Crack sensitivity of high-manganese cryogenic steels in initial solidification during continuous casting

被引:2
|
作者
Li, Yang [1 ,2 ]
Winkler, Johann [3 ]
Presoly, Peter [4 ]
Bernhard, Christian [4 ]
Qin, Xu-feng [1 ,2 ]
Cheng, Chang-gui [1 ,2 ]
机构
[1] Wuhan Univ Sci & Technol, State Key Lab Refractories & Met, Wuhan 430081, Hubei, Peoples R China
[2] Wuhan Univ Sci & Technol, Key Lab Ferrous Met & Resources Utilizat, Minist Educ, Wuhan 430081, Hubei, Peoples R China
[3] K1 MET GmbH, A-8700 Leoben, Austria
[4] Univ Leoben, Ferrous Met, A-8700 Leoben, Austria
基金
中国国家自然科学基金; 中国博士后科学基金;
关键词
High-manganese cryogenic steel; Submerged split chill tensile test; Crack sensitivity; Initial solidification; Hot crack; CARBON; GROWTH; MOLD;
D O I
10.1007/s42243-024-01421-0
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Cryogenic steels, i.e., steels with maximum toughness at particularly low temperature, are increasingly becoming the focus of research. Cryogenic steels are usually alloyed with 5%-9% nickel. Ni can also be substituted by manganese as an austenite former. These high-manganese cryogenic grades are a cost-effective alternative to nickel-alloyed steels for use in liquefied natural gas storage tanks. The Mn content can then be more than 20 wt.% and lead to problems in production, particularly in the continuous casting process. In continuous casting of high-Mn-grades, quality issues and even breakout may result from the initial solidification behavior of the steel grades at high temperatures. Hot cracks form when a critical load is exceeded during solidification, close to the solidus temperature of the steel. A selected high-Mn-steel grade was characterized with respect to liquidus and solidus temperatures by means of thermal analysis and computational thermodynamics. In addition, so-called submerged split chill tensile tests were carried out to further understand the crack sensitivity of the solidifying shell for high-manganese cryogenic steels. The results reveal the presence of coarse hot tears, and also, a high frequency of hot cracks was observed at the location with the maximum accumulated strain, which is in line with the applied cracking criterion of Pierer and Bernhard for this investigation. In summary, the initial solidification phase of continuous casting poses a high risk of cracking for high-manganese cryogenic steel.
引用
收藏
页码:682 / 694
页数:13
相关论文
共 50 条
  • [41] Effect of intermittent high frequency magnetic field on initial solidification in continuous casting
    Li, T.J.
    Sassa, K.
    Asai, S.
    Acta Metallurgica Sinica Series A, Physical Metallurgy & Materials Science, 1997, 10 (02): : 151 - 156
  • [42] EFFECT OF INTERMITTENT HIGH FREQUENCY MAGNETIC FIELD ON INITIAL SOLIDIFICATION IN CONTINUOUS CASTING
    T. J. Li(Dalian University of Technology
    Acta Metallurgica Sinica(English Letters), 1997, (02) : 151 - 156
  • [43] The Casting Process Design and Simulation of the High-manganese Steel Roller
    Zhi, Xiaohui
    Yin, Yimin
    Han, Yanjun
    MATERIALS PROCESSING TECHNOLOGIES, PTS 1 AND 2, 2011, 154-155 : 1522 - +
  • [44] From High-Manganese Steels to Advanced High-Entropy Alloys
    Haase, Christian
    Barrales-Mora, Luis Antonio
    METALS, 2019, 9 (07)
  • [45] An approach to calculating the casting temperature of high-manganese austenite steel
    Arapov, S. L.
    V. Belyaev, S.
    Kosovich, A. A.
    Partyko, E. G.
    CIS IRON AND STEEL REVIEW, 2023, 26 : 45 - 50
  • [46] Twin-roll strip casting: A competitive alternative for the production of high-manganese steels with advanced mechanical properties
    Daamen, Markus
    Haase, Christian
    Dierdorf, Jens
    Molodov, Dmitri A.
    Hirt, Gerhard
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 627 : 72 - 81
  • [47] THERMALLY INDUCED SEGREGATION IN HIGH-MANGANESE STAINLESS-STEELS
    GERMAN, RM
    ODEGARD, BC
    MATERIALS SCIENCE AND ENGINEERING, 1978, 35 (02): : 299 - 301
  • [48] Effect of exciting current of high frequency electromagnetic field on initial solidification of steel during electromagnetic continuous casting
    Wang, H. -M.
    Li, G. -R.
    Ren, Z. -M.
    Zhao, Y. -T.
    IRONMAKING & STEELMAKING, 2009, 36 (08) : 615 - 622
  • [49] Fracture toughness of High-Manganese steels with TWIP/ TRIP effects
    Bordone, M.
    Monsalve, A.
    Perez Ipina, J.
    ENGINEERING FRACTURE MECHANICS, 2022, 275
  • [50] EFFECT OF VANADIUM ON THE STRUCTURE AND PROPERTIES OF HIGH-MANGANESE STEELS.
    Sil'man, G.I.
    Pristuplyuk, N.I.
    Frol'tsov, M.S.
    Metal Science and Heat Treatment (English Translation of Metallovedenie i Termicheskaya Obrabotka Metallov), 1980, 22 (1-2): : 124 - 127