Effect of pre-strain on hydrogen-induced delayed cracking and hydrogen trapping behavior in high-strength martensitic steels

被引:0
|
作者
Li, Weiguo [1 ]
Cao, Zhongqian [1 ]
Yang, Zixuan [2 ]
Zhou, Qingjun [3 ]
Li, Jinxu [1 ,4 ]
机构
[1] Corrosion and Protection Center, Institute for Advanced Materials and Technology, University of Science and Technology Beijing, Beijing,100083, China
[2] Zhejiang Provincial Engineering Research Center for the Safety of Pressure Vessel and Pipeline, Ningbo University, Ningbo,315211, China
[3] Central Research Institute, Baoshan Iron & Steel Co., Ltd., Shanghai,201900, China
[4] State Key Laboratory of Nuclear Power Safety Technology and Equipment, University of Science and Technology Beijing, Beijing,100083, China
关键词
This project was supported by the National Natural Science Foundation of China (52271050) and the Science and Technology Innovation 2025 Major Project of Ningbo City (2022Z209; 2023Z005).This project was supported by the National Key R&D Program of China (2022YFB4003000) and the Science and Technology Innovation 2025 Major Project of Ningbo City (2022Z209; 2023Z005);
D O I
10.1016/j.ijhydene.2024.10.170
中图分类号
学科分类号
摘要
引用
收藏
页码:470 / 487
相关论文
共 50 条
  • [21] Quantifying Heat-Affected Zone Hydrogen-Induced Cracking in High-Strength Naval Steels
    Yue, X.
    Feng, X. L.
    Lippold, J. C.
    WELDING JOURNAL, 2013, 92 (09) : 265S - 273S
  • [22] Effect of microstructure on hydrogen embrittlement and hydrogen-induced cracking behaviour of a high-strength pipeline steel weldment
    Zhang, Peng
    Laleh, Majid
    Hughes, Anthony E.
    Marceau, Ross K. W.
    Hilditch, Tim
    Tan, Mike Yongjun
    CORROSION SCIENCE, 2024, 227
  • [23] Hydrogen-Induced Delayed Cracking
    Pohl, M.
    PRAKTISCHE METALLOGRAPHIE-PRACTICAL METALLOGRAPHY, 2019, 56 (09): : 556 - 566
  • [24] Analysis of hydrogen-induced delayed cracking and hydrogen trapping behavior in plastically deformed quenching and partitioning steel
    Li, Weiguo
    Wu, Weijie
    Zhou, Qingjun
    Li, Wenyao
    Li, Jinxu
    CORROSION SCIENCE, 2023, 223
  • [25] HYDROGEN-INDUCED CRACKING SUSCEPTIBILITY IN HIGH-STRENGTH WELD METAL.
    Okuda, N.
    Ogata, Y.
    Nishikawa, Y.
    Aoki, T.
    Goto, A.
    Abe, T.
    Welding Journal (Miami, Fla), 1987, 66 (05):
  • [26] Effect of Nb on hydrogen-induced delayed fracture in high strength hot stamping steels
    Zhang, Shiqi
    Huang, Yunhua
    Sun, Bintang
    Liao, Qingliang
    Lu, Hongzhou
    Jian, Bian
    Mohrbacher, Hardy
    Zhang, Wei
    Guo, Aimin
    Zhang, Yue
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 626 : 136 - 143
  • [27] Effect of Nb on the hydrogen-induced cracking of high-strength low-alloy steel
    Zhang Shiqi
    Fan Endian
    Wan Jifang
    Liu Jing
    Huang Yunhua
    Li Xiaogang
    CORROSION SCIENCE, 2018, 139 : 83 - 96
  • [28] Hydrogen-induced cracking in a very-high-purity high-strength steel
    Liu, X. -Y.
    Kameda, J.
    Anderegg, J. W.
    Takaki, S.
    Abiko, K.
    McMahon, C. J., Jr.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 492 (1-2): : 218 - 220
  • [29] Novel Cu-bearing high-strength pipeline steels with excellent resistance to hydrogen-induced cracking
    Shi, Xianbo
    Yan, Wei
    Wang, Wei
    Shan, Yiyin
    Yang, Ke
    MATERIALS & DESIGN, 2016, 92 : 300 - 305
  • [30] PREDICTION ON INITIATION OF HYDROGEN-INDUCED DELAYED CRACKING IN HIGH-STRENGTH STEEL BASED ON COHESIVE ZONE MODELING
    Wang, Yanfei
    Gong, Jianming
    Geng, Luyang
    Jiang, Yong
    ASME PRESSURE VESSELS AND PIPING CONFERENCE - 2014, VOL 6B, 2014,