimens reveals that the phases undergoing selective attack by the stress of cavitation erosion at the early stage of cavitation erosion are: martensite in the WZ, α phase in the heat-affected zone(HAZ) and eutectoidal phase in the base metal; the microcracks causing cavitation damage initiate at the phase boundaries.
引用
收藏
页码:1317 / 1324
页数:8
相关论文
共 50 条
  • [31] A new nickel-aluminum bronze alloy with low magnetic permeability
    P. Wenschot
    [J]. Metallurgical and Materials Transactions A, 1997, 28 : 689 - 697
  • [32] On cavitation erosion behavior of friction stir processed surface of cast nickel aluminium bronze
    Thapliyal, Shivraman
    Dwivedi, Dheerendra Kumar
    [J]. WEAR, 2017, 376 : 1030 - 1042
  • [33] Defects studies of nickel aluminum bronze subjected to cavitation
    Siemek, K.
    Eseev, M. K.
    Horodek, P.
    Kobets, A. G.
    Kuziv, I., V
    [J]. APPLIED SURFACE SCIENCE, 2021, 546
  • [34] CAVITATION EROSION OF LASER QUENCHED FE-ALUMINUM BRONZE
    GABRIEL, MW
    PREECE, CM
    STAUDINGER, A
    DRAPER, CW
    [J]. IEEE JOURNAL OF QUANTUM ELECTRONICS, 1981, 17 (10) : 2000 - 2003
  • [35] Cavitation Erosion Corrosion Behaviour of Manganese-nickel-aluminum Bronze in Comparison with Manganese-brass
    Yu, Hong
    Zheng, Yugui
    Yao, Zhiming
    [J]. JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2009, 25 (06) : 758 - 766
  • [36] Effect of laser surface melting on microstructure evolution and cavitation behavior of nickel aluminum bronze
    Zeng, Si-qi
    Tian, Jing-jing
    Hu, Shu-bing
    Xiao, Ming
    Peng, Bo
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2023, 33 (07) : 2090 - 2109
  • [38] Laser processing of nickel-aluminum bronze for improved surface corrosion properties
    Cottam, R.
    Barry, T.
    McDonald, D.
    Li, H.
    Edwards, D.
    Majumdar, A.
    Dominguez, J.
    Wang, J.
    Brandt, M.
    [J]. JOURNAL OF LASER APPLICATIONS, 2013, 25 (03)
  • [39] THE MORPHOLOGY, CRYSTALLOGRAPHY, AND CHEMISTRY OF PHASES IN AS-CAST NICKEL-ALUMINUM BRONZE
    HASAN, F
    JAHANAFROOZ, A
    LORIMER, GW
    RIDLEY, N
    [J]. METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1982, 13 (08): : 1337 - 1345
  • [40] Improving Corrosion Resistance of a Nickel-Aluminum Bronze Alloy via Nickel Ion Implantation
    Qin, Zhenbo
    Wu, Zhong
    Zen, Xiangsen
    Luo, Qin
    Liu, Lei
    Lu, Weijie
    Hu, Wenbin
    [J]. CORROSION, 2016, 72 (10) : 1269 - 1280