Effects of Hot-pressing Parameters on the Properties of Waste Tetra Pak/Bamboo Composites

被引:0
|
作者
Jiang, Rui [1 ]
Xu, Yuan Fei
Yang, Xue Jian [2 ]
Zhang, Lei [1 ]
Fan, Zhen Yu [1 ]
Guo, Xiao Yan [1 ]
Guo, Hui [3 ]
Qing, Bin [3 ,4 ]
Li Yu, Li [3 ,4 ]
机构
[1] China Natl Tobacco Corp, Yunnan Prov Branch, Kunming 650000, Yunnan, Peoples R China
[2] Dali Tobacco Co, Dali 671000, Yunnan, Peoples R China
[3] Tianjin Univ Sci & Technol, Tianjin Key Lab Pulp & Paper, Tianjin 300457, Peoples R China
[4] Tianjin Univ Sci & Technol, Inst Carbon Neutral, Tianjin 300222, Peoples R China
来源
BIORESOURCES | 2025年 / 20卷 / 01期
关键词
Waste Tetra Pak; Hot pressing parameters; Orthogonal test; Strength property; Dimensional stability; MECHANICAL-PROPERTIES;
D O I
10.15376/biores.20.1.826-841
中图分类号
TB3 [工程材料学]; TS [轻工业、手工业、生活服务业];
学科分类号
0805 ; 080502 ; 0822 ;
摘要
Waste Tetra Pak containers, from the same brand of milk, were crushed into fibers. They were formed into composites with 40-mesh bamboo fibers with phenolic resin and hot pressed with different parameters. The effects of hot-pressing temperature, hot-pressing time, hot-pressing pressure, phenolic resin amount, and the ratio of Tetra Pak and bamboo on the elastic modulus, static bending strength, internal adhesive bonding strength, and 24 h thickness swelling rate of the composites were investigated by orthogonal testing. The results showed that during the hot- pressing process, hot-pressing temperature was the most important factor for the elastic modulus and static bending strength of the composites and the hot-pressing pressure was the most important factor for the 24 h thickness swelling of the composites. Optimal hot-pressing parameters of TP/bamboo composites were a hot-pressing temperature of 180 degrees C, hot- pressing time of 16 min, hot-pressing pressure of 1.0 MPa, phenolic resin amount of 12%, and ratio of Tetra Pak/bamboo of 9:1, in which the least phenolic resin and the most Tetra Pak materials were added. Moreover, the elastic modulus was 7670 MPa, the bending strength was 40 MPa, the internal adhesive bonding strength was 0.86 MPa, and 24 h thickness swelling rate was 10.6%, meeting the requirements for MDF in different states.
引用
收藏
页码:826 / 841
页数:16
相关论文
共 50 条
  • [41] Mechanical and tribological properties of alumina-MWCNTs composites sintered by rapid hot-pressing
    Hanzel, Ondrej
    Lofaj, Frantisek
    Sedlacek, Jaroslav
    Kabatova, Margita
    Tatarkova, Monika
    Sajgalik, Pavol
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2017, 37 (15) : 4821 - 4831
  • [42] Processing and Properties of ZrB2-Cu Composites Sintered by Hot-pressing Sintering
    Shang, Wei
    Wang, Hailong
    Zhao, Shijing
    Zhao, Xiaotong
    Xu, Hongliang
    Lu, Hongxia
    Chen, Deliang
    Fan, Bingbing
    Zhang, Rui
    HIGH-PERFORMANCE CERAMICS VIII, 2014, 602-603 : 447 - 450
  • [43] Mechanical and tribological properties of NiAl–NbC–Ag composites prepared by hot-pressing sintering
    Xiaochun Feng
    Junhong Jia
    Wenzhen Wang
    Yu Shan
    Journal of Materials Research, 2017, 32 : 2361 - 2372
  • [44] Mechanical properties of aluminide matrix composites fabricated by reactive hot-pressing in several environments
    Inoue, M
    Suganuma, K
    Nichara, K
    INTERMETALLICS, 2000, 8 (9-11) : 1035 - 1042
  • [45] STRUCTURE AND SUPERCONDUCTING PARAMETERS OF COMPOSITES YBACUO-AG PREPARED BY STATIC, DYNAMIC AND HOT-PRESSING
    DOTSENKO, VI
    BRAUDE, IS
    IVANCHENKO, LG
    KISLYAK, IG
    PUZANOVA, AD
    IEEE TRANSACTIONS ON APPLIED SUPERCONDUCTIVITY, 1995, 5 (02) : 1456 - 1458
  • [46] Solidification of waste containing sodium borate by hydrothermal hot-pressing
    Yamasaki, Nakamichi
    Yanagisawa, Kazumichi
    Kinoshita, Koki
    Kashiwai, Toshihiko
    Nippon Genshiryoku Gakkaishi/Journal of the Atomic Energy Society of Japan, 1988, 30 (08): : 714 - 724
  • [47] HOT-PRESSING OF FACE BRICK .3. PRESSING PARAMETERS FOR QUALITY PRODUCTS
    BROWNELL, WE
    MCMANN, FC
    JANG, SD
    AMERICAN CERAMIC SOCIETY BULLETIN, 1974, 53 (05): : 440 - 442
  • [48] PROCESS CONSIDERATIONS FOR HOT-PRESSING CERAMIC NUCLEAR WASTE FORMS
    WILSON, CN
    BRITE, DW
    AMERICAN CERAMIC SOCIETY BULLETIN, 1981, 60 (03): : 418 - 418
  • [49] GRAPHITE AND BORON-CARBIDE COMPOSITES MADE BY HOT-PRESSING
    MIYAZAKI, K
    HAGIO, T
    KOBAYASHI, K
    JOURNAL OF MATERIALS SCIENCE, 1981, 16 (03) : 752 - 762
  • [50] Study on FeAl/TiC composites fabricated by reactive hot-pressing
    Liu, FX
    Yong, L
    Huang, BY
    Zhou, KC
    He, YH
    RARE METAL MATERIALS AND ENGINEERING, 2004, 33 (06) : 127 - 131