Development of oxidation-resistant carbon fibers and evaluation of their performance in a carbon matrix composite

被引:0
|
作者
Chouhan, Bhavika [1 ]
Vekariya, Nikhil [2 ]
Raut, Bikash [1 ]
Jaswal, Ashish [1 ]
Valand, Jignesh [2 ]
Sharma, Swati [1 ]
机构
[1] Indian Inst Technol Mandi, Sch Mech & Mat Engn, Mandi 175075, Himachal Prades, India
[2] Sardar Patel Univ, Dept Mat Sci, Vallabh Vidyanagar 388120, Gujarat, India
关键词
Carbon/ carbon composite; Carbon fiber; Electrospinning; Oxidation resistance; High-temperature material; MECHANICAL-PROPERTIES; COMPRESSION; PROTECTION;
D O I
10.1016/j.diamond.2025.112105
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Here we report on a novel approach to achieve an inherent oxidation protection up to 620 degrees C in electrospun carbon fiber (CF) mats by incorporating a SiO2 precursor into a CF precursor polymer. A carbon/carbon (C/C) composite is prepared using these CF mats in a pitch-derived carbon matrix and its performance is evaluated. Oxidation resistance in CFs is achieved by a controlled addition of polydimethylsiloxane (PDMS) directly into the polyacrylonitrile (PAN) prior to electrospinning. The concentration of PDMS is optimized such that the mechanical properties of the fibers remain within the usable range. C/C composite prepared using these fibers is characterized for its thermal and mechanical properties through flame treatment and compression tests, respectively. The composite, having <0.5 wt% CFs in a carbon matrix, shows a good thermal stability and retains similar to 60 % weight at 800 degrees C in zero air atmosphere. Addition of electrospun CFs has improved its mechanical properties, which are evaluated against those of the matrix material. The prepared composite exhibits a compressive strength of similar to 68 MPa and Rockwell hardness of similar to 72 HRB. Flame treatment tests indicate a lower surface erosion and weight loss in the composite caused by a thermal shock when compared to the matrix. The fabrication method is simple, low-cost, and suitable for research applications such as device fabrication.
引用
收藏
页数:8
相关论文
共 50 条
  • [21] A Multilayer Ceramic Matrix for Oxidation Resistant Carbon Fibers-Reinforced CMCs
    Lamouroux, F.
    Bertrand, S.
    Pailler, R.
    Naslain, R.
    Key Engineering Materials, 164-165 : 365 - 368
  • [22] OXIDATION RESISTANT CARBON MATRIX COMPOSITES
    ROGERS, DC
    SHUFORD, DM
    SEEGER, JW
    AMERICAN CERAMIC SOCIETY BULLETIN, 1972, 51 (09): : 714 - &
  • [23] THE DEVELOPMENT OF OXIDATION-RESISTANT NIOBIUM ALLOYS
    SMITH, R
    JOURNAL OF THE LESS-COMMON METALS, 1960, 2 (2-4): : 191 - 206
  • [24] DEVELOPMENT OF OXIDATION-RESISTANT NIOBIUM ALLOYS
    KLING, HT
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1957, 104 (03) : C70 - C70
  • [25] Aluminum Matrix Composite Reinforced by Carbon Fibers
    Galyshev, Sergey
    Gomzin, Andrey
    Musin, Fanil
    MATERIALS TODAY-PROCEEDINGS, 2019, 11 : 281 - 285
  • [26] Oxidation-Resistant and Elastic Mesoporous Carbon with Single-Layer Graphene Walls
    Nishihara, Hirotomo
    Simura, Tomoya
    Kobayashi, Shunsuke
    Nomura, Keita
    Berenguer, Raul
    Ito, Masashi
    Uchimura, Masanobu
    Iden, Hiroshi
    Arihara, Kazuki
    Ohma, Atsushi
    Hayasaka, Yuichiro
    Kyotani, Takashi
    ADVANCED FUNCTIONAL MATERIALS, 2016, 26 (35) : 6418 - 6427
  • [27] THE DEVELOPMENT AND PROPERTIES OF AN OXIDATION-RESISTANT COATING FOR URANIUM
    BUDDERY, JH
    CLARK, ME
    PEARCE, RJ
    STOBBS, JJ
    JOURNAL OF NUCLEAR MATERIALS, 1964, 13 (02) : 169 - 181
  • [28] ZRPT3 AS A HIGH-TEMPERATURE, REFLECTIVE, OXIDATION-RESISTANT COATING FOR CARBON-CARBON COMPOSITES
    ALVEY, MD
    GEORGE, PM
    CARBON, 1991, 29 (4-5) : 523 - 530
  • [29] A SiC/Mo( Six , Al1-x ) 2 oxidation-resistant coating for carbon/carbon composites
    Wang Xiang-hui
    Weng Li
    Zhang Wei-gang
    NEW CARBON MATERIALS, 2014, 29 (02) : 126 - 131
  • [30] A Si-SiC Oxidation-resistant Coating for Carbon/Carbon Composites by Hot-pressing Reaction Technique
    Fu, Qiangang
    Cao, Cuiwei
    Li, Hejun
    Tao, Jun
    Li, Kezhi
    INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2014, 11 (02) : 342 - 349