Compression behavior of magnesium-lithium alloy at room temperature

被引:1
|
作者
王聪
李卓群
徐永波
韩恩厚
机构
[1] Environmental Corrosion Center Institute of Metal Research
[2] Chinese Academy of Sciences
[3] Shenyang 110016
[4] China
[5] Shenyang National Laboratory for Materials Science
基金
中国国家自然科学基金;
关键词
compression; LA40 magnesium alloy; twinning; PLC effect;
D O I
暂无
中图分类号
TG115 [金属的分析试验(金属材料试验)];
学科分类号
摘要
The mechanical properties of LA40 magnesium alloy were investigated under compression at room temperature. In the applied strain rate range from 1.33×10-4s-1 to 6.66×10-4s-1,this alloy shows positive strain rate sensitivity (SRS). Most importantly, the Portevin-Le Chatelier(PLC) effect which is an interesting and dominant feature in tensile tests disappears under compressive conditions. Only one twinning system is activated under tensile deformation, while at least two twinning modes are operative during compression. Additionally, the effect of dynamic strain aging (DSA), and the main mechanism for the onset of PLC phenomenon during tension, will be weakened because the strengthened obstructing influence of twins on solute atoms and the disappearance of PLC is inevitable.
引用
收藏
页码:1721 / 1724
页数:4
相关论文
共 50 条
  • [31] Electrodeposition of gold on magnesium-lithium alloys
    Sharma, A.K.
    Metal Finishing, 1988, 86 (12) : 33 - 34
  • [32] SOLUBILITY OF ZIRCONIUM IN MAGNESIUM-LITHIUM ALLOYS
    DEMAINE, PD
    FOWLER, GA
    JOURNAL OF THE INSTITUTE OF METALS, 1963, 91 (11): : 380 - &
  • [33] Solubility of iron in magnesium-lithium melts
    Schwerdtfeger, K
    Mutale, CT
    Ditze, A
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2002, 33 (06): : 929 - 930
  • [34] A new approach to improving the macrosegregation in zirconium-containing magnesium-lithium alloy
    Wang, L.
    Guan, H.
    Wu, G.
    Pan, Y.
    Sun, S.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2018, 49 (09) : 1125 - 1134
  • [35] Fabrication of Nanocrystalline High-Strength Magnesium-Lithium Alloy by Rotary Swaging
    Chen, Xin
    Liu, Chuming
    Jiang, Shunong
    Chen, Zhiyong
    Wan, Yingchun
    ADVANCED ENGINEERING MATERIALS, 2022, 24 (01)
  • [36] Formability of Magnesium-Lithium Alloy Sheet by Multi-stage Deep Drawing
    Harada, Yasunori
    Yamamoto, Atsushi
    Goto, Takayuki
    Nakamura, Eiji
    THERMEC 2011, PTS 1-4, 2012, 706-709 : 1164 - +
  • [37] Microstructure and mechanical properties of magnesium-lithium alloy prepared by friction stir processing
    Che, Qian-Ying
    Wang, Kuai-She
    Wang, Wen
    Huang, Li-Ying
    Li, Tian-Qi
    Xi, Xiao-Peng
    Peng, Pai
    Qiao, Ke
    RARE METALS, 2021, 40 (09) : 2552 - 2559
  • [38] ELASTIC CONSTANTS OF MAGNESIUM-LITHIUM ALLOYS
    WAZZAN, AR
    ROBINSON, LB
    PHYSICAL REVIEW, 1967, 155 (03): : 586 - +
  • [39] Tailoring the degradation rate of magnesium-lithium alloy with alloying elements of gadolinium and nickel
    Pang, Mengyao
    Zhong, Tao
    Jin, Siyuan
    Ma, Xiaochun
    Wu, Ruizhi
    Hou, Legan
    Tashlykova-Bushkevich, Iya I.
    Krit, Boris
    Zhang, Jinghuai
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 976
  • [40] Recent progress in magnesium-lithium alloys
    Wu, R.
    Yan, Y.
    Wang, G.
    Murr, L. E.
    Han, W.
    Zhang, Z.
    Zhang, M.
    INTERNATIONAL MATERIALS REVIEWS, 2015, 60 (02) : 65 - 100