Impact of Si content on the thermal stability and oxidation resistance of cubic structured CrAlSiN coatings

被引:0
|
作者
Zhang, Xiang D. [1 ]
Chen, Li [1 ,2 ]
Du, Jian W. [1 ]
Hu, Chun [1 ]
Wang, She Q. [2 ]
机构
[1] Cent South Univ, State Key Lab Powder Met, Changsha 410083, Peoples R China
[2] Zhuzhou Cemented Carbide Cutting Tools Co Ltd, Zhuzhou 412007, Peoples R China
基金
中国国家自然科学基金;
关键词
CrAlSiN; Mechanical properties; Thermal stability; Oxidation resistance; CR-AL-N; MECHANICAL-PROPERTIES; LATTICE-PARAMETER; ELASTIC-MODULUS; MICROSTRUCTURE; SUPERHARD; EVOLUTION; BEHAVIOR; HARDNESS; ORIGIN;
D O I
10.1016/j.matchar.2025.114848
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Thermal stability and oxidation resistance are crucial factors for evaluating the industrial potential of CrAlSiN coatings. Nevertheless, most of the studies focus on the microstructure and performance of CrAlSiN coatings with nanocomposite structure, the thermal stability, oxidation resistance, and the underlying mechanisms of CrAlSiN solid solution coatings still remain unknown. Here, Cr1-x-zAlxSizN coatings with gradient Si contents (z = 0-0.09) were prepared by arc evaporation. The influence of Si content on microstructure, mechanical properties, thermal stability, and oxidation resistance of CrAlSiN solid solution coatings is thoroughly discussed. The Cr1-x-zAlxSizN coatings are cubic structured up to z = 0.08, whereas the Cr0.37Al0.54Si0.09N coating demonstrates a mixed cubic and hexagonal wurtzite structure. The hardness of cubic Cr1-x-zAlxSizN coatings increases with Si content rises due to solid solution effect and grain refinement, from the 27.7 f 0.9 GPa of Cr0.46Al0.54N to the 36.1 f 0.5 GPa of Cr0.38Al0.54Si0.08N. While Cr0.37Al0.54Si0.09N coating shows a declined hardness of 33.5 f 0.6 GPa resulted from wurtzite formation. Furthermore, the breakage of Cr-N bonds is suppressed by Si-addition, where the formation temperature of hexagonal Cr2N is enhanced from 1000 degrees C for Cr0.46Al0.54N to 1100 degrees C for all Si- containing coatings. Notably, oxidation resistance is also improved by increasing Si content owing to the promoted formation of dense Cr-rich oxide scale, grain refinement, and inhibited thermal decomposition process. After oxidation at 1100 degrees C for 15 h, Cr0.44Al0.55Si0.01N, Cr0.43Al0.55Si0.02N, Cr0.42Al0.54Si0.04N, Cr0.38Al0.54Si0.08N and Cr0.37Al0.54Si0.09N coatings form oxides with thicknesses of-1.20,-0.95,-0.90,-0.90 and- 0.64 mu m, compared to the-1.49 mu m of that on Cr0.46Al0.54N coating.
引用
收藏
页数:11
相关论文
共 50 条
  • [1] Thermal Stablility and Oxidation Resistance of CrAlSiN Nano-structured Coatings Deposited by Lateral Rotating Cathode Arc
    Cheong, Jhun Yew
    Ding, X. Z.
    Tay, Beng Kang
    Zeng, X. T.
    ADVANCED PRECISION ENGINEERING, 2010, 447-448 : 725 - +
  • [2] Effect of Si content on the thermal stability and oxidation resistance of arc-deposited TiAlSiN films with cubic structure
    Gu, Jin Z.
    Zhang, Jie
    Chen, Li
    Hu, Chun
    SURFACE & COATINGS TECHNOLOGY, 2024, 478
  • [3] Oxidation behavior of Si-doped nanocomposite CrAlSiN coatings
    Chen, Hsien-Wei
    Chan, Yu-Chen
    Lee, Jyh-Wei
    Duh, Jenq-Gong
    SURFACE & COATINGS TECHNOLOGY, 2010, 205 (05): : 1189 - 1194
  • [4] Influence of Si content on the microstructure, thermal stability and oxidation resistance of TiAlSiN/CrAlN multilayers
    Hu, Chun
    Chen, Li
    Lou, Yumin
    Zhao, Ningning
    Yue, Jianling
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 855
  • [5] Thermal stability and oxidation resistance of Cr1-xAlxN coatings with single phase cubic structure
    He, Linqing
    Chen, Li
    Xu, Yuxiang
    Du, Yong
    JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A, 2015, 33 (06):
  • [6] High temperature steam oxidation resistance of magnetron sputtered cralsin coatings
    Liu H.-Y.
    Zhu H.
    Dong Y.
    Ge F.-F.
    Huang F.
    Shu J.
    Surface Technology, 2021, 50 (03): : 308 - 314
  • [7] Influence of Nitrogen Content on the Microstructure Evolution and Oxidation Resistance toward Ambient Air of CrAlSiN Coatings Deposited by FCVAD Technique
    Zhang, Gaowei
    Liu, Yangbin
    Zhao, Cheng
    Cao, Hongshuai
    Wu, Jie
    Chen, Lin
    Wu, Jiakun
    Wang, Junfeng
    Zhang, Xu
    Liao, Bin
    ACS APPLIED MATERIALS & INTERFACES, 2024, 16 (47) : 65565 - 65580
  • [8] Thermal stability and oxidation resistance of TiAlN/CrN multilayer coatings
    Sheffield Hallam Univ, Sheffield, United Kingdom
    Surf Coat Technol, 1-3 (315-321):
  • [9] Hard nanocomposite coatings: Thermal stability, oxidation resistance and toughness
    Musil, J.
    SURFACE & COATINGS TECHNOLOGY, 2012, 207 : 50 - 65
  • [10] Interfacial structure, mechanical properties and thermal stability of CrAlSiN/CrAlN multilayer coatings
    He, Linqing
    Chen, Li
    Xu, Yuxiang
    MATERIALS CHARACTERIZATION, 2017, 125 : 1 - 6