关键词
CrAlSiN; Mechanical properties; Thermal stability; Oxidation resistance; CR-AL-N; MECHANICAL-PROPERTIES; LATTICE-PARAMETER; ELASTIC-MODULUS; MICROSTRUCTURE; SUPERHARD; EVOLUTION; BEHAVIOR; HARDNESS; ORIGIN;
D O I
10.1016/j.matchar.2025.114848
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Thermal stability and oxidation resistance are crucial factors for evaluating the industrial potential of CrAlSiN coatings. Nevertheless, most of the studies focus on the microstructure and performance of CrAlSiN coatings with nanocomposite structure, the thermal stability, oxidation resistance, and the underlying mechanisms of CrAlSiN solid solution coatings still remain unknown. Here, Cr1-x-zAlxSizN coatings with gradient Si contents (z = 0-0.09) were prepared by arc evaporation. The influence of Si content on microstructure, mechanical properties, thermal stability, and oxidation resistance of CrAlSiN solid solution coatings is thoroughly discussed. The Cr1-x-zAlxSizN coatings are cubic structured up to z = 0.08, whereas the Cr0.37Al0.54Si0.09N coating demonstrates a mixed cubic and hexagonal wurtzite structure. The hardness of cubic Cr1-x-zAlxSizN coatings increases with Si content rises due to solid solution effect and grain refinement, from the 27.7 f 0.9 GPa of Cr0.46Al0.54N to the 36.1 f 0.5 GPa of Cr0.38Al0.54Si0.08N. While Cr0.37Al0.54Si0.09N coating shows a declined hardness of 33.5 f 0.6 GPa resulted from wurtzite formation. Furthermore, the breakage of Cr-N bonds is suppressed by Si-addition, where the formation temperature of hexagonal Cr2N is enhanced from 1000 degrees C for Cr0.46Al0.54N to 1100 degrees C for all Si- containing coatings. Notably, oxidation resistance is also improved by increasing Si content owing to the promoted formation of dense Cr-rich oxide scale, grain refinement, and inhibited thermal decomposition process. After oxidation at 1100 degrees C for 15 h, Cr0.44Al0.55Si0.01N, Cr0.43Al0.55Si0.02N, Cr0.42Al0.54Si0.04N, Cr0.38Al0.54Si0.08N and Cr0.37Al0.54Si0.09N coatings form oxides with thicknesses of-1.20,-0.95,-0.90,-0.90 and- 0.64 mu m, compared to the-1.49 mu m of that on Cr0.46Al0.54N coating.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Effect of Al, Si, and Cr on the thermal stability and high-temperature oxidation resistance of coatings based on titanium boronitride
    F. V. Kiryukhantsev-Korneev
    M. I. Petrzhik
    A. N. Sheveiko
    E. A. Levashov
    D. V. Shtanskii
    The Physics of Metals and Metallography, 2007, 104 : 167 - 174
  • [22] Comparative investigation of oxidation resistance and thermal stability of nanostructured Ti–B–N and Ti–Si–B–N coatings
    A. Fabrizi
    R. Cecchini
    Ph. V. Kiryukhantsev-Korneev
    A. N. Sheveyko
    S. Spigarelli
    M. Cabibbo
    Protection of Metals and Physical Chemistry of Surfaces, 2017, 53 : 452 - 459
  • [23] Hard a-Si3N4/MeNx nanocomposite coatings with high thermal stability and high oxidation resistance
    Musil, J.
    Zeman, P.
    DESIGNING OF INTERFACIAL STRUCTURES IN ADVANCED MATERIALS AND THEIR JOINTS, 2007, 127 : 31 - +
  • [24] Thermal Stability and Oxidation Resistance of Nanocomposite TiC/a-C Protective Coatings
    Martinez-Martinez, Diego
    Lopez-Cartes, Carlos
    Gago, Raul
    Fernandez, Asuncion
    Carlos Sanchez-Lopez, Juan
    PLASMA PROCESSES AND POLYMERS, 2009, 6 : S462 - S467
  • [25] A comparative investigation of the thermal stability and oxidation resistance of AlCrSiWN and AlCrSiN/AlCrWN coatings
    Chen, Lvbin
    Yan, Chenkai
    Mei, Fangsheng
    Yu, Yang
    Gao, Jiangxiong
    Yuan, Tiechui
    CERAMICS INTERNATIONAL, 2024, 50 (24) : 55766 - 55778
  • [26] Improved thermal stability and oxidation resistance of electrodeposited NiCrP amorphous alloy coatings
    Guo, Y. Q.
    Yu, J. K.
    Yang, H. B.
    Qiao, Q.
    Li, Q. Y.
    Zhao, X. C.
    BULLETIN OF MATERIALS SCIENCE, 2020, 43 (01)
  • [27] Effect of V-addition on the thermal stability and oxidation resistance of CrAlN coatings
    Xu, Yu X.
    Hu, Chun
    Chen, Li
    Pei, Fei
    Du, Yong
    CERAMICS INTERNATIONAL, 2018, 44 (06) : 7013 - 7019
  • [28] Improved thermal stability and oxidation resistance of electrodeposited NiCrP amorphous alloy coatings
    Y Q Guo
    J K Yu
    H B Yang
    Q Qiao
    Q Y Li
    X C Zhao
    Bulletin of Materials Science, 2020, 43
  • [29] Mechanical properties, thermal stability and oxidation resistance of TiN/CrN multilayer coatings
    Du, Jian W.
    Chen, Li
    Chen, Jie
    Du, Yong
    VACUUM, 2020, 179
  • [30] A superhard CrAlSiN superlattice coating deposited by a multi-arc ion plating: II. Thermal stability and oxidation resistance
    Zhang, Shihong
    Wang, Lei
    Wang, Qimin
    Li, Mingxi
    SURFACE & COATINGS TECHNOLOGY, 2013, 214 : 153 - 159