摘要
Porous anodic oxide films were fabricated galvanostatically on titanium alloy Ti-10V-2Fe-3Al in ammonium tartrate solution with different anodizing time.Scanning electron microscopy(SEM) and field emission scanning electron microscopy(FE-SEM) were used to investigate the morphology evolution of the anodic oxide film.It is shown that above the breakdown voltage,oxygen is generated with the occurrence of drums morphology.These drums grow and extrude,which yields the compression stress.Subsequently,microcracks are generated.With continuous anodizing,porous oxides form at the microcracks.Those oxides grow and connect to each other,finally replace the microcrack morphology.The depth profile of the anodic oxide film formed at 1 800 s was examined by Auger electron spectroscopy(AES).It is found that the film is divided into three layers according to the molar fractions of elements.The outer layer is incorporated by carbon,which may come from electrolyte solution.The thickness of the outer layer is approximately 0.2-0.3 μm.The molar fractions of elements in the intermediate layer are extraordinarily stable,while those in the inner layer vary significantly with sputtering depth.The thicknesses of the intermediate layer and the inner layer are 2 μm and 1.0-1.5 μm,respectively.Moreover,the growth mechanism of porous anodic oxide films in neutral tartrate solution was proposed.
引用
收藏
页码:6 / 15
页数:10
相关论文
共 50 条
  • [31] On the fatigue crack growth behavior of Ti-10V-2Fe-3Al in gaseous hydrogen
    Harris, Zachary D.
    Ronevich, Joseph A.
    Stavila, Vitalie
    Somerday, Brian P.
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (51) : 27929 - 27940
  • [32] Fatigue and Fracture Evaluations in Ti-10V-2Fe-3Al (Ti 10-2-3)
    Bache, Martin
    METALS, 2023, 13 (12)
  • [33] Mechanical properties of beta solution treated and aged Ti-10V-2Fe-3Al alloy
    Sugiura, Y
    Nakamura, K
    Hamai, S
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 2000, 86 (03): : 181 - 188
  • [34] STRUCTURE-PROPERTY RELATIONSHIPS TI-10V-2FE-3AL
    COSTA, JE
    HANDERHAN, K
    ROSENBERG, HW
    JOURNAL OF METALS, 1980, 32 (12): : 37 - 37
  • [35] HEATING EFFECTS DURING FRACTURE IN TI-10V-2FE-3AL
    BRYANT, JD
    WILSDORF, HGF
    JOURNAL OF METALS, 1985, 37 (11): : A70 - A70
  • [36] Superelasticity in Ti-10V-2Fe-3Al alloys with nitrogen addition
    Furuhara, T.
    Annaka, S.
    Tomio, Y.
    Maki, T.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 438 : 825 - 829
  • [37] FATIGUE CRACK-PROPAGATION IN TI-10V-2FE-3AL
    DUERIG, TW
    WILLIAMS, JC
    JOURNAL OF METALS, 1980, 32 (08): : 41 - 41
  • [38] The Study on Quench Transformation in Ti-10V-2Fe-3Al Alloy
    张少卿
    陶春虎
    JournalofMaterialsScience&Technology, 1989, (05) : 351 - 356
  • [39] The powder sintering and isothermal forging of Ti-10V-2Fe-3Al
    Guo, Hongzhen
    Zhao, Zhanglong
    Duan, Chunyan
    Yao, Zekun
    JOM, 2008, 60 (11) : 47 - 49
  • [40] Ti-10V-2Fe-3Al合金的再结晶
    胡大为
    潘雅琴
    吴云书
    金属学报 , 1987, (03) : 240 - 242