Effect of vanadium on stress corrosion cracking for high-strength railway steel in simulated SO2-polluted environment

被引:0
|
作者
Wang, Shuoyang [1 ]
Zhou, Yiqi [1 ,2 ]
Liu, Yikun [1 ]
Yue, Zhanshu [1 ]
Huang, Yunhua [1 ,3 ]
Li, Xiaogang [1 ,2 ,3 ]
机构
[1] Univ Sci & Technol Beijing, Inst Adv Mat & Technol, Key Lab Corros & Protect, Minist Educ, Beijing, Peoples R China
[2] Univ Sci & Technol Beijing, Inst Adv Mat & Technol, Beijing Adv Innovat Ctr Mat Genome Engn, Beijing, Peoples R China
[3] Univ Sci & Technol Beijing, Natl Mat Corros & Protect Data Ctr, Beijing, Peoples R China
关键词
Railway steel; Vanadium; Stress corrosion cracking; Anodic dissolution; Hydrogen embrittlement; STRAIN-GRADIENT PLASTICITY; LOW-ALLOY STEEL; BEHAVIOR; MICROSTRUCTURE; HYDROGEN; PEARLITE; TRANSFORMATION; DISSOLUTION; MECHANISM; FERRITE;
D O I
10.1016/j.matchemphys.2025.130680
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Railway steel plays critical role in railway tracks, which influences the safety of this system. In this work, the effect of vanadium on the SCC under anodic dissolution (AD) and hydrogen embrittlement (HE) mode of railway steel is investigated. A high-strength railway steel is alloyed with 0.08 wt % vanadium and compared with the original steel. The results indicate that adding V reduces the galvanic effect between phases in the railway steel, then decreases the general corrosion rate, and retards the formation of localized corrosion, which is the crack source. Therefore, V reduces the AD-SCC risk from the elongation loss of railway steel from 69.6 % to 44.5 % under open circuit potential (OCP) conditions. Additionally, V refines the interlamellar spacing of pearlite, resulting in a longer length between ferrite and cementite, which is a hydrogen storage site. Therefore, the elongation loss at a hydrogen evolution potential is 82.6 % for the railway steel containing V, which is 5.4 % lower than steel without V, indicating V improve the HE-SCC resistance. Overall, V exhibits a reduced risk of ADSCC, characterized by a lower likelihood of localized corrosion initiation and slower corrosion propagation rates. Furthermore, it offers an increased number of hydrogen trap sites, which help prevent the accumulation of high hydrogen concentrations within the material, ultimately enhancing its resistance to HE-SCC.
引用
收藏
页数:12
相关论文
共 50 条
  • [41] 2 TYPES OF KINETICS OF CORROSION CRACKING OF A HIGH-STRENGTH STEEL WITH A MARTENSITIC STRUCTURE
    KRUPIN, YA
    KISELEV, IK
    SOVIET MATERIALS SCIENCE, 1990, 26 (05): : 521 - 523
  • [43] EFFECT OF COLD WORK ON SULFIDE STRESS CRACKING OF HIGH-STRENGTH TUBULAR STEEL
    MCKENZIE, KA
    BRADFORD, SA
    CIM BULLETIN, 1987, 80 (902): : 86 - 86
  • [44] Stress Corrosion Cracking of High-Strength Maraging Steels.
    Prikrylova, Marcela
    Hutnicke Listy, 1977, 32 (02): : 116 - 120
  • [45] STRESS-CORROSION CRACKING CRITERIA FOR HIGH-STRENGTH STEELS
    KARLINSKI, W
    SZACHNOWSKI, W
    BRITISH CORROSION JOURNAL, 1995, 30 (02): : 116 - 118
  • [46] Corrosion fatigue cracking behaviors of Q690qE high-strength bridge steel as a weld joint in simulated marine environment
    Lu, Cuiping
    Yao, Qiong
    Li, Ningning
    Sun, Liyang
    Dai, Wenhe
    Zhang, Chuang
    Ma, Hongchi
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2024, 47 (11) : 4341 - 4355
  • [47] Cathodic and Anodic Stress Corrosion Cracking of a New High-Strength CrNiMnMoN Austenitic Stainless Steel
    Truschner, Mathias
    Deutsch, Jacqueline
    Mori, Gregor
    Keplinger, Andreas
    METALS, 2020, 10 (11) : 1 - 12
  • [48] ENHANCING THE STRESS-CORROSION CRACKING RESISTANCE OF HIGH-STRENGTH STEEL KH13
    ZHIGACHEVA, NI
    NAZAROV, AA
    PROTECTION OF METALS, 1983, 19 (04): : 446 - 451
  • [49] INFLUENCES OF VIBRATORY STRESSES ON INITIATION BEHAVIOR OF STRESS-CORROSION CRACKING IN A HIGH-STRENGTH STEEL
    KOMAI, K
    MINOSHIMA, K
    FUJITO, T
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1984, 48 (03) : 307 - 313
  • [50] STRESS-CORROSION CRACKING IN HIGH-STRENGTH STEEL UNDER MODE-III LOADING
    CHU, WY
    HSIAO, CM
    XU, BJ
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1986, 17 (04): : 711 - 716