Effect of calcium carbide slag on the durability of alkali-activated ground granulated blast furnace slag-fly ash cementitious system

被引:0
|
作者
Mei, Junpeng [1 ,2 ,3 ]
Yin, Chen [1 ]
Zhao, Yanjun [4 ]
Niu, Yinlong [4 ]
Xie, Anhe [1 ]
Li, Shuang [1 ]
机构
[1] Wuhan Univ Sci & Technol, Sch Urban Construct, Wuhan 430065, Peoples R China
[2] Hubei Prov Engn Res Ctr Urban Regenerat, Wuhan 430065, Peoples R China
[3] Wuhan Univ Sci & Technol, Inst High Performance Engn Struct, Wuhan 430065, Peoples R China
[4] China Construct Third Bur First Engn Co Ltd, Wuhan 430040, Peoples R China
来源
ZKG INTERNATIONAL | 2024年 / 77卷 / 08期
关键词
SHRINKAGE; GEOPOLYMER;
D O I
暂无
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
In this paper, alkali-activated composite cementitious materials were prepared by using calcium carbide slag, ground granulated blast-furnace slag (GGBS), and fly ash as raw materials, and a combination of sodium hydroxide and sodium silicate solutions were used as alkali activators of binders. The drying shrinkage, resistance to chlorine ion permeability, sulfate resistance, and mechanical properties of GGBS-fly ash cementitious system with different contents of calcium carbide slag were investigated. In addition, the changes in hydration products were also analyzed by X-ray diffraction (XRD). The results show that: when the content of calcium carbide slag instead of fly ash or GGBS is gradually increased, the drying shrinkage of the composite cementitious material decreases dramatically, the compressive strength and flexural strengths corrosion resistance coefficient increase first and then decrease, the compressive strength corrosion resistance coefficient decreases weakly. The primary hydration products of the composite cementitious material with varying calcium carbide slag content are calcium silicate hydrate (C-S-H) and calcium aluminosilicate hydrate (C-A-S-H) and these products remain stable under sodium sulfate erosion. Overall, the optimal properties were achieved with 3% calcium carbide slag replacing fly ash, which exhibits a 28 d drying shrinkage of 9672 mu epsilon, an electrical flux of 2868 C, a compressive strength of 67.3 MPa after 120 d of full immersion in sodium sulfate, a flexural strength corrosion resistance coefficient of 1.21, and a compressive strength corrosion resistance coefficient of 1.02.
引用
收藏
页码:42 / 50
页数:9
相关论文
共 50 条
  • [31] Alkali-activated concrete mixes with ground granulated blast furnace slag and paper sludge ash in seawater environments
    Mengasini, Laura
    Mavroulidou, Maria
    Gunn, Michael J.
    SUSTAINABLE CHEMISTRY AND PHARMACY, 2021, 20
  • [32] Effect of activator on rheological properties of alkali-activated slag-fly ash pastes
    Yuan Qiang
    Huang Yan
    Huang Ting-jie
    Yao Hao
    Wu Qi-hong
    JOURNAL OF CENTRAL SOUTH UNIVERSITY, 2022, 29 (01) : 282 - 295
  • [33] Alkali-activated concrete mixes with ground granulated blast furnace slag and paper sludge ash in seawater environments
    Mengasini, Laura
    Mavroulidou, Maria
    Gunn, Michael J.
    SUSTAINABLE CHEMISTRY AND PHARMACY, 2021, 20
  • [34] Effect of metakaolin on the autogenous shrinkage of alkali-activated slag-fly ash paste
    Li, Zhenming
    Liang, Xuhui
    Chen, Yun
    Ye, Guang
    CONSTRUCTION AND BUILDING MATERIALS, 2021, 278
  • [35] Radiological characterisation of alkali-activated construction materials containing red mud, fly ash and ground granulated blast-furnace slag
    Sas, Zoltan
    Sha, Wei
    Soutsos, Marios
    Doherty, Rory
    Bondar, Dali
    Gijbels, Katrijn
    Schroeyers, Wouter
    SCIENCE OF THE TOTAL ENVIRONMENT, 2019, 659 : 1496 - 1504
  • [36] Hydrothermal synthesis and characterization of alkali-activated slag-fly ash-metakaolin cementitious materials
    Wang, Jin
    Wu, Xiu-ling
    Wang, Jun-xia
    Liu, Chang-zhen
    Lai, Yuan-ming
    Hong, Zun-ke
    Zheng, Jian-ping
    MICROPOROUS AND MESOPOROUS MATERIALS, 2012, 155 : 186 - 191
  • [37] Durability Analysis of Basalt Textile Reinforced Alkali-activated Slag-fly Ash Cement Mortars
    Peng Z.
    Zhu D.
    Shi C.
    Guo S.
    Li N.
    Cailiao Daobao/Materials Reports, 2021, 35 (16): : 16058 - 16064
  • [38] Modification mechanism of flue gas desulfurization gypsum on fly ash and ground granulated blast-furnace slag alkali-activated materials: Promoting green cementitious material
    Luan, Yingcheng
    Wang, Jianhua
    Ma, Tao
    Wang, Siqi
    Li, Chao
    CONSTRUCTION AND BUILDING MATERIALS, 2023, 396
  • [39] Modification of phase evolution in alkali-activated blast furnace slag by the incorporation of fly ash
    Ismail, Idawati
    Bernal, Susan A.
    Provis, John L.
    Nicolas, Rackel San
    Hamdan, Sinin
    van Deventer, Jannie S. J.
    CEMENT & CONCRETE COMPOSITES, 2014, 45 : 125 - 135
  • [40] Study on properties of pervious concrete with alkali-activated slag-fly ash
    Bian, Wei
    Ma, Kunlin
    Long, Guangcheng
    Liu, Wanwan
    Zhang, Chuanqin
    Journal of Railway Science and Engineering, 2020, 17 (02) : 349 - 357