Axial Tensile Adhesively Bonded Performance of Carbon Fiber Composite Tubes Under Room-Temperature and Low-Temperature Circulation

被引:0
|
作者
Luo, Haibo [1 ,2 ]
Wang, Qian [2 ]
Yang, Yanchu [2 ]
Li, Tao [2 ]
Wu, Jun [2 ]
Gong, Wentao [2 ]
Feng, Hui [2 ]
He, Xiaohui [2 ]
机构
[1] Hainan Aerosp Informat Res Inst, Key Lab Earth Observat Hainan Prov, Wenchang 571300, Peoples R China
[2] Chinese Acad Sci, Aerosp Informat Res Inst, Beijing 100094, Peoples R China
基金
海南省自然科学基金;
关键词
composite circular tube; titanium alloy tube; thermal cycling (room-to-low-to-room-temperature); adhesive bonding performance; experimental study; SINGLE-LAP JOINTS; STRENGTH; FAILURE; STRESSES; ANGLE;
D O I
10.3390/ma18051124
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This study investigated the axial tensile performance of adhesively bonded T700/C204 carbon fiber composite and TC4 titanium alloy tubular single-lap joints under three distinct temperature conditions: room temperature, low temperature (-65 degrees C), and room-low-room-temperature cycling. Two configurations of adhesively bonded joints-composite-composite and composite-titanium-were tested. Specimens were designed to evaluate the influence of spew-fillet and perfect lap configurations on uniaxial tensile bonding strength across varying temperature environments. Analysis of the final failure morphology, stress concentration locations, ultimate failure loads, and load-displacement curves revealed that stress concentration and peeling stress were most pronounced at the ends of the bonded region, which served as the initiation points for failure. The adhesively bonded joints exhibited two distinct failure modes, strongly correlated with material properties and environmental temperature. The titanium alloy tubular joints predominantly experienced adhesive layer failure, while the carbon fiber three-way tubular joints were primarily characterized by fiber-tear failure. Environmental temperature significantly influenced the strength of the adhesively bonded joints. Specifically, the tensile failure limit of the bonded specimens subjected to low-temperature cycling (25 similar to-65 similar to 25 degrees C) was approximately 61% higher than that observed under the room or low-temperature conditions. Furthermore, the experimental results demonstrated that a maximum failure load of 27.522 kN and a shear strength of 10.956 MPa were achieved. Notably, the presence of adhesive spew-fillet had a negligible impact on the bonding strength of the joints.
引用
收藏
页数:17
相关论文
共 50 条
  • [31] Research on dynamic microwave low-temperature carbonization of high performance carbon fiber
    Zhao, Guozhen
    Zhang, Cheng
    Lv, Long
    Liu, Jianhua
    Guo, Shenghui
    DIAMOND AND RELATED MATERIALS, 2022, 125
  • [32] EFFECT OF LOW-TEMPERATURE STRAIN ON MECHANICAL-PROPERTIES OF CHROMIUM NICKEL STEELS AT ROOM-TEMPERATURE
    LEBEDEV, AA
    RUDENKO, VN
    KOVALCHUK, BI
    STRENGTH OF MATERIALS, 1983, 15 (09) : 1287 - 1290
  • [33] ROOM-TEMPERATURE FLUORESCENCE AND LOW-TEMPERATURE PHOSPHORESCENCE PROPERTIES OF BIPHENYL AND SOME POLYCHLORINATED-BIPHENYLS
    KHASAWNEH, IM
    WINEFORDNER, JD
    MICROCHEMICAL JOURNAL, 1988, 37 (01) : 86 - 92
  • [34] INVESTIGATIONS OF A NEW SAMPLE COMPARTMENT ASSEMBLY FOR LOW-TEMPERATURE AND ROOM-TEMPERATURE SOLID SUBSTRATE PHOSPHORIMETRY
    SCHARF, G
    SMITH, BW
    WINEFORDNER, JD
    ANALYTICAL CHEMISTRY, 1985, 57 (07) : 1230 - 1237
  • [35] SPECTROPHOSPHORIMETRIC ANALYSIS OF PESTICIDES - COMPARATIVE-STUDY OF PHOSPHORESCENCE CHARACTERISTICS AT LOW-TEMPERATURE AND ROOM-TEMPERATURE
    AARON, JJ
    WINEFORDNER, JD
    BULLETIN DE LA SOCIETE CHIMIQUE DE FRANCE PARTIE I-PHYSICOCHIMIE DES SYSTEMES LIQUIDES ELECTROCHIMIE CATALYSE GENIE CHIMIQUE, 1979, (9-10): : 355 - 356
  • [36] IMMOBILIZATION OF YEAST ON DELIGNIFIED CELLULOSIC MATERIAL FOR ROOM-TEMPERATURE AND LOW-TEMPERATURE WINE-MAKING
    BARDI, EP
    KOUTINAS, AA
    JOURNAL OF AGRICULTURAL AND FOOD CHEMISTRY, 1994, 42 (01) : 221 - 226
  • [37] Scanning Microwave Impedance Microscopy: Room-Temperature and Low-Temperature Applications for Device and Material Characterization
    Chintala, Ravi Chandra
    Rubin, Kurt
    Yang, Yongliang
    IEEE MICROWAVE MAGAZINE, 2020, 21 (10) : 22 - 35
  • [38] Effects of Temperature on Tensile Strength of Carbon fiber and Carbon/Epoxy Composite Sheets
    Cao, Shenghu
    Wu, Zhishen
    Li, Feng
    NEW MATERIALS AND PROCESSES, PTS 1-3, 2012, 476-478 : 778 - +
  • [39] Processing and properties of low-temperature cure carbon fiber-reinforced bismaleimide composite
    Waller, Matthew D.
    Bakis, Charles E.
    Koudela, Kevin L.
    McIntyre, Sean M.
    JOURNAL OF COMPOSITE MATERIALS, 2022, 56 (08) : 1191 - 1209
  • [40] Low-temperature resistance thermometers of carbon composite material
    Meshkovskii, I.K.
    Novikov, A.F.
    Sologub, V.V.
    Tatarinova, M.L.
    Instruments and experimental techniques New York, 1990, 32 (5 pt 2): : 1254 - 1255