Longitudinal surface cracks on continuous casting slabs of P and Cu containing container steel

被引:0
|
作者
Xinhua Wang
机构
关键词
container steel; CC slab; longitudinal surface crack; mold; hot ductility;
D O I
暂无
中图分类号
TG142 [钢];
学科分类号
摘要
The fact that the amount of the mold flux components differs at different locations on the cracking surface indicates that the longitudinal surface cracks are initially formed in the mold and are enlarged in the secondary cooling zone. Based on the hot ductility measurement of two typical container used steels, it is known that the steels are in severe embrittlement state in the temperature range of 825-775℃. By means of increasing Cr/Ni plating thickness on the upper part of the mold, reducing mold heat flux, adopting new secondary cooling pattern, etc., the occurrence of the surface longitudinal cracks on the steel CC (continuous casting) slabs has been significantly reduced.
引用
收藏
页码:16 / 19
页数:4
相关论文
共 50 条
  • [31] A thermomechanical modelling of continuous casting to master steel slabs internal soundness and surface quality
    Triolet, N.
    Bobadilla, M.
    Bellet, M.
    Avedian, L.
    Mabelly, P.
    REVUE DE METALLURGIE-CAHIERS D INFORMATIONS TECHNIQUES, 2005, 102 (05): : 343 - 353
  • [32] CAUSES OF OCCURRENCE OF INTERNAL AND SURFACE DEFECTS AT CONTINUOUS CASTING OF STEEL SLABS AND POSSIBILITIES OF THEIR REMOVAL
    Masarik, Milos
    Camek, Libor
    Duda, Jiri
    METAL 2014: 23RD INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2014, : 105 - 110
  • [33] NATURE OF LONGITUDINAL SURFACE CRACKS IN CONTINUOUSLY CAST SLABS
    MOISEEV, BP
    ESAULOV, VS
    NIKOLAEV, VA
    EMELYANOV, VV
    GUBIN, NI
    STEEL IN THE USSR, 1986, 16 (12): : 590 - 593
  • [34] Mechanism of longitudinal midface interdendritic surface crack in continuous casting of steel
    El-Bealy, MO
    84TH STEELMAKING CONFERENCE PROCEEDINGS, 2001, 84 : 377 - 390
  • [35] Study for the Initiation Locations of Longitudinal Surface Cracks on Beam Blank in the Mould of Continuous Casting
    Chen, Wei
    Yu, Xingwang
    Chen, Ying
    Wang, Baoxiang
    TMS 2017 146TH ANNUAL MEETING & EXHIBITION SUPPLEMENTAL PROCEEDINGS, 2017, : 511 - 520
  • [36] INFLUENCE OF THE MOLTEN POWDER POOL ON THE LONGITUDINAL SURFACE CRACKS IN CONTINUOUSLY CAST STEEL SLABS.
    Nakano, Taketo
    Fuji, Masao
    Nagano, Kyoichi
    Mizoguchi, Syozo
    Yamamoto, Toshiki
    Asano, Keisuke
    Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan, 1981, 67 (08): : 1210 - 1219
  • [37] FACTORS AFFECTING THE FORMATION OF SHELL AND LONGITUDINAL CRACKS IN MOLD DURING HIGH-SPEED CONTINUOUS-CASTING OF SLABS
    NAKATO, H
    OZAWA, M
    KINOSHITA, K
    HABU, Y
    EMI, T
    TRANSACTIONS OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1984, 24 (11) : 957 - 965
  • [38] Transient flow and temperature transport in continuous casting of steel slabs
    Zhao, B
    Thomas, BG
    Vanka, SP
    O'Malley, RJ
    JOURNAL OF HEAT TRANSFER-TRANSACTIONS OF THE ASME, 2005, 127 (08): : 807 - 807
  • [39] Eliminating surface transverse cracks in the novel vertical bending continuous casting of pure aluminum 1070 thin slabs
    Mao, Qijia
    Hua, Fuan
    Wu, Zhuohuang
    Fu, Yuxiao
    Jia, Guanglin
    Yuan, Guo
    Wang, Guodong
    SCIENTIFIC REPORTS, 2025, 15 (01):
  • [40] Modeling of the solidification process in a continuous casting installation for steel slabs
    Gonzalez, M
    Goldschmit, MB
    Assanelli, AP
    Berdaguer, EF
    Dvorkin, EN
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2003, 34 (04): : 455 - 473