Effects of Pre-Deformation in Corrosion Fatigue Crack Growth of Al-Mg-Zn Alloy

被引:0
|
作者
Jiang, Hui [1 ]
Jin, Junjun [2 ,3 ]
Fang, Yu [1 ]
Gou, Guoqing [3 ]
Lu, Wei [3 ]
Zhang, Zhiyi [4 ]
Zhou, Hongmei [5 ]
Sun, Hairong [6 ]
Feng, Jikui [7 ]
Chen, Jia [1 ]
Fu, Zhenghong [2 ,8 ]
机构
[1] Chengdu Ind & Trade Coll, Sch Mech Engn, Chengdu 610031, Peoples R China
[2] Cent South Univ, State Key Lab Precis Mfg Extreme Serv Performance, Changsha 410083, Peoples R China
[3] Southwest Jiaotong Univ, Sch Mat Sci & Engn, Key Lab Adv Technol Mat, Minist Educ, Chengdu 610031, Peoples R China
[4] CRRC Qingdao Sifang Co Ltd, Qingdao 266111, Peoples R China
[5] Chengdu Technol Univ, Sch Mat & Environm Engn, Chengdu 610031, Peoples R China
[6] Sichuan Special Equipment Inspect Inst, Chengdu 610031, Peoples R China
[7] Hubei Aerosp Flight Vehicle Inst, Wuhan 430000, Peoples R China
[8] Southwest Jiaotong Univ, Sch Mech & Aerosp Engn, Appl Mech & Struct Safety Key Lab Sichuan Prov, Chengdu 610031, Peoples R China
关键词
Al-Mg-Zn alloy; pre-deformation; corrosion fatigue; cracking path; dislocation density; FLOW-STRESS BEHAVIOR; ALUMINUM-ALLOY; MICROSTRUCTURE EVOLUTION; DISLOCATION DENSITY; GRAIN-BOUNDARY; PROPAGATION; BCC; TEMPERATURE; HYDROGEN;
D O I
10.3390/ma18020365
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This study investigated the effect of pre-deformation on the corrosion fatigue crack propagation (CFCG) of Al-Mg-Zn alloy in a corrosive environment. Tensile tests at different pre-deformation levels and molecular dynamics simulations analyzed changes in dislocation density. Corrosion fatigue experiments were conducted in a 3.5% NaCl solution at room temperature, and crack propagation morphology was characterized using electron backscatter diffraction (EBSD), scanning electron microscopy (SEM), and transmission electron microscopy (TEM). The results showed that tensile strength increased by 2.63% and 10.00% for 5% and 10% pre-deformation, respectively. The crack propagation threshold values were L-2 (6.36 MPa<middle dot>m(1/2)) > L-0 (6.05 MPa<middle dot>m(1/2)) > L-1 (5.13 MPa<middle dot>m(1/2)), attributed to increased dislocation density and material strength. At 5% pre-deformation, dislocation pile-ups created stress concentrations that facilitated crack propagation. In contrast, the non-uniform dislocation distribution at 10% pre-deformation enhanced both material strength and resistance to crack growth.
引用
收藏
页数:18
相关论文
共 50 条
  • [21] Effects of pre-deformation on microstructure and properties of Al–Cu–Mg–Ag heat-resistant alloy
    刘晓艳
    崔好选
    张喜亮
    王召朋
    李庆帅
    张晓亮
    Journal of Central South University, 2017, 24 (05) : 1027 - 1033
  • [22] Quantifying the Effect of Pre-deformation on Microstructure-Property Relationships in an Overaged Al-Zn-Mg-Cu Alloy
    Lianghua Lin
    Yupeng He
    Zan Li
    Shufeng Huang
    JOM, 2024, 76 : 2043 - 2052
  • [23] Effect of Microstructure on the Fatigue Crack Growth Behavior in Al-Zn-Mg-Cu Alloy
    Nandana, M. S.
    Udaya, Bhat K.
    Manjunatha, C. M.
    STRUCTURAL INTEGRITY ASSESSMENT, ICONS 2018, 2020, : 545 - 554
  • [24] Effect of large pre-deformation on the microstructure, texture and mechanical properties of Al-Zn-Mg alloy extruded profiles
    Chang, Cong
    Li, Hui
    Huang, Yuanchun
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [25] THE MICROMECHANISMS OF FATIGUE CRACK-GROWTH IN A COMMERCIAL AL-ZN-MG-CU ALLOY
    NIX, KJ
    FLOWER, HM
    ACTA METALLURGICA, 1982, 30 (08): : 1549 - 1559
  • [26] Quantifying the Effect of Pre-deformation on Microstructure-Property Relationships in an Overaged Al-Zn-Mg-Cu Alloy
    Lin, Lianghua
    He, Yupeng
    Li, Zan
    Huang, Shufeng
    JOM, 2024, 76 (04) : 2043 - 2052
  • [27] Effects of service environment and pre-deformation on the fatigue behaviour of 2524 aluminium alloy
    Chen, Y. Q.
    Zhang, H.
    Pan, S. P.
    Song, Y. F.
    Liu, X.
    Liu, W. H.
    ARCHIVES OF CIVIL AND MECHANICAL ENGINEERING, 2020, 20 (01) : 1 - 16
  • [28] Effects of service environment and pre-deformation on the fatigue behaviour of 2524 aluminium alloy
    Y. Q. Chen
    H. Zhang
    S. P. Pan
    Y. F. Song
    X. Liu
    W. H. Liu
    Archives of Civil and Mechanical Engineering, 20
  • [29] Effects of aging treatment and pre-deformation on stress corrosion cracking of magnesium alloy
    Gong, Xiaole
    Chen, Jihua
    Yan, Hongge
    Xia, Weijun
    Su, Bin
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 22 : 2844 - 2861
  • [30] Effect of pre-deformation on agehardening and microstructure in Al-Mg-Si-Cu alloy
    Gu, Yuan
    Chen, Jianghua
    Liu, Chunhui
    Zhu, Donghui
    Liu, Limei
    Tao, Guanhui
    Jinshu Xuebao/Acta Metallurgica Sinica, 2015, 51 (11): : 1400 - 1406