Investigating Hot corrosion, CMAS, and Thermal Shock Behaviour of Double-layer YSZ/La2Ce2O7 + YSZ Thermal Barrier Coatings

被引:3
|
作者
Pakseresht, Amirhossein [1 ]
Ariharan, S. [1 ,2 ]
Sekar, Anusha [1 ]
Parchoviansky, Milan [1 ]
机构
[1] Alexander Dubcek Univ Trencin, Ctr Funct & Surface Functionalized Glass, Trencin 91150, Slovakia
[2] Vikram Sarabhai Space Ctr, Mat & Mech Ent, Thiruvananthapuram, Kerala, India
基金
欧盟地平线“2020”;
关键词
CMAS corrosion; hot corrosion; TBCs; thermal shock resistance; ALUMINO-SILICATE CMAS; BARRIER COATINGS; FAILURE; TEMPERATURE; ZIRCONIA; POWDER; DELAMINATION; MULTILAYER; MECHANISM; SUBJECT;
D O I
10.1007/s11666-024-01845-w
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this work, new double-layer YSZ/La2Ce2O7 (LC) + YSZ coatings were developed using air plasma spraying (APS). The surface of the prepared coatings was relatively smooth and consisted of melted and partially melted areas. Their resistance to hot corrosion, CaO-MgO-Al2O3-SiO2 (CMAS), and thermal shock were examined. YSZ was added to the upper layer to enhance the lanthanum cerate (La2Ce2O7, LC) properties. During the hot corrosion tests, the corrosion salt reacted with the upper layer, and the CeO2 phase and new corrosion products were identified. The main phase was LaVO4, and the secondary phases were CeVO4 and YVO4. SEM confirmed the formation of new, cuboidal-shaped corrosion products. The infiltration of CMAS led to the formation of additional new products: Ca(4)MgxAl(4)Si(6-x-gamma)O-14 and Ca-2.8(LaxCe1-x).(6)(SiO4)O6-4x. SEM revealed CMAS infiltration through the upper layer in the form of islands. Following the thermal shock resistance tests, the upper layer gradually peeled off, and the coating survived 67 cycles. Possible failure mechanisms were identified, and failure was attributed to the spallation of the upper layer from the surface layer by layer. After all tests, the top layer showed partial spalling and delamination. This was mainly caused by the reaction of corrosive salt or CMAS with the top layer, which changed its composition, leading to the formation and propagation of cracks and, ultimately, the separation of part of the upper layer. Peeling of the upper layer through mainly horizontal cracks was observed after hot corrosion, CMAS and thermal shocks. The NiCrAlY bond coat and YSZ interlayer remained undamaged.
引用
收藏
页码:809 / 822
页数:14
相关论文
共 50 条
  • [1] Mechanical Properties and CMAS Corrosion Resistance of La2Ce2O7/YSZ Composite Thermal Barrier Coatings
    Kang, Y. X.
    Bai, Y.
    Bao, C. G.
    Fan, W.
    Zhang, L.
    INTERNATIONAL THERMAL SPRAY CONFERENCE AND EXPOSITION (ITSC 2018), 2018, : 75 - 78
  • [2] Effect of Ceramic Layer Thickness Ratio on Thermal Shock Resistance of La2Ce2O7/YSZ Thermal Barrier Coatings
    Ren Xiaoxue
    Jiang Peng
    Fan Xueling
    Wang Tiejun
    RARE METAL MATERIALS AND ENGINEERING, 2018, 47 (12) : 3703 - 3709
  • [3] Mechanisms of La2Ce2O7/YSZ Double-Ceramic-Layer Thermal Barrier Coatings against Volcanic Ash Corrosion
    Xia, Jie
    Du, Xuelin
    Xiao, Yiqi
    Zhang, Ling
    Wu, Rudder Tse
    Matsushita, Yoshitaka
    COATINGS, 2024, 14 (07)
  • [4] Thermal cycling performance of La2Ce2O7/50 vol.% YSZ composite thermal barrier coating with CMAS corrosion
    Kang, Y. X.
    Bai, Y.
    Fan, W.
    Yuan, T.
    Gao, Y.
    Bao, C. G.
    Li, B. Q.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (07) : 2851 - 2862
  • [5] Biaxial stress in La2Ce2O7/YSZ thermal barrier coatings for oxidation evolution
    Zhao, Xianli
    Wang, Qianwen
    Liu, Wei
    Yan, Gang
    Li, Cong
    Yang, Li
    Zhou, Yichun
    SURFACE & COATINGS TECHNOLOGY, 2022, 447
  • [6] Thermo-Physical Properties and Thermal Shock Resistance of Segmented La2Ce2O7/YSZ Thermal Barrier Coatings
    Guo, Hongbo
    Wang, Yi
    Wang, Lu
    Gong, Shengkai
    JOURNAL OF THERMAL SPRAY TECHNOLOGY, 2009, 18 (04) : 665 - 671
  • [7] Thermo-Physical Properties and Thermal Shock Resistance of Segmented La2Ce2O7/YSZ Thermal Barrier Coatings
    Hongbo Guo
    Yi Wang
    Lu Wang
    Shengkai Gong
    Journal of Thermal Spray Technology, 2009, 18 : 665 - 671
  • [8] Biaxial stress in La2Ce2O7/YSZ thermal barrier coatings for oxidation evolution
    Zhao, Xianli
    Wang, Qianwen
    Liu, Wei
    Yan, Gang
    Li, Cong
    Yang, Li
    Zhou, Yichun
    Surface and Coatings Technology, 2022, 447
  • [9] Hot corrosion properties of plasma sprayed La2Ce2O7/YSZ vis-a-vis La2Ce2O7/cluster paired zirconia thermal barrier coatings
    Lashmi, P. G.
    Balaji, N.
    Kumar, S. Senthil
    Aruna, S. T.
    SURFACE & COATINGS TECHNOLOGY, 2021, 409
  • [10] Solid Particle Erosion Behavior of La2Ce2O7/YSZ Double-Ceramic-Layer and Traditional YSZ Thermal Barrier Coatings at High Temperature
    Zhao, Xianli
    Liu, Wei
    Li, Cong
    Yan, Gang
    Wang, Qianwen
    Yang, Li
    Zhou, Yichun
    COATINGS, 2022, 12 (11)