Microstructural Insights into Solid Particle Erosion in a High-Chromium Cast Iron

被引:0
|
作者
Suman, Alessio [1 ]
Fortini, Annalisa [1 ]
Zanini, Nicola [1 ]
机构
[1] Univ Ferrara, Dept Engn, I-44122 Ferrara, Italy
关键词
high-chromium cast irons; solid particle erosion; carbide volume fraction; impact velocity; image analysis; erosion rate; WEAR BEHAVIOR; RESISTANCE; VELOCITY; MOLYBDENUM; IMPACT; SIZE;
D O I
10.3390/met15010006
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Solid particle erosion (SPE) significantly limits the service life of High-Chromium Cast Irons (HCCIs), widely used in power generation and mining industries. This study investigates how microstructural features influence the erosion resistance of a Fe-Cr-C cast iron, focusing on the interplay between particle kinetic energy and carbide features, i.e., carbide volume fraction (CVF). Erosion tests, conducted per ASTM G76 standards, revealed that substrates with similar CVFs exhibited varying damage levels, even at consistent particle kinetic energies. The findings underscored that impact conditions have a greater influence on erosion resistance than CVF alone, emphasizing the critical role of carbide morphology and distribution in mitigating damage. This work provides valuable insights for optimizing HCCIs to enhance material performance and durability in demanding erosive environments by tailoring carbide distribution to specific operational conditions.
引用
收藏
页数:11
相关论文
共 50 条
  • [21] Effects of solidification conditions on the microstructural morphologies and strengths of hypereutectic high-chromium white cast iron castings
    Goto, Ikuzo
    Fukuchi, Kohei
    Kurosawa, Kengo
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2023, 886
  • [22] SLURRY SPEED DEPENDENCE OF SAND-EROSION RATE IN HIGH-CHROMIUM WHITE CAST-IRON
    ASO, S
    SUGAWARA, T
    TAGAMI, M
    GOTO, S
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1993, 57 (03) : 312 - 319
  • [23] Effect of titanium on the microstructure of hypereutectic high-chromium cast iron
    Zhi Xiaohui
    Han Yanjun
    Peng Jiyun
    Xing Handong
    Gao Yimin
    RARE METAL MATERIALS AND ENGINEERING, 2008, 37 (01) : 101 - 104
  • [24] The particle size effect on abrasive wear of high-chromium white cast iron mill balls
    Pintaude, G
    Tschiptschin, AP
    Tanaka, DK
    Sinatora, A
    WEAR, 2001, 250 : 66 - 70
  • [25] Refining Effect of Nb on Hypereutectic High-Chromium Cast Iron
    Zhi Xiaohui
    Han Yanjun
    Xing Jiandong
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 : 169 - 171
  • [26] Relation between the microstructure and properties of high-chromium cast iron
    Komarov, OS
    Sadovskii, VM
    Urbanovich, NI
    Grigor'ev, SV
    METAL SCIENCE AND HEAT TREATMENT, 2003, 45 (7-8) : 259 - 262
  • [27] PHASE COMPOSITION OF HIGH-CHROMIUM WHITE CAST-IRON
    PASKAL, YI
    BERKUN, MN
    SHOLOKHOVA, LV
    PASKAL, AS
    ZHIVITSA, IV
    METAL SCIENCE AND HEAT TREATMENT, 1977, 19 (11-1) : 1068 - 1071
  • [28] Relation Between the Microstructure and Properties of High-Chromium Cast Iron
    O. S. Komarov
    V. M. Sadovskii
    N. I. Urbanovich
    S. V. Grigor'ev
    Metal Science and Heat Treatment, 2003, 45 : 259 - 262
  • [29] Refining Mechanism of Ti on Hypereutectic High-Chromium Cast Iron
    Zhi Xiaohui
    Han Yanjun
    Xing Jiandong
    Fu Hanguang
    RARE METAL MATERIALS AND ENGINEERING, 2011, 40 : 237 - 240
  • [30] Effect of impingement angle on slurry erosion behaviour and mechanisms of 1017 steel and high-chromium white cast iron
    Al-Bukhaiti, M. A.
    Ahmed, S. M.
    Badran, F. M. F.
    Emara, K. M.
    WEAR, 2007, 262 (9-10) : 1187 - 1198