Voltage and temperature effects on low cobalt lithium-ion battery cathode degradation

被引:0
|
作者
Malabet, Hernando J. Gonzalez [1 ]
Gober, Megan [1 ]
Patel, Prehit [1 ]
L'Antigua, Alex [1 ]
Gabhart, Austin [1 ]
Amai, Joseah [1 ]
Xiao, Xianghui [2 ]
Nelson, George J. [1 ]
机构
[1] Univ Alabama, Dept Mech & Aerosp Engn, Huntsville, AL 35899 USA
[2] Brookhaven Natl Lab, Natl Synchrotron Lightsource 2, Upton, NY 11973 USA
来源
ENERGY ADVANCES | 2025年 / 4卷 / 02期
关键词
RELAXATION-TIMES; ELECTRODE THICKNESS; COMPOSITE CATHODES; AGING MECHANISMS; CELLS; STATE; DECONVOLUTION; PERFORMANCE; DISCHARGE; SURFACE;
D O I
10.1039/d4ya00530a
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Degradation of low cobalt lithium-ion cathodes was tested using a full factorial combination of upper cut-off voltage (4.0 V and 4.3 V vs. Li/Li+) and operating temperature (25 degrees C and 60 degrees C). Half-cell batteries were analyzed with electrochemical and microstructural characterization methods. Electrochemical performance was assessed with galvanostatic cycling, cyclic voltammetry (CV), and electrochemical impedance spectroscopy (EIS) supported by distribution of relaxation times (DRT) analysis. Electrode microstructure was characterized with scanning electron microscopy (SEM), X-ray diffraction (XRD), and X-ray absorption near edge structure (XANES) imaging. Higher cut-off voltage cycling shows presence of NiOx formation, a low diffusivity rock-salt phase, in both CV and XRD data. XRD patterns confirmed that the rock-salt phase was beginning to form at the low cut-off voltage at high temperature, but in much lower intensity than at the high cut-off voltage. Higher temperature accelerates degradation processes at both voltages. Degradation factors at high temperature include NiOx formation, cathode material dissolution, and electrolyte decomposition. SEM analysis suggests that supporting phases may isolate and disconnect active material particles reducing capacity retention and battery life cycle. DRT analysis and XANES imaging show that both high temperature samples revealed a NiOx phase based on an increased diffusive impedance and a visible shift in the XANES spectra. The low cut-off voltage, high temperature sample showed a split peak and shift to lower energies indicating early formation of the NiOx phase. The diffusive impedance, which hinders intercalation and deintercalation, is driven by the formation of the NiOx phase. While primarily driven by cut-off voltage, elevated temperature also contributes to this degradation mechanism.
引用
收藏
页码:304 / 319
页数:16
相关论文
共 50 条
  • [31] Temperature estimation from current and voltage measurements in lithium-ion battery systems
    Wang, P.
    Yang, L.
    Wang, H.
    Tartakovsky, D. M.
    Onori, S.
    JOURNAL OF ENERGY STORAGE, 2021, 34
  • [32] Lithium-Ion Battery Relaxation Effects
    Messing, Marvin
    Shoa, Tina
    Habibi, Saeid
    2019 IEEE TRANSPORTATION ELECTRIFICATION CONFERENCE AND EXPO (ITEC), 2019,
  • [33] Electrochemical modeling and parameter sensitivity of lithium-ion battery at low temperature
    Gholami, Javad
    Barzoki, Mohammad Fallah
    JOURNAL OF ENERGY STORAGE, 2021, 43
  • [34] A Low Cost Lithium-Ion Battery Tester with a Zero Voltage Discharge Capability
    Pyo, Young-Hak
    Choi, See-Young
    Choi, Yeong-Jun
    Kim, Rae-Young
    PROCEEDINGS OF THE IECON 2016 - 42ND ANNUAL CONFERENCE OF THE IEEE INDUSTRIAL ELECTRONICS SOCIETY, 2016, : 3135 - 3140
  • [35] Effect of Ethyl Acetate on Low Temperature Property in Lithium-ion Battery
    Park, Dong-Won
    Chung, Myoung-Woo
    Kim, Shin-Kook
    Choi, Yong-Kook
    JOURNAL OF THE KOREAN CHEMICAL SOCIETY-DAEHAN HWAHAK HOE JEE, 2008, 52 (06): : 676 - 683
  • [36] Electrochemical performance of Mo doped high voltage spinel cathode material for lithium-ion battery
    Kazda, T.
    Vondrak, J.
    Visintin, A.
    Sedlarikova, M.
    Tichy, J.
    Cudeka, P.
    JOURNAL OF ENERGY STORAGE, 2018, 15 : 329 - 335
  • [37] Effects of Nonuniform Temperature Distribution on Degradation of Lithium-Ion Batteries
    Cavalheiro, Gabriel M.
    Iriyama, Takuto
    Nelson, George J.
    Huang, Shan
    Zhang, Guangsheng
    JOURNAL OF ELECTROCHEMICAL ENERGY CONVERSION AND STORAGE, 2020, 17 (02)
  • [38] Degradation of organic pollutants accompanied by the ultrasonic separation of the spent lithium-ion battery cathode materials
    Huang, Youbao
    Sun, Mingze
    Xu, Chengjian
    Hu, Hao
    Zhu, Shuguang
    He, Wenzhi
    WASTE MANAGEMENT & RESEARCH, 2024, 42 (01) : 74 - 80
  • [39] Characterizing and Mitigating Chemomechanical Degradation in High-Energy Lithium-Ion Battery Cathode Materials
    Luu, Norman S.
    Park, Kyu-Young
    Hersam, Mark C.
    ACCOUNTS OF MATERIALS RESEARCH, 2022, 3 (05): : 511 - 524
  • [40] Lithium plating in a commercial lithium-ion battery A low-temperature aging study
    Petzl, Mathias
    Kasper, Michael
    Danzer, Michael A.
    JOURNAL OF POWER SOURCES, 2015, 275 : 799 - 807