Hot-pressed SmCo5/DyF3 composite magnets with high electrical resistivities

被引:0
|
作者
Zheng, Liyun [1 ,2 ]
Hou, Bingze [1 ]
Zhou, Dong [2 ]
Yu, Xiaojun [2 ]
Zhao, Lixin [1 ,3 ]
Fang, Yikun [2 ]
Wu, Licheng [1 ]
Li, Wei [1 ,2 ]
Hadjipanayis, George C. [4 ]
机构
[1] Hebei Univ Engn, Hebei Engn Res Ctr Rare Earth Permanent Magnet Mat, Handan 056038, Hebei, Peoples R China
[2] China Iron & Steel Res Inst Grp Co Ltd, Div Funct Mat, Beijing 100081, Peoples R China
[3] Hebei Univ Engn, Sch Mech & Equipment Engn, Handan 056038, Hebei, Peoples R China
[4] Univ Delaware, Dept Phys & Astron, Newark, DE 19716 USA
关键词
SmCo5; magnet; Hot pressing process; Magnetic properties;
D O I
10.1016/j.jmmm.2025.172946
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
DyF3 powders have been milled in different processes and SmCo5 permanent magnets with DyF3 additions have been prepared by hot-pressing method. Influences of milling process, particle sizes, morphologies and amounts of DyF3 on the microstructures, electrical resistivities and magnetic properties of the hot-pressed SmCo5/DyF3 composite magnets have been investigated. The results show that DyF3 milled in ethanol has much smaller particle size and more concentrated size distribution than that milled in argon and obtained flake and rice shapes. The DyF3 powders milled in ethanol for 0.5 h obtained the smallest average size of 1.16 mu m. The DyF3 powders milled in argon agglomerated and their particle sizes increased. The SmCo5/DyF3 magnets with DyF3 milled in ethanol had higher electrical resistivities than those samples with the same amounts of DyF3 unmilled and milled in argon and obtained the highest resistivity of 120 mu S2 center dot cm when the milling time in ethanol was 2 h. With the increase of the milling times, the remanences of the SmCo5/DyF3 magnets with DyF3 milled in argon increased firstly and then decreased, and their coercivities decreased, thus their maximum magnetic energy products, (BH)max, had little changes. When the milling time was 0.5 h, the (BH)max of the SmCo5/DyF3 magnet with DyF3 milled in ethanol increased to 6.43 MGOe. With further increase of the milling times of DyF3 in ethanol, the (BH)max of the SmCo5/DyF3 magnets decreased. The electrical resistivities of the SmCo5/DyF3 magnets increased monotonously with the increase of the DyF3 amounts, but the excessive amounts of the DyF3 additions led to the deterioration of the magnetic properties of the SmCo5/DyF3 magnets. When the doping amount was 11 wt%, the SmCo5/DyF3 magnets obtained the highest resistivity of 186 mu S2 center dot cm, which is 129 % higher than that of the undoped SmCo5 magnet (81 mu S2 center dot cm). Whilst its remanences and (BH)max decreased from 5.78 kGs, 7.71 MGOe to 5.01 kGs, 3.84 MGOe, respectively.
引用
收藏
页数:7
相关论文
共 50 条
  • [41] FRACTURE-TOUGHNESS ANISOTROPY OF A HOT-PRESSED AL2O3/SICW COMPOSITE
    BREDER, K
    GIANNAKOPOULOS, AE
    ZENG, K
    ROWCLIFFE, D
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1990, 9 (09) : 1085 - 1086
  • [42] Reaction hot-pressed sub-micro Al2O3+TiCceramic composite
    Chen, LM
    Kny, E
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2000, 18 (2-3): : 163 - 167
  • [43] Distinct Electrical and Mechanical Responses of a Cu-10Fe Composite Prepared by Hot-Pressed Sintering and Post Treatment
    Yue, X. Y.
    Peng, S. Y.
    Zhang, X.
    He, C. N.
    Tian, Y. Z.
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2024, 37 (02) : 255 - 265
  • [44] Distinct Electrical and Mechanical Responses of a Cu-10Fe Composite Prepared by Hot-Pressed Sintering and Post Treatment
    X. Y. Yue
    S. Y. Peng
    X. Zhang
    C. N. He
    Y. Z. Tian
    Acta Metallurgica Sinica (English Letters), 2024, 37 : 255 - 265
  • [45] 3D printed magnets with custom field geometry, produced using SmCo5/Fe exchange coupled nanocomposites
    Hirian, R.
    Bortnic, R.
    Popa, F.
    Gutoiu, S.
    Benea, D.
    Souca, G.
    Pop, V.
    CURRENT APPLIED PHYSICS, 2023, 51 : 39 - 43
  • [46] Effect of Different Mineralogical Proportions on the Electrical Conductivity of Dry Hot-Pressed Sintering Gabbro at High Temperatures and Pressures
    Wang, Mengqi
    Dai, Lidong
    Hu, Haiying
    Sun, Wenqing
    Hu, Ziming
    Jing, Chenxin
    MINERALS, 2022, 12 (03)
  • [47] Design of Glass Fiber-Doped High-Resistivity Hot-Pressed Permanent Magnets for Reducing Eddy Current Loss
    Guo, Yingjian
    Zhu, Minggang
    Wang, Ziliang
    Sun, Qisong
    Wang, Yu
    Li, Zhengxiao
    METALS, 2023, 13 (04)
  • [48] Electrical and mechanical properties of hot-pressed versus sintered LiTi2(PO4)3
    Wolfenstine, J.
    Allen, J. L.
    Sumner, J.
    Sakamoto, J.
    SOLID STATE IONICS, 2009, 180 (14-16) : 961 - 967
  • [49] Structure and magnetic properties of nanocrystalline SmCo5 and SmCo3Cu2 prepared by using high-pressure torsion method
    Wang, Fei-Yang
    Qi, Ting-Ting
    Wu, Qiong
    Ge, Hong-liang
    Si, Ping-Zhan
    AIP ADVANCES, 2024, 14 (01)