Research on the Influence of Liquid Metal Embrittlement Cracks on the Strength and Fatigue Life of Spot-Welded Joints of Galvanized Q&P980 Steel

被引:0
|
作者
Zou, Jie [1 ,2 ]
Xiang, Huayang [1 ,2 ]
Zhan, Zhenfei [1 ]
Zhuo, Wenbo [2 ,3 ]
Huang, Li [1 ,4 ]
Ji, Yuxiang [2 ,5 ]
Liu, Qing [2 ]
机构
[1] Chongqing Jiaotong Univ, Sch Mech & Elect & Vehicle Engn, Chongqing 400074, Peoples R China
[2] Mat Acad Jitri, Mat Bigdata & Applicat Div, Suzhou 215131, Peoples R China
[3] Nanjing Univ Sci & Technol, Sch Mech Engn, Nanjing 210094, Peoples R China
[4] Nanjing Tech Univ, Key Lab Light Weight Mat, Nanjing 210009, Peoples R China
[5] Xian Jiaotong Liverpool Univ, Sch Adv Technol, Suzhou 215123, Peoples R China
关键词
liquid metal brittleness; resistance spot welding; fatigue test; finite element analysis; BEHAVIOR; SIZE;
D O I
10.3390/ma17246149
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Galvanized high-strength steel has emerged as a key focus in automotive lightweighting research. During resistance spot welding of galvanized steel, the phenomenon of liquid metal embrittlement (LME) can occur, which is characterized by the appearance of irregular cracks on the weld spot surface. However, the impact of LME cracks on the mechanical properties of joints remains unclear. This study investigates the LME phenomenon and its effects on the performance of spot-welded joints using galvanized QP980 steel as the subject. By combining theoretical analysis, experimental methods, and simulations, the formation and characteristics of LME cracks are explored through resistance spot welding experiments and elemental analysis. The influence of LME cracks on the static strength of joints is assessed through quasi-static tensile tests, fracture surface analysis, and theoretical calculations. Finite element simulations of the static tensile process reveal that LME cracks alter the stress-strain fields during joint failure. Additionally, the study examines how the location and size of LME cracks influence these effects. Finally, fatigue testing and fracture analysis of spot-welded joints demonstrate that LME cracks can negatively impact the fatigue life of joints.
引用
收藏
页数:20
相关论文
共 36 条
  • [21] Deformation behavior of dissimilar ultrasonic spot-welded joints of a clad 7075 aluminum alloy to galvanized high-strength low-alloy steel
    Dash, S. S.
    Biswas, S.
    Peng, H.
    Jiang, X. Q.
    Li, D. Y.
    Chen, D. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 894
  • [22] Microstructural evolution of liquid metal embrittlement in resistance-spot-welded galvanized TWinning-Induced Plasticity (TWIP) steel sheets
    Lee, Hyungsoo
    Jo, Min Chul
    Sohn, Seok Su
    Kim, Sang-Heon
    Song, Taejin
    Kim, Sung-Kyu
    Kim, Hyoung Seop
    Kim, Nack J.
    Lee, Sunghak
    MATERIALS CHARACTERIZATION, 2019, 147 : 233 - 241
  • [23] Fatigue life prediction for Q420qFNH weathering steel welded joints considering the effect of multiple cracks
    Ma, Yan
    Cui, Chuang
    Zhang, Qing-hua
    Tang, Kun
    Cheng, Zhen-yu
    INTERNATIONAL JOURNAL OF FATIGUE, 2025, 190
  • [24] Three-dimension characterization of the liquid metal embrittlement crack in the resistance spot welded joint of the advanced high strength steel
    Dong, Wufeng
    Pan, Hua
    Lei, Ming
    Wang, Shujuan
    Ding, Kai
    Gao, Yulai
    MATERIALS TODAY COMMUNICATIONS, 2023, 34
  • [25] Fracture modeling of resistance spot welded ultra-high-strength steel considering the effect of liquid metal embrittlement crack
    Ma, Yunwu
    Yu, Yang
    Geng, Peihao
    Ihara, Ryohei
    Maeda, Kyohei
    Suzuki, Reiichi
    Suga, Tetsuo
    Ma, Ninshu
    MATERIALS & DESIGN, 2021, 210
  • [26] Study on Fatigue Life and Fracture Behaviour of Similar and Dissimilar Resistance Spot-Welded Joints of Titanium Grade 2 Alloy and Austenitic Stainless Steel 304
    Mezher, Marwan T.
    Pereira, Alejandro
    Trzepiecinski, Tomasz
    APPLIED SCIENCES-BASEL, 2025, 15 (04):
  • [27] Effect of sheet thickness on liquid metal embrittlement cracking of Galva-annealed quench & partitioning (Q&P) 980 MPa steel during resistance spot welding
    Kwon, Hyuck Min
    Oh, Gyu Hwan
    Lee, Chang-Wook
    Jeong, Junyeong
    JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2025, 39 (01) : 339 - 345
  • [28] Effects of Sheared Edge and Overlap Length on Reduction in Tensile Fatigue Limit before and after Hydrogen Embrittlement of Resistance Spot-Welded Ultra-High-Strength Steel Sheets
    Yagita, Ryo
    Abe, Yohei
    METALS, 2023, 13 (12)
  • [29] Effect of Welding Consumables on Fatigue Performance of Shielded Metal Arc Welded High Strength, Q&T Steel Joints
    G. Magudeeswaran
    V. Balasubramanian
    G. Madhusudhan Reddy
    Journal of Materials Engineering and Performance, 2009, 18 : 49 - 56
  • [30] Effect of Welding Consumables on Fatigue Performance of Shielded Metal Arc Welded High Strength, Q&T Steel Joints
    Magudeeswaran, G.
    Balasubramanian, V.
    Reddy, G. Madhusudhan
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2009, 18 (01) : 49 - 56