High-performance thermoplastic polyimide enabled by ketone-based diamine monomer

被引:0
|
作者
Du, Qi-Yuan [1 ]
Chen, Wei-Peng [1 ]
Guo, Hao [1 ]
Wang, Zhi [1 ]
Qiu, Xiao-Kun [1 ]
Tan, Wan-Yi [1 ]
Min, Yonggang [1 ]
Liu, Yidong [2 ,3 ]
机构
[1] Guangdong Univ Technol GDUT, Guangzhou 510640, Peoples R China
[2] Chinese Acad Sci, Inst Mech, Beijing 100190, Peoples R China
[3] Guangdong Aerosp Res Acad, Guangzhou 511458, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
Thermoplastic polyimide; Peel strength; Coefficients of thermal expansion; DIANHYDRIDE; STABILITY;
D O I
10.1016/j.reactfunctpolym.2025.106230
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
Thermoplastic polyimide (TPI) as adhesive can meet the requirements of flexible copper clad laminates (FCCLs) applied under extreme condition. Incorporating flexible groups, asymmetric structures and bulky side groups into the main chain, and copolymerization are common ways to achieve thermoplasticity, through reducing the rigidity of polymer chains or intermolecular interaction. However, it induces a trade-off between thermoplasticity and thermal dimensional stability as well as mechanical property. Furthermore, the adhesion strength between TPI film and copper foil is highly desirable in FCCL. Herein, we develop a ketone-based diamine 1,3phenylenebis((3 '-amino-[1,1 '-biphenyl]-4-yl)methanone) (Ph-BiAmMe) to afford copolymerized TPI with 4,4 ' oxydianiline (ODA) and 3,3 ',4,4'-Biphenyltetracarboxylic dianhydride (BPDA). As for thermoplasticity, flexible linkages such as ether and ketone enhance the movability of polymer chains, and copolymerization weakens the intermolecular interaction between polymer chains to some extent. Furthermore, the incorporation of PhBiAmMe promotes denser chain packing and stronger CTC effect, thereby maintaining good thermal dimensional stability and mechanical properties. Simultaneously, ketone moieties enhance the peel strength of TPI when bonded with copper. Based on this strategy, the as-prepared TPI shows good thermoplasticity with a proper Tg of 274 degrees C. Meanwhile, it preserves a low CTE of 46.5 ppm K- 1, high tensile strength of 117.4 MPa, elongation at break of 27.3 % and peel strength of 1.11 N mm- 1.
引用
收藏
页数:8
相关论文
共 50 条
  • [31] Progress of High-Performance Thermosetting Polyimide Resins
    Xue S.
    Lei X.
    Lian R.
    Chen Y.
    Zhang Q.
    Gaofenzi Cailiao Kexue Yu Gongcheng/Polymeric Materials Science and Engineering, 2021, 37 (05): : 149 - 162
  • [32] Study of the degradation of high-performance polyimide foams
    Holland, DB
    Palou, JJ
    Williams, MK
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2003, 225 : U511 - U511
  • [33] Chapter 6: High-performance polyimide fibers
    Zhang, Qinghua
    Li, Xiuting
    Dong, Jie
    Zhao, Xin
    ADVANCED INDUSTRIAL AND ENGINEERING POLYMER RESEARCH, 2022, 5 (02) : 107 - 116
  • [34] Systematic Coarse Graining of a High-Performance Polyimide
    Pandiyan, Sudharsan
    Parandekar, Priya V.
    Prakash, Om
    Tsotsis, Thomas K.
    Basu, Sumit
    MACROMOLECULAR THEORY AND SIMULATIONS, 2015, 24 (05) : 513 - 520
  • [35] High-performance thermoplastic toughener for bismaleimide resin: Feature application of reactive polyarylether ketone bearing propenyl group
    Wang, Chuanhao
    Huang, Xiaohua
    Wang, Honghua
    Zhou, Guangyuan
    JOURNAL OF APPLIED POLYMER SCIENCE, 2024, 141 (32)
  • [36] READILY PROCESSED THERMOPLASTIC SHOWS HIGH-PERFORMANCE
    BRIGHT, JP
    FOSS, PN
    INDUSTRIAL RESEARCH & DEVELOPMENT, 1982, 24 (07): : 82 - 87
  • [37] High-performance thermoplastic elastomers from glucose
    Hillmyer, Marc A.
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2014, 248
  • [38] POLYETHERIMIDE - A NEW HIGH-PERFORMANCE THERMOPLASTIC RESIN
    JOHNSON, RO
    BURLHIS, HS
    JOURNAL OF POLYMER SCIENCE-POLYMER SYMPOSIA, 1983, (70) : 129 - 143
  • [39] HIGH-PERFORMANCE AND THERMOPLASTIC SILICONES FOR BIOMEDICAL APPLICATIONS
    ARKLES, B
    PLASTICS ENGINEERING, 1984, 40 (03) : 58 - 58
  • [40] THERMOPLASTIC PREPREG TECHNOLOGY FOR HIGH-PERFORMANCE COMPOSITES
    CLEMANS, S
    HARTNESS, T
    SAMPE QUARTERLY-SOCIETY FOR THE ADVANCEMENT OF MATERIAL AND PROCESS ENGINEERING, 1989, 20 (04): : 38 - 42