Determination of mixed-mode interfacial fracture toughness for thermal barrier coatings

被引:0
|
作者
DENG HongXia 1
2 Beijing Institute of Aeronautical Materials
机构
基金
中国国家自然科学基金;
关键词
thermal barrier coating; multilayer; mixed-mode; interface; fracture toughness; energy release rate;
D O I
暂无
中图分类号
O346.1 [断裂理论];
学科分类号
摘要
In this work,a test method was developed to determine the interfacial fracture toughness of the air plasma sprayed (APS) thermal barrier coatings (TBCs) over a wide range of mode mixities.For this mixed-mode test method,the analytical expressions for the energy release rate and stress intensity factors were derived based on the energy theory and the concept of "equivalence".The fidelity of these expressions was affirmed by selected finite element analysis.The experimental results showed that the critical energy release rate increased with the increase of the positive mode mixity,which was mainly due to the increase in contact/friction effect and plastic work dissipation with increasing shear mode loading.Furthermore,an elliptical interfacial failure criterion in terms of the stress intensity factors was proposed.The agreement between the experimental results in the literature and those in our work indicated that our test method and the corresponding analytical solutions can well determine the interfacial fracture toughness of the TBCs over a wide range of mode mixities.
引用
收藏
页码:618 / 624
页数:7
相关论文
共 50 条
  • [31] Fracture behavior under mixed-mode loading of ceramic plasma-sprayed thermal barrier coatings at ambient and elevated temperatures
    Choi, SR
    Zhu, D
    Miller, RA
    ENGINEERING FRACTURE MECHANICS, 2005, 72 (13) : 2144 - 2158
  • [32] Interfacial mixed-mode fracture characterization of adhesively bonded joints
    Choupani, Naghdali
    INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2008, 28 (06) : 267 - 282
  • [33] Interfacial mixed-mode fracture characterization of adhesively bonded joints
    Choupani, Naghdali
    International Journal of Adhesion and Adhesives, 2008, 28 (06): : 267 - 282
  • [34] Measurements of the interfacial fracture energy of thermal barrier coatings
    Shaw, LL
    Barber, B
    Jordan, EH
    Gell, M
    SCRIPTA MATERIALIA, 1998, 39 (10) : 1427 - 1434
  • [35] Analysis of a "barb test" for measuring the mixed-mode delamination toughness of coatings
    Liu, Yu-Fu
    Kagawa, Y.
    Evans, A. G.
    ACTA MATERIALIA, 2008, 56 (01) : 43 - 49
  • [36] ASSESSMENT OF MIXED-MODE FRACTURE-TOUGHNESS TESTING METHODS FOR ROCK
    LIM, IL
    JOHNSTON, IW
    CHOI, SK
    INTERNATIONAL JOURNAL OF ROCK MECHANICS AND MINING SCIENCES & GEOMECHANICS ABSTRACTS, 1994, 31 (03) : 265 - 272
  • [37] Adhesive thickness effects on the mixed-mode fracture toughness of bonded joints
    Oliveira, J. J. G.
    Campilho, R. D. S. G.
    Silva, F. J. G.
    Marques, E. A. S.
    Machado, J. J. M.
    da Silva, L. F. M.
    JOURNAL OF ADHESION, 2020, 96 (1-4): : 300 - 320
  • [38] Fracture mechanical characterisation of mixed-mode toughness of thermoplast/glass interfaces
    Dollhofer, J
    Beckert, W
    Lauke, B
    Schneider, K
    COMPUTATIONAL MATERIALS SCIENCE, 2000, 19 (1-4) : 223 - 228
  • [39] COMBINED STRESS HYPOTHESIS FOR MIXED-MODE FRACTURE-TOUGHNESS CRITERION
    YATOMI, C
    FUJII, K
    NAKAGAWA, K
    ENGINEERING FRACTURE MECHANICS, 1989, 32 (06) : 881 - 888
  • [40] DETERMINATION OF IN-SITU MIXED-MODE FRACTURE PARAMETERS
    ZHAO, XL
    INTERNATIONAL JOURNAL OF FRACTURE, 1995, 70 (03) : R63 - R68