Effect of hydrofluoric acid etching and resin cement on the flexural strength of a leucite-reinforced glass ceramic with simulating CAD-CAM milling

被引:0
|
作者
Alves, William Garcia [1 ]
Souza, Luiza Freitas Brum [2 ]
Pereira, Gabriel Kalil Rocha [2 ]
Fraga, Sara [3 ]
机构
[1] Univ Fed Rio Grande do Sul UFRGS, Sch Dent, Porto Alegre, Brazil
[2] Univ Fed Santa Maria UFSM, Postgrad Program Dent Sci, Prosthodont Unit, Santa Maria, Brazil
[3] Univ Fed Rio Grande do Sul UFRGS, Dept Conservat Dent, Div Prosthodont, Porto Alegre, Brazil
关键词
Glass ceramic; CAD-CAM; Diamond bur; Resistance; Acid etching; COMPOSITE RESIN; DENTAL RESTORATIONS; WATER SORPTION; FATIGUE; MODULUS; FABRICATION; DESIGN; FILLER;
D O I
10.1016/j.ijadhadh.2025.103946
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Objectives: To evaluate the effect of hydrofluoric acid etching and resin cement coating on the surface roughness and biaxial flexural strength of a leucite-reinforced glass ceramic ground with a diamond bur, following a protocol simulating CAD-CAM milling. Methods: Leucite-reinforced glass ceramic (IPS Empress CAD, Ivoclar AG) discs were prepared and divided into four groups (n = 20): polishing (P); grinding (G); grinding followed by 5 % hydrofluoric acid application for 60s (GH); and grinding followed by 5 % hydrofluoric acid (HA) for 60s, silane, and resin cement application (GHRC). The discs were aged in distilled water at 37 C-degrees for three months and subjected to surface roughness analysis and biaxial flexural strength testing (ISO 6872:2015). Data were compared using the Kruskal-Wallis test followed by Bonferroni-corrected multiple comparisons (alpha = 0.05). The flexural strength data were also subjected to Weibull analysis to determine the Weibull modulus. Results: Grinding the ceramic surface with an extra-fine diamond bur increased the roughness and reduced the fracture strength when compared to the polishing group. Hydrofluoric acid (GH group) produced roughness values similar to those of the G group, without affecting the material's flexural strength (p > 0.05). Resin cement coating (GHRC group) was able to significantly increase the fracture strength, when compared to the GH group (p < 0.001), reaching similar values to the polishing group (p = 0.138). Weibull modulus of the P group was significantly lower than the G group. Conclusion: Resin cement reversed the damage from grinding, restoring flexural strength to levels similar to the polished group. Hydrofluoric acid did not affect flexural strength.
引用
收藏
页数:8
相关论文
共 50 条
  • [1] CAD/CAM leucite-reinforced glass-ceramic for simulation of attrition in human enamel in vitro
    Almejrad, Lamya
    Almansour, Abdullah
    Bartlett, David
    Austin, Rupert
    DENTAL MATERIALS, 2024, 40 (02) : 173 - 178
  • [2] Effect of milling, fitting adjustments, and hydrofluoric acid etching on the strength and roughness of CAD-CAM glass-ceramics: A systematic review and meta-analysis
    May, Michele Mirian
    Fraga, Sara
    May, Liliana Gressler
    JOURNAL OF PROSTHETIC DENTISTRY, 2022, 128 (06): : 1190 - 1200
  • [3] Biaxial flexural strength of various CAD-CAM glass-ceramic materials
    Alakkad, Layali
    Kostagianni, Aikaterini
    Finkelman, Matthew
    Maawadh, Ahmed
    Ali, Ala
    Papathanasiou, Aikaterini
    AMERICAN JOURNAL OF DENTISTRY, 2021, 34 (02): : 91 - 96
  • [4] Effect of etching with low concentration hydrofluoric acid on the bond strength of CAD/CAM resin block
    Niizuma, Yuiko
    Kobayashi, Mikihiro
    Toyama, Toshinari
    Manabe, Atsufumi
    DENTAL MATERIALS JOURNAL, 2020, 39 (06) : 1000 - 1008
  • [5] Influence of Low-Pressure Plasma on the Surface Properties of CAD-CAM Leucite-Reinforced Feldspar and Resin Matrix Ceramics
    Sevilla, Pablo
    Lopez-Suarez, Carlos
    Pelaez, Jesus
    Tobar, Celia
    Rodriguez-Alonso, Veronica
    Suarez, Maria J.
    APPLIED SCIENCES-BASEL, 2020, 10 (24): : 1 - 13
  • [6] Effect of Different Etching Times with Hydrofluoric Acid on the Bond Strength of CAD/CAM Ceramic Material
    Avram, Liane Tabitha
    Galatanu, Sergiu-Valentin
    Opris, Carmen
    Pop, Cristian
    Jivanescu, Anca
    MATERIALS, 2022, 15 (20)
  • [7] Hard machining, glaze firing and hydrofluoric acid etching: Do these procedures affect the flexural strength of a leucite glass-ceramic?
    Fraga, Sara
    Valandro, Luiz F.
    Bottino, Marco A.
    May, Liliana G.
    DENTAL MATERIALS, 2015, 31 (07) : E131 - E140
  • [8] Biaxial flexural strength and Weilbull characteristics of adhesively luted hybrid and reinforced CAD/CAM materials to dentin: effect of self-etching ceramic primer versus hydrofluoric acid etching
    Mendes Tribst, Joao Paulo
    de Oliveira Dal Piva, Amanda Maria
    Lopes, Gabriel Cirone
    Souto Borges, Alexandre Luiz
    Bottino, Marco Antonio
    Ozcan, Mutlu
    de Melo, Renata Marques
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2020, 34 (12) : 1253 - 1268
  • [9] Effect of resin cement space on the fatigue behavior of bonded CAD/CAM leucite ceramic crowns
    Venturini, Andressa Borin
    Wandscher, Vinicius Felipe
    Estivalete Marchionatti, Ana Maria
    Evangelisti, Edoardo
    Ramos, Gabriela Freitas
    Melo, Renata Marques
    May, Liliana Gressler
    Baldissara, Paolo
    Valandro, Luiz Felipe
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2020, 110 (110)
  • [10] Effect of etching with distinct hydrofluoric acid concentrations on the flexural strength of a lithium disilicate-based glass ceramic
    Prochnow, Catina
    Venturini, Andressa B.
    Grasel, Rafaella
    Bottino, Marco C.
    Valandro, Luiz Felipe
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2017, 105 (04) : 885 - 891