Effect of Severe Plastic Deformation and Aging States on Microstructure and Mechanical Properties of 2024 Aluminum Alloy

被引:0
|
作者
Demirtas, Muhammet [1 ]
Yanar, Harun [2 ]
Uzun, Muhammet [2 ]
Ustalar, Melih [2 ]
Zhang, Zhenjun [3 ]
Dai, Renjie [3 ]
Jin, Jiewen [3 ]
Purcek, Gencaga [2 ]
机构
[1] Samsun Univ, Dept Aerosp Engn, TR-55420 Samsun, Turkiye
[2] Karadeniz Tech Univ, Dept Mech Engn, TR-61080 Trabzon, Turkiye
[3] Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Peoples R China
关键词
Al2024; alloys; mechanical properties; microstructural characterization; severe plastic deformation; WORK-HARDENING BEHAVIOR; CU-MG ALLOY; GRAIN-REFINEMENT; THERMAL-STABILITY; TENSILE DEFORMATION; AL-ALLOY; STRENGTH; PRECIPITATION; DUCTILITY; FRACTURE;
D O I
10.1002/adem.202402728
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al2024 aluminum alloy is subjected to equal channel angular pressing (ECAP) as severe plastic deformation in the quenched and overaged states to analyze the effect of different ECAP-based thermomechanical processes on microstructure and mechanical properties of the alloy. Application of ECAP process to both overaged and quenched samples brings about significant grain refinement in the microstructures. Aging the overaged + ECAPed sample at 180 degrees C for 24 h results in a partially aged (underaged) microstructure with GPB (Guinier-Preston-Bagaryatsky) zone, semicoherent S '', and S ' precipitates. Such a microstructural alteration is achieved in the quenched + ECAPed sample after aging at 100 degrees C for 7 h. 225 HV hardness as the highest hardness value reported in the Al2024 alloy subjected to thermomechanical processes including ECAP and aging steps is achieved after aging the quenched + ECAPed sample at 100 degrees C for 7 h. For both cases (overaged + ECAP and quenched + ECAP), strength-plasticity matching is achieved in the ECAP + underaged state where the microstructure consists of GPB zones, semicoherent S '', and S ' precipitates rather than incoherent S precipitates. Such a strength-plasticity matching is attributed to the planar slip in the underaged samples rather than cross-slip that occurs in the overaged samples.
引用
收藏
页数:12
相关论文
共 50 条
  • [1] Effects of aging on mechanical properties of 2024 aluminum alloy by severe cold plastic deformation
    Ning, Ailin
    Liu, Zhiyi
    Zeng, Sumin
    Tezhong Zhuzao Ji Youse Hejin/Special Casting and Nonferrous Alloys, 2006, 26 (08): : 529 - 531
  • [2] Effect of severe plastic deformation on mechanical properties and microstructure in 7075 aluminum alloy
    Kuramoto, Shigeru
    Horibuchi, Kayo
    Aoi, Ichiro
    Oh-Ishi, Keiichiro
    Keikinzoku/Journal of Japan Institute of Light Metals, 2014, 64 (06): : 241 - 248
  • [3] Natural Aging of Aluminum Alloy 2024 After Severe Plastic Deformation
    Irina Volokitina
    Andrey Bychkov
    Andrey Volokitin
    Alexandr Kolesnikov
    Metallography, Microstructure, and Analysis, 2023, 12 : 564 - 566
  • [4] Natural Aging of Aluminum Alloy 2024 After Severe Plastic Deformation
    Volokitina, Irina
    Bychkov, Andrey
    Volokitin, Andrey
    Kolesnikov, Alexandr
    METALLOGRAPHY MICROSTRUCTURE AND ANALYSIS, 2023, 12 (03) : 564 - 566
  • [5] Aging behavior and mechanical properties of 6013 aluminum alloy processed by severe plastic deformation
    Liu, Man-ping
    Jiang, Ting-hui
    Wang, Jun
    Liu, Qiang
    Wu, Zhen-jie
    Yu, Ying-da
    Skaret, Pal C.
    Roven, Hans J.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2014, 24 (12) : 3858 - 3865
  • [6] Effect of Deformation on Microstructure, Texture and Properties of 2024 Aluminum Alloy
    Haigen, Jian
    Man, Yang
    Miao, Chen
    Kemou, Xiao
    METALLOGRAPHY MICROSTRUCTURE AND ANALYSIS, 2024, 13 (03) : 364 - 375
  • [7] Microstructure evolution and hardening behavior of 2024 aluminum alloy processed by the severe plastic deformation
    Kang, SB
    Lim, CY
    Kim, HW
    Mao, JF
    ALUMINUM ALLOYS 2002: THEIR PHYSICAL AND MECHANICAL PROPERTIES PTS 1-3, 2002, 396-4 : 1163 - 1168
  • [8] Characterization of the microstructure, texture and mechanical properties of 7075 aluminum alloy in early stage of severe plastic deformation
    Moghaddam, M.
    Zarei-Hanzaki, A.
    Pishbin, M. H.
    Shafieizad, A. H.
    Oliveira, V. B.
    MATERIALS CHARACTERIZATION, 2016, 119 : 137 - 147
  • [9] Effect of Artificial Aging on the Mechanical Properties of an Aerospace Aluminum Alloy 2024
    Reis, D. A. P.
    Couto, A. A.
    Domingues, N. I., Jr.
    Hirschmann, A. C. O.
    Zepka, S.
    Moura Neto, C.
    DIFFUSION IN SOLIDS AND LIQUIDS VII, 2012, 326-328 : 193 - +
  • [10] Microstructure and mechanical properties of a biomedical β-type titanium alloy subjected to severe plastic deformation after aging treatment
    Yilmazer, H.
    Niinomi, M.
    Nakai, M.
    Hieda, J.
    Akahori, T.
    Todaka, Y.
    MATERIALS INTEGRATION, 2012, 508 : 152 - +