Natural Aging of Aluminum Alloy 2024 After Severe Plastic Deformation

被引:11
|
作者
Volokitina, Irina [1 ]
Bychkov, Andrey [2 ]
Volokitin, Andrey [3 ]
Kolesnikov, Alexandr [4 ]
机构
[1] Rudny Ind Inst, 50 Let Oktyabrya Str 38, Rudny 111500, Kazakhstan
[2] Lomonosov Moscow State Univ, Leninskie Gory GSP 1, Moscow 119234, Russia
[3] Karaganda Ind Univ, Republ Ave 30, Temirtau 101400, Kazakhstan
[4] M Auezov South Kazakhstan Univ, Ave Tauke Khan,5, Shymkent 160012, Kazakhstan
关键词
Aluminum alloy; Severe plastic deformation; High-pressure torsion; Microstructure; Aging;
D O I
10.1007/s13632-023-00966-y
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
This paper provides a laboratory-level evaluation of the cryogenic strain potential of aluminum alloy 2024 after severe plastic deformation by equal channel angular pressing method. Characteristics of the samples were determined by transmission electron microscopy, tensile tests and microhardness determination. Natural aging at room temperature for 24 days resulted in a change in the microhardness of aluminum samples. Thus, in samples strained at room temperature, the decrease in microhardness occurs by 250 MPa and in samples strained at a cryogenic temperature by 110 MPa. This can be explained by return processes which improve the characteristics of plasticity. As a result, a thermo-mechanical treatment mode was developed for aluminum alloy, including quenching, straining by equal channel angular pressing at liquid nitrogen temperature, followed by natural aging, which allows to obtain samples with certain parameters of structural strength of the alloy.
引用
下载
收藏
页码:564 / 566
页数:3
相关论文
共 50 条
  • [1] Natural Aging of Aluminum Alloy 2024 After Severe Plastic Deformation
    Irina Volokitina
    Andrey Bychkov
    Andrey Volokitin
    Alexandr Kolesnikov
    Metallography, Microstructure, and Analysis, 2023, 12 : 564 - 566
  • [2] On the natural aging behavior of Aluminum 6061 alloy after severe plastic deformation
    Farshidi, M. H.
    Kazeminezhad, M.
    Miyamoto, H.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2013, 580 : 202 - 208
  • [3] Effects of aging on mechanical properties of 2024 aluminum alloy by severe cold plastic deformation
    Ning, Ailin
    Liu, Zhiyi
    Zeng, Sumin
    Tezhong Zhuzao Ji Youse Hejin/Special Casting and Nonferrous Alloys, 2006, 26 (08): : 529 - 531
  • [4] Flow stress of 2024 aluminum alloy during multi-directional forging process and natural aging after plastic deformation
    Nouri, Sasan
    Kazeminezhad, Mohsen
    Shadkam, Ashkan
    MATERIALS CHEMISTRY AND PHYSICS, 2020, 254
  • [5] Aging behavior of aluminum alloys after severe plastic deformation
    Horita, Zenji
    ALUMINIUM ALLOYS 2006, PTS 1 AND 2: RESEARCH THROUGH INNOVATION AND TECHNOLOGY, 2006, 519-521 : 1485 - 1492
  • [6] Microstructure evolution and hardening behavior of 2024 aluminum alloy processed by the severe plastic deformation
    Kang, SB
    Lim, CY
    Kim, HW
    Mao, JF
    ALUMINUM ALLOYS 2002: THEIR PHYSICAL AND MECHANICAL PROPERTIES PTS 1-3, 2002, 396-4 : 1163 - 1168
  • [7] Aging behavior and mechanical properties of 6013 aluminum alloy processed by severe plastic deformation
    Liu, Man-ping
    Jiang, Ting-hui
    Wang, Jun
    Liu, Qiang
    Wu, Zhen-jie
    Yu, Ying-da
    Skaret, Pal C.
    Roven, Hans J.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2014, 24 (12) : 3858 - 3865
  • [8] Change of anisotropic tensile strength due to amount of severe plastic deformation in aluminum 2024 alloy
    Ma, Young Wha
    Choi, Jeong Woo
    Yoon, Kee Bong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 529 : 1 - 8
  • [9] Effect of plastic deformation on the precipitation sequence of 2024 aluminum alloy
    J. C. Guía-Tello
    C. G. Garay-Reyes
    G. Rodríguez-Cabriales
    H. M. Medrano-Prieto
    M. A. Ruiz-Esparza-Rodríguez
    L. J. García Hernández
    J. M. Mendoza-Duarte
    K. A. García-Aguirre
    I. Estrada-Guel
    S. González
    R. Martínez-Sánchez
    Journal of Materials Science, 2022, 57 : 2180 - 2193
  • [10] Effect of plastic deformation on the precipitation sequence of 2024 aluminum alloy
    Guia-Tello, J. C.
    Garay-Reyes, C. G.
    Rodriguez-Cabriales, G.
    Medrano-Prieto, H. M.
    Ruiz-Esparza-Rodriguez, M. A.
    Garcia Hernandez, L. J.
    Mendoza-Duarte, J. M.
    Garcia-Aguirre, K. A.
    Estrada-Guel, I
    Gonzalez, S.
    Martinez-Sanchez, R.
    JOURNAL OF MATERIALS SCIENCE, 2022, 57 (03) : 2180 - 2193