Influence of Lamellar Direction in Pearlitic Steel Wire on Mechanical Properties and Microstructure Evolution

被引:0
|
作者
Tian-zhang ZHAO [1 ]
Guang-liang ZHANG [2 ]
Shi-hong ZHANG [3 ]
Ling-yun ZHANG [1 ]
机构
[1] Key Laboratory of Fundamental Science for National Defence of Aeronautical Digital Manufacturing Process,Shenyang Aerospace University
[2] School of Mechanical Engineering,Taizhou University
[3] Institute of Metal Research,Chinese Academy of Sciences
基金
中国国家自然科学基金;
关键词
pearlitic lamellae; steel wire; drawing; mechanical property; representative volume element;
D O I
暂无
中图分类号
TG356.45 [];
学科分类号
080201 ; 080503 ;
摘要
During cold drawing of pearlitic steel wire,the lamellar structure becomes gradually aligned with the drawing axis,which contributes to the ultra-high strength.A direct simulation about the mechanical behaviors and microstructural evolution of pearlitic lamellae was presented.A representative volume element( RVE) containing one pearlitic colony was established based on the real transmission electron microscope( TEM) observation.The deformation of pearlitic colony during tension,shear and wire drawing were successfully simulated.The numerical results show that this metallographic texture leads to a strong anisotropy.The colony has higher yielding stress when the lamellar direction is parallel and perpendicular to the tensile direction.The lamellar evolution is strongly dependent on the initial direction and deformation mode.The formation of typical period shear bands is analyzed.In the wire drawing,the pearlitic colony at the sub-surface experiences a complex strain path: rotation,stretching along the die surface,and rotation back.
引用
收藏
页码:1290 / 1296
页数:7
相关论文
共 50 条
  • [21] Microstructure evolution and mechanical hardening of hypereutectoid pearlitic steel during cold rolling
    Zhang, X.
    Wang, C.X.
    Liu, X.M.
    Shi, Q.N.
    Acta Metallurgica Sinica (English Letters), 2007, 20 (04) : 287 - 292
  • [22] Microstructure evolution in pearlitic steels during wire drawing
    Zelin, M
    ACTA MATERIALIA, 2002, 50 (17) : 4431 - 4447
  • [24] Quantitative characterization of lamellar microstructure in ultra-high strength pearlitic steel wire during cold drawing
    Wu, Yong-Gang
    Zhou, Zheng
    Yang, Ben
    Wang, Li-Xin
    Liu, Qing
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2015, 36 (06): : 159 - 163
  • [26] Evaluation of fatigue limit characteristics of lamellar pearlitic steel in consideration of microstructure
    Hamada S.
    Sakoda Y.
    Sasaki D.
    Ueda M.
    Noguchi H.
    Zairyo/Journal of the Society of Materials Science, Japan, 2011, 60 (09) : 790 - 795
  • [27] Influence of steel microstructure on their mechanical properties
    Galtier, André
    Bouaziz, Olivier
    Lambert, Astride
    2002, EDP Sciences, 17 Avenue du Hoggar - BP 112, Les Ulis Cedex A, F-91944, France (03):
  • [28] Bridging microstructure and crystallography with the micromechanics of cleavage fracture in a lamellar pearlitic steel
    Barik, Rakesh Kumar
    Ghosh, Abhijit
    Sk, Md Basiruddin
    Biswal, Sankalp
    Dutta, Amlan
    Chakrabarti, Debalay
    ACTA MATERIALIA, 2021, 214
  • [29] Overview of pearlitic rail steel: Accelerated cooling, quenching, microstructure and mechanical properties
    Sahay, Satyam S.
    Mohapatra, Goutam
    Totten, George E.
    Journal of ASTM International, 2009, 6 (07):
  • [30] Influence of hybrid plastic deformation on the microstructure and mechanical properties of carbon-steel wire
    Chukin M.V.
    Polyakova M.A.
    Gulin A.E.
    Steel in Translation, 2016, 46 (8) : 548 - 551