Kinetic model for the generation and accumulation of Al2O3 in mold flux during the continuous casting of a Fe-Al-Mn-C steel

被引:0
|
作者
Mo, Rongzhen [1 ]
Zhang, Chihao [1 ]
Ren, Ying [1 ]
Zhang, Lifeng [2 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[2] North China Univ Technol, Sch Mech & Mat Engn, Beijing 100144, Peoples R China
关键词
Fe-Al-Mn-C steel; Kinetic model; Mold flux; Continuous casting; ALUMINUM; SLAGS; BEHAVIOR;
D O I
10.1016/j.jmrt.2025.02.146
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The relationship between temperature and Al mass transfer coefficient through experiments was established. A kinetic model was developed to predict the generation and accumulation of Al2O3 in mold flux during the continuous casting of the Fe-Al-Mn-C steel. The model aimed to adjust casting conditions, optimizing the actual property of Fe-Al-Mn-C steel. There were three main influence factors of Al2O3 evolution in the mold flux during the continuous casting of Fe-Al-Mn-C steels was considered, including the reaction between steels and mold fluxes, the consumption of the mold flux, and the addition of the mold flux. The accuracy of the model was validated using plant data from the casting of Fe-2%Al-23%Mn-0.17%C steel with 40% SiO2 mold flux as well as the casting of Fe-1.42%Al steel with 10% SiO2 mold flux. The influences of the casting temperature, pool depth, mold flux consumption rate, and casting speed on the evolution of Al2O3 in the mold flux during the continuous casting process of Fe-Al-2.2%Mn-C steels were predicted. Additionally, the effect of various initial Al contents in steels and initial Al2O3/SiO2 ratio in mold fluxes on Al2O3 evolution was further investigated.
引用
收藏
页码:5137 / 5146
页数:10
相关论文
共 50 条
  • [21] Kinetic study of glycerol hydrodeoxygenation on Al2O3 and NiMo2C/Al2O3 catalysts
    Duarte, Rafael Belo
    Corazza, Marcos Lucio
    Pimenta, Joao Lourenco Castagnari Willimann
    Jorge, Luiz Mario de Matos
    FUEL, 2023, 354
  • [22] Effect of SiO2 substitution with Al2O3 during high-Al TRIP steel casting on crystallization and structure of low-basicity CaO–SiO2-based mold flux
    Ding-li Zheng
    Cheng-bin Shi
    Zhi-jun Li
    Jing Li
    Jung-wook Cho
    Journal of Iron and Steel Research International, 2020, 27 : 33 - 41
  • [23] Effect of SiO2 substitution with Al2O3 during high-Al TRIP steel casting on crystallization and structure of low-basicity CaO-SiO2-based mold flux
    Zheng, Ding-li
    Shi, Cheng-bin
    Li, Zhi-jun
    Li, Jing
    Cho, Jung-wook
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2020, 27 (01) : 33 - 41
  • [24] Nanocarbon containing Al2O3 - C continuous casting refractories: Effect of graphite content
    Pilli, Venkatesh
    Sarkar, Ritwik
    JOURNAL OF ALLOYS AND COMPOUNDS, 2018, 735 : 1730 - 1736
  • [25] Effect of Al2O3 on the fluoride volatilization during melting and ion release in water of mold flux
    Gao, Jinxing
    Wen, Guanghua
    Liu, Qi
    Tan, Wenfeng
    Tang, Ping
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2015, 409 : 8 - 13
  • [26] Laser-induced luminescence of model Fe/Al2O3 and Cr/Al2O3 catalysts
    V. N. Snytnikov
    V. O. Stoyanovskii
    T. V. Larina
    O. P. Krivoruchko
    V. A. Ushakov
    V. N. Parmon
    Kinetics and Catalysis, 2008, 49 : 291 - 298
  • [27] Laser-induced luminescence of model Fe/Al2O3 and Cr/Al2O3 catalysts
    Snytnikov, V. N.
    Stoyanovskii, V. O.
    Larina, T. V.
    Krivoruchko, O. P.
    Ushakov, V. A.
    Parmon, V. N.
    KINETICS AND CATALYSIS, 2008, 49 (02) : 291 - 298
  • [28] Effect of Al2O3/SiO2 and CaO/Al2O3 ratios on wettability and structure of CaO-SiO2-Al2O3-based mold flux system
    Wang, Wan-lin
    Gao, Er-zhuo
    Zhou, Le-jun
    Zhang, Lei
    Li, Huan
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2019, 26 (04) : 355 - 364
  • [29] Effect of w(CaO)/w(Al2O3) on the Crystallization Properties of CaO-Al2O3-based Mold Flux
    Qi J.
    Liu C.-J.
    Zhang J.-H.
    Jiang M.-F.
    Dongbei Daxue Xuebao/Journal of Northeastern University, 2021, 42 (12): : 1717 - 1723
  • [30] Three Composite Coatings Al + Al2O3, Fe–Al and Fe–Al + Al2O3 as a Barrier Against LBE Alloys on F/M Steel by Multi-arc Ion Plating
    Chenhao Huang
    Shunlin Zhang
    Dong Pan
    Xing Yin
    Yong Chen
    Haibo Zhao
    Jun Wang
    Metallurgical and Materials Transactions A, 2023, 54 : 4701 - 4715