Effect of heat treatments on mechanical properties and wear resistance of laser-powder bed-fused Ti6Al4V alloy

被引:0
|
作者
Wang, Sen [1 ,2 ]
Wang, Linzhi [1 ,2 ]
Li, Jing [1 ,2 ]
Li, Ting [1 ,3 ]
Qiu, Yingkun [3 ]
Yang, Runqi [1 ,4 ]
机构
[1] Univ Chinese Acad Sci, Chongqing 400714, Peoples R China
[2] Chinese Acad Sci, Chongqing Inst Green & Intelligent Technol, Chongqing Key Lab Addit Mfg Technol & Syst, Chongqing 400714, Peoples R China
[3] Chongqing Univ Technol, Coll Mat Sci & Engn, Chongqing 400054, Peoples R China
[4] Chongqing Jiaotong Univ, Chongqing 400074, Peoples R China
来源
MODERN PHYSICS LETTERS B | 2024年 / 38卷 / 26期
关键词
Selective laser melting; Ti6Al4V alloy; heat treatment; mechanical properties; wear resistance; MELTED TI-6AL-4V; BEHAVIOR; MICROSTRUCTURE; TEMPERATURE; PERFORMANCE;
D O I
暂无
中图分类号
O59 [应用物理学];
学科分类号
摘要
The effects of heat treatment on the microstructure, mechanical properties and wear resistance of Selective Laser Melting Ti6Al4V alloy were systematically studied. The results show that the as-built part has an acicular alpha ' martensite structure. The increase in heat treatment temperature causes the decomposition of acicular alpha ' martensite, which leads to the decrease of the hardness of Ti6Al4V alloy. When the heat treatment temperature is 800 degrees C, the alloy forms an alpha '/alpha structure, which increases the tensile strength and elongation of the alloy by 12% and 23%, respectively. When the heat treatment reaches above 900 degrees C, the mechanical properties of the alloy decrease sharply due to the disappearance of the alpha '/alpha structure, the coarse grains of the alpha phase, and the increase of the content of the beta phase. The tensile strength decreased from 935 MPa to 815 MPa, and the elongation decreased from 8.7% to 3.1%. With the increase of heat treatment temperature, the friction coefficient and wear rate increase linearly, which is opposite to the changing trend of hardness, and the wear mechanism is changed from single abrasive wear to abrasive wear and oxidative wear. This is attributed to the increase in the grain size of the alloy and the increase in the content of the beta phase, resulting in a decrease in the overall hardness of the alloy.
引用
收藏
页数:15
相关论文
共 50 条
  • [31] Microstructure and Corrosion Resistance of Ti6Al4V Manufactured by Laser Powder Bed Fusion
    Luo, Yiwa
    Wang, Mingyong
    Zhu, Jun
    Tu, Jiguo
    Jiao, Shuqiang
    METALS, 2023, 13 (03)
  • [32] Effect of Thermal Oxidation Temperature on Wear Resistance of Ti6Al4V Alloy
    Lin Naiming
    Wang Yating
    Zou Jiaojuan
    Ma Yong
    Wang Zhenxia
    Tian Wei
    Yao Xiaofei
    Tang Bin
    RARE METAL MATERIALS AND ENGINEERING, 2016, 45 (06) : 1615 - 1619
  • [33] Impact of Heat Treatment on Microstructure and Mechanical Characteristics of Laser Powder Bed Fused Ti-6Al-4V Alloy: A Comprehensive Investigation
    Rizwee, Mumtaz
    Kumar, Deepak
    Husain, Md Murtuja
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025,
  • [34] Effect of Heat Treatment on Microstructure and Mechanical Properties of Ti6Al4V Alloy Fabricated by Selective Laser Melting
    Waqas, Muhammad
    He, Dingyong
    Liu, Yude
    Riaz, Saleem
    Afzal, Farkhanda
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2023, 32 (02) : 680 - 694
  • [35] Effect of Heat Treatment on Microstructure and Mechanical Properties of Ti6Al4V Alloy Fabricated by Selective Laser Melting
    Muhammad Waqas
    Dingyong He
    Yude Liu
    Saleem Riaz
    Farkhanda Afzal
    Journal of Materials Engineering and Performance, 2023, 32 : 680 - 694
  • [36] Microstructural, mechanical and wear behaviour of Inconel-718 produced through laser-powder bed-fused additive manufacturing
    Jeyaprakash, N.
    Yang, Che-Hua
    Ramkumar, K. R.
    MATERIALS SCIENCE AND TECHNOLOGY, 2021, 37 (03) : 326 - 337
  • [37] Competing roles of microstructure and defects on the mechanical properties of laser-powder bed fused Ti-6Al-2Sn-4Zr-2Mo alloy
    Kaushik, Harish Chandra
    Shakerin, Sajad
    Korayem, Mahdi Habibnejad
    Mohammadi, Mohsen
    Hadadzadeh, Amir
    PROGRESS IN ADDITIVE MANUFACTURING, 2025, 10 (02) : 1605 - 1627
  • [38] Microstructure and mechanical properties of selective laser melted Ti6Al4V alloy
    Losertova, M.
    Kubes, V.
    27TH JOINT SEMINAR DEVELOPMENT OF MATERIALS SCIENCE IN RESEARCH AND EDUCATION, 2017, 266
  • [39] Effect of Processing Routes on Microstructural Development, Mechanical Properties, and Wear Behavior of Ti6Al4V Alloy
    Maghazei, Parastoo
    Ranjbar, Khalil
    Naseri, Javid
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025, 34 (03) : 1992 - 2003
  • [40] The role of annealing heat treatment in high-temperature oxidation resistance of laser powder bed fused Ti6Al4V alloy subjected to massive laser shock peening treatment
    Wang, Zhao
    Huang, Shu
    Lu, Haifei
    Liu, Jiajun
    Alexandrov, Igor V.
    Luo, Kaiyu
    Lu, Jinzhong
    CORROSION SCIENCE, 2022, 209