Dry sliding wear behaviour of AA6082/BN/Mos2 hybrid metal matrix composites synthesized using stir casting process

被引:0
|
作者
James, D. Jafrey Daniel [1 ]
Pandiyan, G. Karthik [2 ]
Aruna, M. Thanga [3 ]
Katiyar, Jitendra Kumar [4 ]
机构
[1] K Ramakrishnan Coll Engn, Dept Mech Engn, Tiruchirappalli, Tamil Nadu, India
[2] Sri Vidya Coll Engn & Technol, Dept Mech Engn, Virudunagar, Tamil Nadu, India
[3] PSR Engn Coll, Dept Comp Sci & Engn, Sivakasi, Tamil Nadu, India
[4] Chitkara Univ, Ctr Res Impact & Outcome, Chandigarh-Patiala Natl Highway NH-7, Rajpura 140401, Punjab, India
关键词
Metal matrix composite; wear; friction; stir casting; tribofilm; fillers; TRIBOLOGICAL PROPERTIES; OPTIMIZATION; DESIGN; MOS2;
D O I
10.1177/13506501241291390
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This study examines the wear behaviour of AA6082/x Boron Nitride (BN) (x = 1, 2, 3 wt.%)/1 wt.% of Molybdenum Disulphide (MoS2), a novel hybrid metal matrix composite (MMC), under dry sliding conditions. The composite was fabricated through liquid-state processing, i.e., stir casting. A pin-on-disk tribometer was used to estimate the coefficient of friction (COF) and wear rate by varying tribological process parameters under dry sliding conditions. The results show that at the maximum load of 40 N, the wear rate of the unreinforced alloy is observed 4.077 x 10-2 mm3/m, while at the AA6082/3 wt. of %, BN/1 wt. % of the MoS2 composite's wear rate is reduced to 2.162 x 10-2 mm3/m. Further, the wear rate increases as the sliding distance increases from 500 m to 2000 m. Moreover, the friction coefficient of the unreinforced alloy is observed 0.37, whereas the AA6082/3 wt.% of BN/1 wt.% of MoS2 composites is observed 0.31 under reduced loads. It might be due to the presence of hard ceramic BN and MoS2 reinforcements enhancing the developed composite's resistance to wear by forming a mechanically mixed layer (Fe2O3) on the sliding contact surface. Moreover, the novel hybrid composite materials exhibit a lower coefficient of friction at higher sliding velocities, sliding distances, and applied loads. However, minimal fine grooves with limited abrasion are observed on the worn surface, which was examined through a scanning electron microscope.
引用
收藏
页数:15
相关论文
共 50 条
  • [31] OPTIMIZATION AND ANALYSIS OF DRY SLIDING WEAR BEHAVIOUR OF N-B4C/MOS2 UREINFORCED AA2219 NANO HYBRID COMPOSITES USING RESPONSE SURFACE METHODOLOGY
    Chitwadgi, Riddhisha
    Siddesh, B.
    Shankar, B. Latha
    Suresh, R.
    Siddeshkumar, N.
    METALLURGICAL & MATERIALS ENGINEERING, 2022, 28 (03) : 469 - 485
  • [32] Machinability analysis and optimisation of EDM in AA6082/3 wt% BN/1 wt% MoS2 hybrid composites using entropy method weights integrated with complex proportional assessment (COPRAS) method
    Karthik Pandiyan Ganesan
    Jafrey Daniel James Dhilip
    Vinothkumar Sivalingam
    Arjun Duraipalam
    Gowtham Seenivasan
    Gokul Kannan Perumal
    Bhuvaneshwar Karthikeyan
    Ram Kumar Rajagopal
    Mohanraj Chandran
    The International Journal of Advanced Manufacturing Technology, 2022, 123 : 4051 - 4064
  • [33] Synthesis, Characterization and Dry Sliding Wear Behaviour of Al 7075–MoSi2 Composites Prepared by Stir Casting Technique
    M. K. Manoj
    Vikas Gadpale
    Transactions of the Indian Institute of Metals, 2019, 72 : 3153 - 3169
  • [34] Synthesis, Characterization and Dry Sliding Wear Behaviour of Al 7075-MoSi2 Composites Prepared by Stir Casting Technique
    Manoj, M. K.
    Gadpale, Vikas
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2019, 72 (12) : 3153 - 3169
  • [35] Microstructure and temperature-dependent fretting wear behaviour of AA7075/MoS2/Red-Mud Hybrid composites via vacuum-assisted stir casting route
    Gurmaita, Priyeshiv Kumar
    Singh, Virendra Pratap
    Pongen, Rosang
    VACUUM, 2025, 232
  • [36] Taguchi Grey Relational Analysis of Dry Sliding Wear Behaviour of Annealed AA7075-TiC metal matrix composites
    Baskaran, S.
    Anandakrishnan, V.
    Duraiselvam, Muthukannan
    Raghuraman, S.
    Muthaiyaa, V. M. Illayaraja
    ENGINEERING AND MANUFACTURING TECHNOLOGIES, 2014, 541-542 : 258 - +
  • [37] Characterization of Y2O3 particles reinforced AA6082 aluminum matrix composites produced using friction stir processing
    Kumar, J. Ramesh
    Jayaraman, M.
    Kumar, T. Satish
    Priyadharshini, G. Suganya
    Kumar, J. Satheesh
    MATERIALS RESEARCH EXPRESS, 2019, 6 (08):
  • [38] Parametric study of the dry sliding wear behaviour of AA6082-T6/SiC and AA6082-T6/B4C composites using RSM
    Gurpreet Singh
    Sanjeev Goyal
    Georgina Miranda
    Neeraj Sharma
    Journal of Mechanical Science and Technology, 2018, 32 : 579 - 592
  • [39] Parametric study of the dry sliding wear behaviour of AA6082-T6/SiC and AA6082-T6/B4C composites using RSM
    Singh, Gurpreet
    Goyal, Sanjeev
    Miranda, Georgina
    Sharma, Neeraj
    JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2018, 32 (02) : 579 - 592
  • [40] Parametric study on the dry sliding wear behaviour of AA6082-T6/TiB2 in situ composites using response surface methodology
    Singh, Gurpreet
    Chan, Sammy Lap-Ip
    Sharma, Neeraj
    JOURNAL OF THE BRAZILIAN SOCIETY OF MECHANICAL SCIENCES AND ENGINEERING, 2018, 40 (06)