Improving hot corrosion behaviour of Cr3C2-25NiCr coatings by reinforcing nano yttria-stabilized zirconia at 850 °C

被引:0
|
作者
Singh, Sukhjinder [1 ]
Goyal, Khushdeep [1 ]
Bhatia, Rakesh [2 ]
机构
[1] Punjabi Univ, Dept Mech Engn, Patiala, India
[2] Punjabi Univ, Yadavindra Dept Engn, Guru Kashi Campus, Damdama Sahib, India
关键词
Boiler steel tube; thermally sprayed coatings; zirconia ceramic; hardness; SPRAYED CR3C2-NICR; NI;
D O I
10.5599/jese.2485
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
High-temperature corrosion poses a significant threat to the longevity and performance of boiler tube materials in harsh industrial environments, necessitating the development of advanced protective coatings. Yttria-stabilized zirconia (YSZ)-enhanced Cr3C2-25NiC coatings were applied to T22 boiler tube steel using the high-velocity oxyfuel method. Conventional Ni-20Cr, 5 wt.% YSZ- Cr3C2-25NiC and 10 wt.% YSZ- Cr3C2-25NiC composite coatings were prepared. High-temperature corrosion tests were conducted on both uncoated and coated samples in a Na(2)SO(4-)60% V2O5 environment at 850 degrees C under fluctuating thermal conditions. These experiments were carried out in a silicon tube furnace at high temperatures, with each sample subjected to 50 exposure cycles. Each cycle consisted of 1 h in the corrosive environment followed by 20 minutes of cooling at room temperature. Corrosion products were analysed using energy-dispersive x-ray analysis and scanning electron microscopy. The addition of YSZ to the Cr3C2-25NiC coatings significantly improved corrosion resistance, with the Ni-20Cr, 5 wt.% YSZ-Ni-20Cr and 10 wt.% Cr3C2-25NiC coatings reducing overall weight gain by 73.08, 84.70 and 89.96 %, respectively, compared to uncoated T22 steel.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] Corrosion Behavior of Bare, Cr3C2-25%(NiCr), and Cr3C2-25%(NiCr)+0.4% CeO2-Coated Superni 600 Under Molten Salt at 900 °C
    Mudgal, Deepa
    Kumar, Sanjeet
    Singh, Surendra
    Prakash, Satya
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2014, 23 (11) : 3805 - 3818
  • [42] Tailoring microstructural features of Cr3C2-25NiCr coatings through diverse spray variants and understanding the high-temperature erosion behavior
    Alroy, Rahul Jude
    Kamaraj, M.
    Lakshmi, D. Vijaya
    Praveen, K.
    Babu, P. Suresh
    Sivakumar, G.
    TRIBOLOGY INTERNATIONAL, 2023, 188
  • [43] Abrasive wear maps for High Velocity Oxy Fuel (HVOF) sprayed WC-12Co and Cr3C2-25NiCr coatings
    Vashishtha, Nitesh
    Sapate, S. G.
    TRIBOLOGY INTERNATIONAL, 2017, 114 : 290 - 305
  • [44] Structural characteristics and wear, oxidation, hot corrosion behaviors of HVOF sprayed Cr3C2-NiCr hardmetal coatings
    Ozkan, Dervis
    SURFACE & COATINGS TECHNOLOGY, 2023, 457
  • [45] Hot-corrosion behaviour of CNT reinforced Cr3C2-NiCr coatings working under high-temperature sprayed by HVOF method
    Kuruba, Manjunatha
    Gaikwad, Giridhara
    Shivalingappa, D.
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2022, 236 (12) : 2372 - 2383
  • [46] Hot corrosion studies of HVOF sprayed Cr3C2-NiCr and Ni-20Cr coatings on nickel-based superalloy at 900°C
    Sidhu, T. S.
    Prakash, S.
    Agrawal, R. D.
    SURFACE & COATINGS TECHNOLOGY, 2006, 201 (3-4): : 792 - 800
  • [47] Friction Behavior of WC-12Co, WC-10Co4Cr and Cr3C2-25NiCr Coatings Prepared by HVOF in Different Media
    Luo Xin
    Wang Shaoyi
    Hong Yuankun
    Wu Jiayi
    Luo Wanqing
    Zhong Zhiqiang
    Yang Qiumin
    RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (12) : 4682 - 4688
  • [48] The Hot Corrosion Performance of NiCr-Cr3C2 Cermet Coating to Boiler Tube
    丁彰雄
    JournalofWuhanUniversityofTechnology-MaterialsScience, 2004, (S1) : 52 - 54
  • [49] Effect of Cr3C2 content on the tribo-corrosion behaviors of Cr3C2-NiCr/DLC duplex coatings
    He, Dongqing
    Feng, Zihan
    Liang, Ruirui
    Wang, Qianqian
    Shang, Lunlin
    SURFACE & COATINGS TECHNOLOGY, 2024, 489
  • [50] The hot corrosion performance of NiCr-Cr3C2 cermet coating to boiler tube
    Ding, ZX
    Tu, GF
    JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION, 2004, 19 : 52 - 54