Microstructure Evolution of Extruded TiAl Alloy During Vacuum Isothermal Superplastic Forging Process

被引:0
|
作者
Li, Jintao [1 ]
Wang, Xiaopeng [1 ,2 ]
Gong, Minyu [1 ]
Guo, Zhenyu [1 ]
Kong, Fantao [1 ]
机构
[1] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Ctr Anal & Measurement, Harbin 150001, Peoples R China
关键词
TiAl alloy; streamline; vacuum isothermal superplastic forging; microstructure evolution; texture; HIGH NB; MECHANICAL-PROPERTIES; DEFORMATION-BEHAVIOR; GAMMA; TEXTURE; RECRYSTALLIZATION; EXTRUSIONS; CRYSTALS;
D O I
10.3390/met15020123
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Vacuum isothermal forging is an ideal method for preparing high-performance TiAl alloy forgings, as it is carried out under the conditions of a uniform temperature field and oxygen isolation. The mechanical properties of TiAl alloys strongly depend on their microstructure, so it is important to study their microstructure evolution during the forging process to improve their properties. In this study, TiAl alloy forgings with different deformations were produced from the extruded billets by vacuum isothermal superplastic forging under lower temperatures and extremely low strain rate conditions. The results indicate that the streamlined structure in the extruded alloy was destroyed during the forging process. As the deformation increased, the dynamic recrystallization was more fully carried out, leading to a substantial decrease in remnant lamellar colonies and a significant increase in the gamma phase, and the microstructure was transformed from nearly lamellar (NL) to near gamma (NG) structure. The proportion of high-angle grain boundaries (HAGB) increased with increasing deformation, while the grain size reduced from 20 mu m to 4.6 mu m. In addition, the streamlined features and textures exhibited a weakening trend with increasing deformation, leading to a decrease in the ultimate strength from 891 MPa to 722 MPa. To maintain the streamlined characteristics and retain strengthening effects, the forging deformation should not exceed 56.7%.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Microstructure evolution during isothermal forging and subsequent heat treatment of Ti-17 alloy with a lamellar colony structure
    Xu, Jianwei
    Zeng, Weidong
    Sun, Xin
    Jia, Zhiqiang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 637 : 449 - 455
  • [32] Constitutive equation and microstructure evolution of TiAl alloy during hot deformation
    Tian, Shiwei
    Yang, Zhenyu
    Zhang, Siyuan
    Liao, Zhiqian
    Zhang, Yongjun
    Yang, Yonggang
    Chen, Yulai
    Jiang, Haitao
    MATERIALS RESEARCH EXPRESS, 2023, 10 (10)
  • [33] MICROSTRUCTURE EVOLUTION DURING ANNEALING OF CAST TiAl-BASED ALLOY
    Klimova, Alena
    Lapin, Juraj
    METAL 2014: 23RD INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2014, : 1145 - 1150
  • [34] Microstructure Evolution of AZ80 Magnesium Alloy during Multi-Directional Forging Process
    Zhu, Qingfeng
    Li, Lei
    Zhang, Zhiqiang
    Zhao, Zhihao
    Zuo, Yubo
    Cui, Jianzhong
    MATERIALS TRANSACTIONS, 2014, 55 (02) : 270 - 274
  • [35] QUASI ISOTHERMAL FORGING SIMULATION OF β-γ TiAl ALLOY CONTAINING HIGH CONTENT OF Nb
    Zheng Junzi
    Zhang Laiqi
    Hou Yongming
    Ma Xiangling
    Lin Junpin
    ACTA METALLURGICA SINICA, 2013, 49 (11) : 1439 - 1444
  • [36] The effects of microstructure evolution on the fracture toughness of BT-25 titanium alloy during isothermal forging and subsequent heat treatment
    He, Shengtong
    Zeng, Weidong
    Xu, Jianwei
    Chen, Wei
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 745 : 203 - 211
  • [37] Effect of forging on the microstructure and texture of a high Nb containing γ-TiAl alloy
    Tao, Hui
    Li, Hui-zhong
    Wang, Li
    Zhou, Rui
    Che, Yi-xuan
    Chen, Yong-hui
    Liang, Xiao-peng
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2024, 31 (06) : 1763 - 1773
  • [38] Microstructure evolution of different loading zones during TA15 alloy multi-cycle isothermal local forging
    Sun, Zhichao
    Liu, Lei
    Yang, He
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (15): : 5112 - 5121
  • [39] Microstructure evolution and mechanical properties of γ-TiAl honeycomb structure fabricated by isothermal forging and pulse current assisted diffusion bonding
    Shi, Chengcheng
    Lu, Zhen
    Zhang, Kaifeng
    Deng, Linwei
    Wang, Cheng
    INTERMETALLICS, 2018, 99 : 59 - 68
  • [40] Mechanical Properties of TiAl Based Alloy during Superplastic Deformation
    Zhang Junhong
    Xu Yajuan
    Huang Baiyun
    He Yuehui
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (06) : 1492 - 1496