Longitudinal surface cracks on continuous casting slabs of P and Cu containing container steel

被引:0
|
作者
Xinhua Wang
机构
关键词
container steel; CC slab; longitudinal surface crack; mold; hot ductility;
D O I
暂无
中图分类号
TG142 [钢];
学科分类号
摘要
The fact that the amount of the mold flux components differs at different locations on the cracking surface indicates that the longitudinal surface cracks are initially formed in the mold and are enlarged in the secondary cooling zone. Based on the hot ductility measurement of two typical container used steels, it is known that the steels are in severe embrittlement state in the temperature range of 825-775℃. By means of increasing Cr/Ni plating thickness on the upper part of the mold, reducing mold heat flux, adopting new secondary cooling pattern, etc., the occurrence of the surface longitudinal cracks on the steel CC (continuous casting) slabs has been significantly reduced.
引用
收藏
页码:16 / 19
页数:4
相关论文
共 50 条
  • [1] Longitudinal surface cracks on continuous casting slabs of P and Cu containing container steel
    Wang, XH
    Zhu, ZY
    Zhang, L
    Xu, GD
    JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 2003, 10 (04): : 16 - 19
  • [2] Control of Surface Longitudinal Cracks During the Steel Continuous Casting
    Wang, Fengkang
    Zeng, Jie
    Wang, Wanlin
    TMS 2024 153RD ANNUAL MEETING & EXHIBITION: SUPPLEMENTAL PROCEEDINGS, 2024, : 1031 - 1039
  • [3] Investigation on longitudinal surface cracks of CC slabs for container
    Zhang, Li
    Xu, Guodong
    Wang, Xinhua
    Zhu, Zhiyuan
    Kang T'ieh/Iron and Steel (Peking), 2002, 37 (01): : 19 - 21
  • [4] Investigation of longitudinal surface cracks in a continuous casting slab of high-carbon steel
    GUO Liangliang
    XU Zhengqi
    SHI Jianbin
    HUANG Zongze
    Baosteel Technical Research, 2014, 8 (02) : 19 - 25
  • [5] CONTINUOUS CASTING OF STEEL SLABS
    PRECHT, H
    PRESTON, T
    SAE TRANSACTIONS, 1968, 77 : 77 - &
  • [6] Behaviour of longitudinal surface cracks in the hot rolling of steel slabs
    Ervasti, E
    Ståhlberg, U
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 1999, 94 (2-3) : 141 - 150
  • [7] Behaviour of longitudinal surface cracks in the hot rolling of steel slabs
    Ervasti, Esa
    Ståhlberg, Ulf
    Journal of Materials Processing Technology, 1999, 94 (02): : 141 - 150
  • [8] Steel cleanliness in continuous casting slabs
    Ferro, L
    Petroni, J
    Madias, J
    Cicutti, C
    Dalmaso, D
    79TH STEELMAKING CONFERENCE PROCEEDINGS, 1996, 79 : 497 - 502
  • [9] Longitudinal surface cracks of thin slabs
    Yan-hui Sun
    You-jin Ni
    Hai-tao Wang
    Zhong-bo Xu
    Kai-ke Cai
    International Journal of Minerals, Metallurgy, and Materials, 2010, 17 : 159 - 166
  • [10] Longitudinal surface cracks of thin slabs
    Sun, Yan-hui
    Ni, You-jin
    Wang, Hai-tao
    Xu, Zhong-bo
    Cai, Kai-ke
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2010, 17 (02) : 159 - 166