Effect of Micro-arc Oxidation on Corrosion Resistance of Ti6Al4V Electron Beam Welded Joint

被引:0
|
作者
Wang, Xiaobo [1 ]
Yu, Zhen [2 ,3 ]
Hu, Yonghui [2 ,3 ]
Wu, Peng [2 ,3 ]
Mei, Jinhui [2 ,3 ]
Cai, Zhihui [4 ]
Xu, Jianping [5 ]
Ma, Yinghe [2 ,3 ]
Zheng, Wenjian [2 ,3 ]
Yang, Jianguo [2 ,3 ]
机构
[1] Institute of Materials, China Academy of Engineering Physics, Sichuan, Mianyang,621700, China
[2] College of Mechanical Engineering, Zhejiang University of Technology, Hangzhou,310023, China
[3] Process Equipment and Remanufacturing Engineering Research Center, The Ministry of Education, Zhejiang University of Technology, Hangzhou,310023, China
[4] Wenzhou Special Equipment Testing Science Research Institute, Zhejiang, Wenzhou,325038, China
[5] Department of Materials and Chemical Engineering, Heilongjiang Institute of Technology, Harbin,150050, China
来源
Surface Technology | 2025年 / 54卷 / 02期
基金
中国国家自然科学基金;
关键词
Aluminum coatings - Aluminum corrosion - Butt welding - Corrosion resistance - Corrosion resistant alloys - Corrosion resistant coatings - Corrosive effects - Crystal orientation - Dealloying - Electric arc welding - Electrochemical corrosion - Electrolytic cleaning - Heat affected zone - High temperature corrosion - Metal cladding - Microbial corrosion - Sodium alloys - Titanium plating - Ultrasonic cleaning - Ultrasonic welding - Weld decay;
D O I
10.16490/j.cnki.issn.1001-3660.2025.02.008
中图分类号
学科分类号
摘要
Micro arc oxidation (MAO) technology is currently one of the widely used methods to improve the surface properties of titanium alloys. To improve the corrosion resistance of Ti6Al4V electron beam welded joints, MAO technology was applied in this paper. The article studied the influence of MAO treatment on the micro-structure and corrosion resistance of welded joints. The reasons for the improvement of joint corrosion resistance were analyzed. After grinding and polishing, the Ti6Al4V titanium alloy samples were sequentially cleaned by ultrasonic cleaning in acetone and alcohol, and dried for later use. An optimized welding process was adopted for titanium alloy flat plate butt welding. The welding parameters were high voltage of 65 kV, welding beam current of 10 mA, and electron beam linear velocity of 300 mm/min. After welding, the acetone and alcohol solution were used to perform ultrasonic cleaning on the welded samples. Then the base materials and the joints were treated by micro-arc oxidation simultaneously. The electrolyte was a mixed solution of 15 g/L Na2SiO3, 10 g/L Na3PO4, and 1 g/L NaOH. The power parameters included a current density of 14 A/dm2, a duty cycle of 20%, a pulse frequency of 500 Hz, and an oxidation time of 20 minutes. Optical microscope (OM), field emission scanning electron microscope (FE-SEM), X-ray diffraction (XRD), electrochemical corrosion test and immersion corrosion test were taken to value the morphologies, phase structure, electrochemical corrosion performance and immersion corrosion performance of the base materials, joints and their coatings, respectively. Compared with the base material, the micro-structure of the welded joint underwent significant changes due to the high temperature and low cooling rate. The primary α phase and intergranular β phase were transformed to the acicular α' martensite, distributed in a feather-like pattern on both sides of the grain boundary. After micro-arc oxidation treatment of the base materials and the joint, the morphology of them were similar, showing unevenly distributed micro-pores of different sizes and molten protrusions resembling volcanoes. However, compared with the coatings on the base materials, the aperture and porosity of the joint coatings were relatively smaller. Compared with the base material coating, the thickness, integrity, and continuity of the joint coating were lower. The phases of the MAO coatings in the BM and WZ regions were similar, mainly showing the rutile phase TiO2 and anatase phase TiO2. And the α phase and α′ phase were also appeared in the XRD spectrum due to the small coating thickness and surface micropores, thus allowing the X-ray to penetrate the coatings. Additionally, due to the formation of an oxide film, the β phase disappeared. Compared with the base materials, the self-corrosion potential of the joint decreased by approximately 0.3 V, and the self-corrosion current increased by one order of magnitude. After the MAO treatment, polarization curves of the base materials and the joint appeared obvious passivation, and joint coating group were obviously wider. Although the corrosion resistance of coated joints was lower compared with coated base materials, their self-corrosion potential (Ecorr) was increased by 290 mV, the self-corrosion current densities (Jcorr) was reduced by an order of magnitude, and the corrosion rate was significantly reduced when immersed in 2 mol/L HCl solution compared with uncoated joints. The MAO treatment can improve the corrosion resistance of the joint in neutral and acidic corrosive medias. © 2025 Chongqing Wujiu Periodicals Press. All rights reserved.
引用
收藏
页码:106 / 118
相关论文
共 50 条
  • [31] Improvement of tribological performance by micro-arc oxidation treatment on selective laser melting Ti6Al4V alloy
    Yan, Xingchen
    Chen, Chaoyue
    Bolof, Rodolphe
    Ma, Wenyou
    Deng, Chunming
    Wang, Jiang
    Ren, Zhongming
    Liao, Hanlin
    Liu, Min
    MATERIALS RESEARCH EXPRESS, 2019, 6 (09)
  • [33] Effect of polarization voltage on the surface componentization and biocompatibility of micro-arc oxidation modified selective laser melted Ti6Al4V
    Chen, Ziyu
    Yan, Xingchen
    Chang, Yu
    Xie, Shiming
    Ma, Wenyou
    Zhao, Guorui
    Liao, Hanlin
    Fang, Hang
    Liu, Min
    Cai, Daozhang
    MATERIALS RESEARCH EXPRESS, 2019, 6 (08)
  • [34] Biocompatibility of micro-arc oxidation coatings developed on Ti6Al4V alloy in a solution containing organic phosphate
    Zhang, R. F.
    Qiao, L. P.
    Qu, B.
    Zhang, S. F.
    Chang, W. H.
    Xiang, J. H.
    MATERIALS LETTERS, 2015, 153 : 77 - 80
  • [35] Enhanced cytocompatibility of Ti6Al4V alloy through selective removal of Al and V from the hierarchical micro-arc oxidation coating
    Guan, Shiwei
    Qi, Min
    Wang, Cong
    Wang, Shuyue
    Wang, Weiqiang
    APPLIED SURFACE SCIENCE, 2021, 541
  • [36] Effects of electrolytic concentration on properties of micro-arc film on Ti6Al4V alloy
    SHI XinglingWANG QingliangWANG FushunGE Shirong School of Material Science and EngineeringChina University of Mining TechnologyXuzhouJiangsu China
    MiningScienceandTechnology, 2009, 19 (02) : 220 - 224
  • [37] Microstructure evolution and strengthening mechanism of electron beam welded TiBw/Ti6Al4V composite joint
    Li, Ning
    Wang, Ting
    Jiang, Siyuan
    Zhang, Lixia
    MATERIALS CHARACTERIZATION, 2021, 178
  • [38] Effect of the oxidation time on properties of ceramic coatings produced on Ti-6Al-4V by micro-arc oxidation
    Jiang, Zhaohua
    Sun, Xuetong
    Li, Yanping
    Wang, Fuping
    Lu, Yandong
    Journal of Materials Science and Technology, 2005, 21 (02): : 281 - 284
  • [39] The Effect of Micro arc Oxidation Process Parameters on Surface Properties of Ti6Al4v Alloy
    Gunyuz, M.
    Baydogan, M.
    Cimenoglu, H.
    Kayali, E. S.
    DIFFUSION IN SOLIDS AND LIQUIDS VI, PTS 1 AND 2, 2011, 312-315 : 1000 - 1003