Immobilisation of iodide in alkali-activated materials

被引:0
|
作者
Chaerun, Raudhatul Islam [1 ,2 ,3 ]
Ishimura, Manami [4 ]
Prihutami, Pramesti [1 ]
Niu, Xiaobo [5 ]
Ohya, Yusuke [1 ]
Kuroda, Kazuma [6 ]
Toda, Kanako [7 ]
Kikuchi, Ryosuke [5 ]
Otake, Tsubasa [5 ]
Provis, John L. [8 ]
Elakneswaran, Yogarajah [5 ]
Sato, Tsutomu [5 ]
机构
[1] Division of Sustainable Resources Engineering, Graduate School of Engineering, Hokkaido University, Hokkaido, Sapporo,060-8628, Japan
[2] Nuclear Fuel Cycle Engineering Laboratories, Japan Atomic Energy Agency, Muramatsu 4-33, Tokai-mura, Naka-gun, Ibaraki, 319-1194, Japan
[3] Fukushima Research and Engineering Institute, Japan Atomic Energy Agency, Muramatsu 4-33, Tokai-mura, Naka-gun, Ibaraki, 319-1194, Japan
[4] Course of Sustainable Resources Engineering, School of Engineering, Hokkaido University, Hokkaido, Sapporo,060-8628, Japan
[5] Division of Sustainable Resources Engineering, Faculty of Engineering, Hokkaido University, Hokkaido, Sapporo,060-8628, Japan
[6] Sustainable System Research Laboratory, Central Research Institute of Electric Power Industry, Abiko-shi, Chiba,270-1194, Japan
[7] Nuclear Professional School, School of Engineering, The University of Tokyo, 2-22 Shirakata Shirane, Tokai-mura, Ibaraki, 319-1188, Japan
[8] Laboratory for Waste Management, Paul Scherrer Institute, Forschungsstrasse 111, Villigen PSI,5232, Switzerland
基金
英国工程与自然科学研究理事会;
关键词
Bioremediation - Coprecipitation - Iodine compounds - Mendelevium - Nitrates - Radioactive waste disposal - Silica - Silver halides - Silver oxides;
D O I
10.1016/j.chemosphere.2024.143871
中图分类号
学科分类号
摘要
At the Fukushima Daiichi Nuclear Power Station (FDNPS), continuous water circulation cools fuel debris, leading to the presence of radionuclides such as Sr-30, Cs-137, and I-129 in the cooling water. These radionuclides are adsorbed and co-precipitated by various materials. Among them, I-129 is a key radionuclide for safety assessment during the final disposal of adsorbent and co-precipitation materials, owing to its long half-life and poor sorption. Alkali-activated materials (AAM) have been demonstrated to immobilise cationic radionuclides but not anionic radionuclides. Here, layered double hydroxide (LDH), magnesium oxide (MgO), and silver nitrate (AgNO3) were investigated as additive materials to immobilise I− in potassium-based AAM (K-AAM). Our findings revealed that LDH and MgO were not effective in retaining I− in K-AAM. In the case of LDH addition, the high anion exchange capacity of LDH was rendered ineffective, as its adsorption sites were occupied by highly selective silicate anions. In the case of MgO addition, magnesium silicate hydrates (M-S-H) were formed, which did not appear to possess the ability to retain I−, despite the desirable in situ synthesis of LDH containing alumina in K-AAM. Conversely, the addition of AgNO3 to K-AAM resulted in a reduced leaching rate, which was attributed to AgI formation. The immobilisation could be enhanced by adjusting the amount of AgNO3 incorporated into the K-AAM during the fabrication process. In conclusion, the leaching of I− from spent adsorbent and co-precipitation materials embedded in the K-AAM matrix could be suppressed when AgI was sufficiently generated within the K-AAM matrix. © 2024 Elsevier Ltd
引用
收藏
相关论文
共 50 条
  • [41] One-part alkali-activated materials: A review
    Luukkonen, Tero
    Abdollahnejad, Zahra
    Yliniemi, Juho
    Kinnunen, Paivo
    Illikainen, Mirja
    CEMENT AND CONCRETE RESEARCH, 2018, 103 : 21 - 34
  • [42] Philosophy of rational mixture proportioning of alkali-activated materials validated by the hydration kinetics of alkali-activated slag and its microstructure
    Bilek Jr, Vlastimil
    Novotny, Radoslav
    Koplik, Jan
    Kadlec, Martin
    Kalina, Lukas
    CEMENT AND CONCRETE RESEARCH, 2023, 168
  • [43] Mechanism understanding of alkali-silica reaction in alkali-activated materials system
    Wang, Wei
    Noguchi, Takafumi
    Maruyama, Ippei
    CEMENT AND CONCRETE RESEARCH, 2022, 156
  • [44] Wear behavior in pastes of alkali-activated materials: Influence of precursor and alkali solution
    Shagnay, S.
    Velasco, F.
    del Campo, A.
    Torres-Carrasco, M.
    TRIBOLOGY INTERNATIONAL, 2020, 147
  • [45] Effect of sodium silicate slurries on the properties of alkali-activated materials
    K. S. Ivanov
    E. A. Korotkov
    Inorganic Materials, 2017, 53 : 973 - 979
  • [46] PAPER SLUDGE ASH AS A PRECURSOR FOR PRODUCTION OF ALKALI-ACTIVATED MATERIALS
    Bernal, Susan A.
    Ball, Richard J.
    Hussein, Oday
    Heath, Andrew C.
    Provis, John L.
    ADVANCES IN CHEMICALLY-ACTIVATED MATERIALS (CAM'2014), 2014, 92 : 140 - 149
  • [47] Adsorption Efficiency of Cadmium (II) by Different Alkali-Activated Materials
    Nikolic, Natasa Mladenovic
    Kljajevic, Ljiljana
    Nenadovic, Snezana S.
    Potocnik, Jelena
    Knezevic, Sanja
    Dolenec, Sabina
    Trivunac, Katarina
    GELS, 2024, 10 (05)
  • [48] Lead immobilization in tailings-based alkali-activated materials
    Wang, Hao
    Wang, Lu
    Ren, Zhisheng
    Liu, Shuhua
    CONSTRUCTION AND BUILDING MATERIALS, 2024, 428
  • [49] Passivation and depassivation of reinforcement steel in alkali-activated materials—A review
    Xu, Xiaoying
    Hu, Xiang
    Khaskhoussi, Amani
    Shi, Caijun
    Cement and Concrete Composites, 2024, 154
  • [50] Application of machine learning in predicting workability for alkali-activated materials
    Kong, Y. K.
    Kurumisawa, Kiyofumi
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2023, 18