Microstructural characteristics and erosion resistance of laser cladding Stellite 6 alloy on an 1Cr11Ni2W2MoV steel surface

被引:1
|
作者
Chen, Meng [1 ]
An, Yinmin [1 ]
Wang, Quanbo [2 ]
Xu, Youwei [2 ]
Shi, Yu [2 ]
机构
[1] China Aviat Guizhou Honglin Aviat Power Control Te, Guiyang 550000, Peoples R China
[2] Lanzhou Univ Technol, State Key Lab Adv Proc & Recycling Nonferrous Met, Lanzhou 730050, Peoples R China
基金
中国国家自然科学基金;
关键词
Laser cladding; Stellite; 6; alloy; Cracks; Microstructure; Erosion resistance;
D O I
10.1016/j.engfailanal.2024.109093
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The cladding process conditions adopted naturally when laser cladding Stellite alloy surface strengthening for key positions of complex components need to be accurately adjusted because of significant differences in the heating rate and heat dissipation conditions in each region of the components. We observed that stress-relief annealing must be supplemented to effectively avoid the generation of cracks when treating small-diameter parts of 1Cr11Ni2W2MoV steel piston rods when the thickness of the cladding layer formed by laser cladding Stellite 6 alloy exceeds 2 mm. In this step, the cracks can be significantly reduced by setting the annealing temperature at 650 degrees C, holding for 2 h, and then cooling with the furnace to ensure the quality of the cladding layer is stable and reliable. We systematically analyzed the microstructure, crack defects, phase composition, and microhardness of the Stellite 6 cladding layer under different process conditions and focused on the performance of the substrate and cladding layer when subjected to erosion to understand the effect of this process on the material properties. This study not only provides an important basis for optimizing the laser cladding process but also provides a useful reference for improving the surface strengthening effect and durability of complex components.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] 1Cr11Ni2W2MoV钢制压气机叶片彩虹斑点故障分析
    唐恩军
    晁国涛
    王轶
    航空维修与工程, 2018, (10) : 79 - 82
  • [32] 1Cr11Ni2W2MoV不锈钢气体渗氮工艺研究
    王铮
    王大宏
    张金卓
    孙小琪
    王占鸿
    晁耀杰
    费岩晗
    金属加工(热加工), 2024, (06) : 23 - 28
  • [33] Process Parameters Optimization of Plasma Nitriding Depth of 1Cr11Ni2W2MoV Stainless Steel: Experimental and Simulation Studies
    Guan, Shiwei
    Li, Guifa
    Shi, Qiang
    Zuo, Linjie
    Xiao, Yixin
    Zheng, Haizhong
    Peng, Ping
    JOM, 2024, 76 (04) : 1937 - 1950
  • [34] Corrosion behavior of a steel 1Cr11Ni2W2MoV coated with NaCl in water vapor at 500-700 °C
    Shu, Yonghua
    Wang, Fuhui
    Zhou, Longjiang
    Wu, Weitao
    Jinshu Xuebao/Acta Metallurgica Sinica, 1998, 34 (05): : 483 - 488
  • [35] 1Cr11Ni2W2MoV闪光对焊接头的组织与性能
    王金雪
    袁鸿
    张国栋
    余槐
    焊接, 2015, (04) : 58 - 60+76
  • [36] Fatigue behavior of (graded) (Ti, Al)N-coated 1Cr11Ni2W2MoV stainless steel at high temperature
    Xin, Li
    Liu, Ping
    Feng, Changjie
    Zhu, Shenglong
    Wang, Fuhui
    SURFACE & COATINGS TECHNOLOGY, 2010, 204 (15): : 2417 - 2423
  • [37] Numerical and experimental study of underwater friction stir welding of 1Cr11Ni2W2MoV heat-resistant stainless steel
    Ragab, Mohamed
    Liu, Hong
    Abdel-Aleem, Hamed. A.
    Seleman, Mohamed. M. El-Sayed
    Ahmed, Mohamed. M. Z.
    Mehboob, Ghazanfar
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 29 : 130 - 148
  • [38] A study of low cycle fatigue life prediction method for 1Cr11Ni2W2MoV at 360°C
    Gao, G. D.
    Zhang, W. X.
    Chen, D.
    2ND INTERNATIONAL CONFERENCE ON NEW MATERIAL AND CHEMICAL INDUSTRY (NMCI2017), 2018, 292
  • [39] 不同热处理制度下1Cr11Ni2W2MoV钢螺栓断裂特性
    徐锐
    单金光
    戴玮高
    张华
    金属热处理, 2013, 38 (09) : 89 - 91
  • [40] 酸性环境中1Cr11Ni2W2MoV不锈钢的腐蚀行为
    孟波
    王凯
    北京石油化工学院学报, 2008, (01) : 35 - 38