A Study of Impact Toughness Behavior and High Cycle Fatigue Properties of Al-Li 8090 Alloy Processed by Cryorolling and Post-Deformation Annealing

被引:0
|
作者
Thapliyal, Subham [1 ]
Joshi, Amit [2 ]
Gairola, Saurabh [3 ]
Kalavathi, G. K. [4 ]
Vasundhara, M. G. [4 ]
Muralidhara, B. [5 ]
Yogesha, K. K. [6 ]
机构
[1] Uttaranchal Univ, Uttaranchal Inst Technol, Dept Mech Engn, Dehra Dun 248007, Uttarakhand, India
[2] Govind Ballabh Pant Inst Engn & Technol Pauri, Dept Mech Engn, Ghurdauri 246194, India
[3] Indian Inst Technol, Dept Engn Design, Chennai 600036, India
[4] Malnad Coll Engn, Hassan 573201, India
[5] Governament Engn Coll, Hassan 573212, T&D, India
[6] Natl Inst Engn, Mysuru 570008, India
关键词
Ultrafine-grained (UFG) structure; High cycle fatigue; Impact toughness; Electron backscattered diffraction; SEVERE PLASTIC-DEFORMATION; MECHANICAL-PROPERTIES; TENSILE; TORSION; GROWTH;
D O I
10.1007/s13632-025-01184-4
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This study investigates the microstructural evolution and mechanical properties such as tensile, impact toughness, and high cycle fatigue (HCF) of cryorolled (CR) and post-rolled annealing treatment of Al-Li 8090 alloy. The solution-treated (ST) Al-Li 8090 alloy was cryorolled to a true strain value of 2.3 and annealed in the temperature range of 100 degrees C - 350 degrees C. The equiaxed microstructure in the ST samples is converted into ultrafine-grained (UFG) elongated microstructure along the rolling direction. The UFG microstructure, along with the high dislocation density in the CR specimen observed using electron backscattered diffraction, led to an increment in the tensile, hardness, impact toughness, and HCF properties such as the impact toughness and fatigue strength increased by 9.10% and 26.38%, respectively. The annealing temperature further enhances the mechanical properties up to 150 degrees C due to the evolution of strengthening precipitates such as Al2CuMg and Al3Ti, as well as the formation of recrystallized grains.
引用
收藏
页数:13
相关论文
共 50 条
  • [31] Investigations of microstructure, impact toughness, and fatigue failure behavior of bulk UFG Al–Li 8090 alloy processed by multi-axial forging
    Amit Panwar
    Amit Joshi
    Sachin Tejyan
    Sādhanā, 49
  • [32] Grain structure and microtexture after high temperature deformation of an Al-Li (8090) alloy
    Eddahbi, M
    Thomson, CB
    Carreño, F
    Ruano, OA
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 284 (1-2): : 292 - 300
  • [33] Microstructure evolution during high-temperature deformation of 8090 Al-Li alloy
    Xun, Y
    Tan, MJ
    MATERIALS AND MANUFACTURING PROCESSES, 2004, 19 (03) : 373 - 389
  • [34] THE TENSILE PROPERTIES AND FRACTURE-BEHAVIOR OF UNIDIRECTIONALLY SOLIDIFIED 8090 AL-LI ALLOY
    LIU, YL
    HU, ZQ
    ZHANG, Y
    ZHAO, HE
    SHI, CX
    SCRIPTA METALLURGICA ET MATERIALIA, 1992, 27 (10): : 1395 - 1400
  • [35] FATIGUE CRACK-PROPAGATION BEHAVIOR OF THE AL-LI ALLOY-8090 COMPARED TO ALLOY-2024
    PETERS, M
    BACHMANN, V
    WELPMANN, K
    JOURNAL DE PHYSIQUE, 1987, 48 (C-3): : 785 - 791
  • [36] Stain anisotropy in AA8090 Al-Li alloy during high temperature deformation
    Kashyap, BP
    Chaturvedi, MC
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 281 (1-2): : 88 - 95
  • [37] Improvement of fracture toughness of ultra fine grained Al-Li 8090 alloy processed through multi axial forging
    Kapil, Rajat
    Joshi, Amit
    Jayaganthan, R.
    Gairola, Saurabh
    Verma, Raviraj
    MATERIALS RESEARCH EXPRESS, 2019, 6 (08):
  • [38] THE EFFECTS OF BE ON MECHANICAL-PROPERTIES AND FRACTURE-BEHAVIOR OF AL-LI ALLOY-8090
    LUO, A
    YOUDELIS, WV
    CANADIAN METALLURGICAL QUARTERLY, 1992, 31 (04) : 283 - 287
  • [39] INFLUENCE OF AGING ON LOW-CYCLE FATIGUE BEHAVIOR IN 8090-AL-LI ALLOY
    AI, SH
    WANG, ZG
    ZHANG, Y
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 1995, 5 (01) : 80 - 83
  • [40] Low-cycle fatigue crack initiation and break in strain-life curve of Al-Li 8090 alloy
    Yong Jun Oh
    Bong Sang Lee
    Sang Chul Kwon
    Jun Hwa Hong
    Soo Woo Nam
    Metallurgical and Materials Transactions A, 1999, 30 : 887 - 890