共 50 条
- [11] Fatigue crack initiation in Ti-5Al-4Sn-2Zr-1Mo-0.7Nd-0.25Si high temperature titanium alloy International Journal of Fatigue, 1997, 19 (Suppl 1):
- [13] Effect of microstructure on fracture characteristics of Ti-6Al-2Sn-2Mo-2Zr-2Cr-Si alloy TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2001, 87 (01): : 55 - 62
- [17] Nd-rich phase particles in as-forged Ti-5Al-4Sn-2Zr-1Mo-0.25Si-1Nd alloy Acta Metal Sin, 4 (261-264):
- [18] Microstructure of second-phase particles in Ti-5Al-4Sn-2Zr-1Mo-0.25Si-1Nd alloy METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1997, 28 (08): : 1595 - 1605
- [19] Microstructure of second-phase particles in Ti-5Al-4Sn-2Zr-1Mo-0.25Si-1Nd alloy Metallurgical and Materials Transactions A, 1997, 28 : 1595 - 1605
- [20] EMBRITTLEMENT OF TI-6AL-2SN-4ZR-2MO ALLOY BY ALPHA2-PHASE PRECIPITATION METALLURGICAL TRANSACTIONS, 1974, 5 (08): : 1949 - 1951