Improving the wear resistance and scratch adhesion strength of TiAlN coatings via Al incorporation

被引:0
|
作者
Akhter, Rumana [1 ,2 ]
Bendavid, Avi [1 ,3 ]
Munroe, Paul [1 ]
机构
[1] Univ New South Wales, Sch Mat Sci & Engn, Sydney, NSW 2052, Australia
[2] Univ New South Wales, Electron Microscope Unit, Sydney, NSW 2052, Australia
[3] CSIRO Mfg, Lindfield, NSW 2070, Australia
基金
澳大利亚研究理事会;
关键词
Titanium aluminium nitride; Coating; Macroparticles; Microstructure; Mechanical properties; Wear resistance; Scratch adhesion strength; NITROGEN PARTIAL-PRESSURE; N THIN-FILMS; TRIBOLOGICAL PROPERTIES; HARD COATINGS; OXIDATION RESISTANCE; THERMAL-STABILITY; ELASTIC-MODULUS; ARC DEPOSITION; SUBSTRATE BIAS; TIN;
D O I
10.1016/j.tsf.2025.140650
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The inclusion of Al into the binary TiN crystal structure may impose a significant influence on the tribological properties of titanium aluminium nitride (TiAlN) coatings. In this study, a suite of TiAlN coatings, with different Al concentrations, were deposited onto tool steel substrates through variation in the composition of the Ti-Al cathode using the cathodic arc evaporation process. The primary objective of this investigation was to explore the wear and scratch response of TiAlN coatings, in particular, the underlying deformation mechanisms of these coatings under cyclical or progressive loading. The maximum nanohardness (similar to 34.5 GPa) was realised in the film containing the lowest Al concentration (similar to 20 at. %), which was attributed to Hall-Petch effects, as well as the effects of solid solution hardening. The wear resistance of these coatings exhibits an inverse relationship with the Al content and was noted to be consistent with the hardness and modulus of these coatings. Enhanced scratch adhesion strength, as defined by higher L-C1, L-C2 and CPR values, was also observed for the TiAlN coating with the lowest Al concentration (similar to 20 at. %), consistent with its higher H/E-r and H-3/E-r(2) ratios, promoting good resistance against adhesive and cohesive failures. In addition, the failure modes under progressive loading were found to be influenced by the geometry and density of macroparticles, arising from the deposition process, accompanied by the residual stresses of the coatings and the hierarchical architecture of these thin film systems.
引用
收藏
页数:18
相关论文
共 50 条
  • [41] Influence of the modes of laser cladding on bond strength and wear resistance of coatings
    Birukov, V. P.
    Tatarkin, D. Yu
    Chriptovish, E. V.
    Fichkov, A. A.
    III INTERNATIONAL CONFERENCE ON LASER AND PLASMA RESEARCHES AND TECHNOLOGIES, 2018, 941
  • [42] Effects of Al content in TiAlN coatings on tool wear and cutting temperature during dry machining IN718
    Zhao, Jinfu
    Liu, Zhanqiang
    Wang, Bing
    Song, Qinghua
    Ren, Xiaoping
    Wan, Yi
    TRIBOLOGY INTERNATIONAL, 2022, 171
  • [43] Improving the wear resistance of Al–Si alloy by ion implantation
    Y. Itoh
    H. Azuma
    A. Itoh
    T. Hioki
    Journal of Materials Research, 1997, 12 : 3246 - 3249
  • [44] Study on adhesion and wear resistance of multi-element (AlCrTaTiZr)N coatings
    Cheng, Keng-Hao
    Weng, Chih-Hui
    Lai, Chia-Han
    Lin, Su-Jien
    THIN SOLID FILMS, 2009, 517 (17) : 4989 - 4993
  • [45] The hardness, adhesion and wear resistance of coatings developed for cobalt-base alloys
    Cockeram, BV
    Wilson, WL
    SURFACE & COATINGS TECHNOLOGY, 2001, 139 (2-3): : 161 - 182
  • [46] Nanomechanical behavior, adhesion and wear resistance of tin oxide coatings for biomedical applications
    Chayoukhi, S.
    Gassoumi, B.
    Dhifelaoui, H.
    Boukhachem, A.
    Amlouk, M.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2024, 55 (04) : 427 - 436
  • [47] Effect of mechanical properties measured at room and elevated temperatures on the wear resistance of cutting tools with TiAlN and AlCrN coatings
    Fox-Rabinovich, GS
    Beake, BD
    Endrino, JL
    Veldhuis, SC
    Parkinson, R
    Shuster, LS
    Migranov, MS
    SURFACE & COATINGS TECHNOLOGY, 2006, 200 (20-21): : 5738 - 5742
  • [48] Improving scratch-resistance and wear-resistance of VN film by deep cryogenic treatment with liquid nitrogen
    Cai, Zhaobing
    Chen, Ran
    Qian, Jianguo
    Zheng, Shujing
    Chen, Shengyu
    Pu, Jibin
    SURFACE ENGINEERING, 2020, 36 (02) : 206 - 215
  • [49] WEAR- AND HEAT RESISTANCE OF VACUUM-ARC TiN AND TiAlN BASED COATINGS WITH Si AND Y ADDITIVES
    Aksenov, I. I.
    Belous, V. A.
    Grigor'ev, A. N.
    Ermolenko, I. G.
    Zadneprovskiy, Yu. A.
    Kovalenko, V. I.
    Lomino, N. S.
    Marinin, V. G.
    Sobol', O. V.
    Tolmachyova, G. N.
    PROBLEMS OF ATOMIC SCIENCE AND TECHNOLOGY, 2011, (04): : 169 - 173
  • [50] Investigation of high temperature wear resistance of TiCrAlCN/TiAlN multilayer coatings over M2 steel
    Sukuroglu, E. E.
    Baran, O.
    Totik, Y.
    Efeoglu, I.
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2018, 32 (13) : 1428 - 1436