High thickness material lift-off using multi-layer photoresist

被引:0
|
作者
Elshenety, Ahmad [1 ,2 ]
Kucuk, Merve Mintas [1 ,2 ]
Yilmaz, Mehmet [2 ]
机构
[1] Bilkent Univ, Inst Mat Sci & Nanotechnol, TR-06800 Ankara, Turkiye
[2] Bilkent Univ, UNAM, Natl Nanotechnol Res Ctr, TR-06800 Ankara, Turkiye
关键词
image reversal photoresist; bi-layer photoresist; tri-layer photoresist; quad-layer photoresist; multi-layer photoresist; AZ; 5214E; 4562;
D O I
10.1088/1361-6439/adac6b
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Lift-off process is an alternative to deposition, lithography, and etching of materials. Lift-off is a simple and economical process because it does not require subsequent wet or dry etching. Lifting-off nanometer thick films is a well-developed and repeatable process. However, lifting-off a few micrometer thick films may be challenging. Previously, different techniques were proposed to lift-off micrometer thick films. Herein, a novel method for lifting-off high thickness materials is proposed using a multi-layer AZ 5214E photoresist. The novel method was successful in lifting-off 4 mu m thick copper while the copper could even be deposited up to 6 mu m with tri-layer AZ 5214E. With four layers of AZ 5214E, the photoresist thickness can be even thicker than 9 mu m. As detailed in the study, the photoresist layer thickness can be adjusted by varying the number of layers. This enables the selection of the appropriate number of layers to achieve the desired material thickness. To show the merits of the proposed method, the method is compared to the bi-layer method with AZ 4562 photoresist which is used for lifting-off high thickness materials. In addition to lifting-off thick materials, the proposed method is faster compared to lifting-off using bi-layer AZ 4562. Despite the ability to lift-off thick films, both methods could suffer from lift-off flags if the deposition process is not anisotropic. Solutions to remove the lift-off flags, and reduce the undercut width are demonstrated.
引用
收藏
页数:9
相关论文
共 50 条
  • [41] Fabrication of high quality PZT thick film using lift-off technique
    Zhao, HJ
    Ren, TL
    Liu, JS
    Liu, LT
    Li, ZJ
    NANOTECH 2003, VOL 1, 2003, : 502 - 505
  • [42] Lift-off lithography using an atomic force microscope
    Bouchiat, V
    Esteve, D
    APPLIED PHYSICS LETTERS, 1996, 69 (20) : 3098 - 3100
  • [43] Metal lift-off using physical vapour deposition
    O'Sullivan, J
    Burgess, S
    Rimmer, N
    MICROELECTRONIC ENGINEERING, 2002, 64 (1-4) : 473 - 478
  • [44] Differential Coupling Double-Layer Coil for Eddy Current Testing With High Lift-Off
    Chen, Kefan
    Gao, Bin
    Tian, Gui Yun
    Yang, Yupei
    Yang, Changrong
    Ma, Qiuping
    IEEE SENSORS JOURNAL, 2021, 21 (16) : 18146 - 18155
  • [45] Chemical lift-off lithography by collapsing soft-material molds
    Liao, Wei-Ssu
    Jan, Hong-Hseng
    ABSTRACTS OF PAPERS OF THE AMERICAN CHEMICAL SOCIETY, 2015, 249
  • [46] Improved bi-layer lift-off process for MEMS applications
    Liang, Jinxing
    Kohsaka, Fusao
    Matsuo, Takahiro
    Li, Xuefeng
    Ueda, Toshitsugu
    MICROELECTRONIC ENGINEERING, 2008, 85 (5-6) : 1000 - 1003
  • [47] Micro-patterning of PZT thick film by lift-off using ZnO as a sacrificial layer
    Li, Junhong
    Ren, Wei
    Wang, Chenghao
    Liu, Mengwei
    Fan, Guoxiang
    CERAMICS INTERNATIONAL, 2015, 41 (06) : 7325 - 7328
  • [48] Measurement of Lift-Off Distance and Thickness of Nonmagnetic Metallic Plate Using Pulsed Eddy Current Testing
    Huang, Pu
    Li, Zhiying
    Long, Jun
    Xu, Lijun
    Xie, Yuedong
    IEEE TRANSACTIONS ON INSTRUMENTATION AND MEASUREMENT, 2023, 72
  • [49] Probe Lift-off Compensation Method for Pulsed Eddy Current Thickness Measurement
    Huang, Chen
    Wu, Xinjun
    PROCEEDINGS OF 2014 3RD ASIA-PACIFIC CONFERENCE ON ANTENNAS AND PROPAGATION (APCAP 2014), 2014, : 937 - 939
  • [50] Research on thickness measurement based on lift-off intersection of pulsed eddy current
    Zheng, Gang
    Liu, Ding
    Zhang, Zhen
    Li, Haowen
    Yi Qi Yi Biao Xue Bao/Chinese Journal of Scientific Instrument, 2008, 29 (08): : 1745 - 1749