CVD-grown SiC nanowires-reinforced SiC coating on C/C composites: Focusing on antioxidation, thermal shock and high-temperature gas erosion resistance

被引:0
|
作者
Qiang, Xinfa [1 ]
Dong, Maoheng [1 ]
Chen, Xiangyu [1 ]
Yang, Zi [1 ]
Zhai, Hengxiang [1 ]
Wu, Chao [1 ]
Tian, Song [2 ]
机构
[1] Nanjing Inst Technol, Jiangsu Key Lab Adv Struct Mat & Applicat Technol, Nanjing 211167, Peoples R China
[2] Chongqing Jiaotong Univ, Sch Mat Sci & Engn, Chongqing 400074, Peoples R China
来源
基金
中国国家自然科学基金;
关键词
SiC nanowires; Mechanical property; Antioxidation; Thermal shock; Gas erosion; OXIDATION PROTECTION; CARBON/CARBON COMPOSITES; MECHANICAL-PROPERTIES; FABRICATION; DEPOSITION;
D O I
10.1016/j.surfcoat.2024.131584
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
To improve the oxidation resistance of C/C composites, a SiCNWs-reinforced SiC (SiCNWs-SiC) coating was successfully fabricated in-situ by a simple chemical vapor deposition (CVD) process on C/C composites. Microstructural analysis revealed uniform beta-SiCNWs with diameters of 50-200 nm and lengths up to tens of micrometers. The thickness of porous SiCNWs layer is approximately 300 mu m. Elevated deposition temperatures deteriorated coating density, with optimal performance at 1373 K. The SiCNWs enhanced deposition efficiency, boosting bending strength from 107.2 MPa to 134.3 MPa and adhesion strength from 6.74 MPa to 14.18 MPa. Oxidation resistance tests at various temperatures confirmed superior performance of SiCNWs-toughened SiC coatings. Thermal shock tests showed minimal weight loss (2.5 %) after 30 cycles, outperforming pure SiC coatings (6.2 %). The 1873 K gas erosion test showed that the weight loss of the SiCNWs-SiC coated C/C samples was only 5.2 % for 53 h, while the pure CVD-SiC coated C/C composite samples broke after 19 h of gas erosion, and the weight loss of pure C/C composite samples reached as high as 38.5 % after 1.3 h of gas erosion.
引用
收藏
页数:16
相关论文
共 50 条
  • [41] Strengthened high-temperature resistance in B 4 C/SiC/2024Al composite via SiC nanowires pinning grain boundary
    Hua, Andong
    Su, Yishi
    Cai, Yunpeng
    Zhang, Di
    Ouyang, Qiubao
    JOURNAL OF ALLOYS AND COMPOUNDS, 2024, 1000
  • [42] Bamboo like SiC Nanowires Grown in a Dual-Temperature Zone Reaction System Enhance the Oxidation and Thermal Shock Resistance of SiC Coatings
    Binbin Li
    Xingbang Wang
    Bangxiao Mao
    Tao He
    Haiquan Huang
    Xiaosen Yuan
    Applied Composite Materials, 2021, 28 : 1 - 15
  • [43] Bamboo like SiC Nanowires Grown in a Dual-Temperature Zone Reaction System Enhance the Oxidation and Thermal Shock Resistance of SiC Coatings
    Li, Binbin
    Wang, Xingbang
    Mao, Bangxiao
    He, Tao
    Huang, Haiquan
    Yuan, Xiaosen
    APPLIED COMPOSITE MATERIALS, 2021, 28 (01) : 1 - 15
  • [44] Oxidation behavior and strength degradation of CVD-SiC coated C/C composites at high temperature in air
    Kobayashi, S
    Wakayama, S
    Aoki, T
    Hatta, H
    ADVANCED COMPOSITE MATERIALS, 2003, 12 (2-3) : 171 - 183
  • [45] Industrial Preparation of SiC Ceramic Coating for High Temperature and Anti-oxidation of C/C Composites
    Fan, Zimin
    Fan, Huiqing
    Wang, Xiaogang
    MANUFACTURING PROCESS TECHNOLOGY, PTS 1-5, 2011, 189-193 : 147 - +
  • [46] Improvement of ablation resistance of CVD-HfC/SiC coating on hemisphere shaped C/C composites by introducing diffusion interface
    Tong, Mingde
    Fu, Qiangang
    Hu, Dou
    Zhou, Lei
    Feng, Tao
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2021, 41 (07) : 4067 - 4075
  • [47] Preparation and properties of C/SiC composites reinforced by high thermal conductivity graphite films
    Zhao, Jiajia
    Cai, Rong
    Ma, Zhaokun
    Zhang, Kaixuan
    Liang, Hengliang
    Qiu, Haipeng
    Liu, Shanhua
    Xie, Weijie
    DIAMOND AND RELATED MATERIALS, 2021, 116
  • [48] Preparation and properties of C/SiC composites reinforced by high thermal conductivity graphite films
    Zhao, Jiajia
    Cai, Rong
    Ma, Zhaokun
    Zhang, Kaixuan
    Liang, Hengliang
    Qiu, Haipeng
    Liu, Shanhua
    Xie, Weijie
    Diamond and Related Materials, 2021, 116
  • [49] SiC fiber strengthened Si-14Ti high-temperature filler alloy for brazing SiCf/SiC and C/C composites
    He, Zongjing
    Xu, Huining
    Yuan, Jie
    Li, Chun
    Zhang, Chenghao
    Cao, Jian
    MATERIALS CHARACTERIZATION, 2024, 207
  • [50] High-temperature reactions of C/C-SiC composites with precursor-derived ceramic coatings
    Wagner, S
    Seifert, HJ
    Aldinger, F
    MATERIALS AND MANUFACTURING PROCESSES, 2002, 17 (05) : 619 - 635