Optimization of pressurization process in low-pressure casting of a 5.4-ton gigantic C95800 copper alloy casting

被引:0
|
作者
Qiu, Zi-ao [1 ,2 ]
Zhao, Xin-yi [3 ]
Zhang, Chao-jun [1 ,2 ]
Yang, Jun-liu [4 ]
Shi, Rui-yun [4 ]
Lue, Tang-qi [4 ]
Yu, Xiao-lei [5 ]
Chen, Qiu-shi [5 ]
Quan, Lin-lin [5 ]
Zhang, Lun-yong [1 ,2 ]
Cao, Fu-yang [1 ,2 ]
Sun, Jian-fei [1 ,2 ]
机构
[1] Harbin Inst Technol, Natl Key Lab Precis Hot Proc Met, Harbin 150001, Peoples R China
[2] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
[3] Jiangsu Univ, Sch Mat Sci & Engn, Zhenjiang 212000, Jiangsu, Peoples R China
[4] Shanghai Marine Equipment Res Inst, Shanghai 200031, Peoples R China
[5] Dalian Marine Propeller Co Ltd, Dalian 116021, Peoples R China
基金
中国国家自然科学基金;
关键词
gigantic copper alloy casting; C95800; low-pressure casting; nonlinear pressurization process; OXIDE-FILM DEFECTS; NUMERICAL-SIMULATION; MAGNESIUM ALLOY; AS-CAST; FLOW; SOLIDIFICATION;
D O I
10.1007/s41230-024-4167-6
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
During the low-pressure casting of extra-large size C95800 copper alloy components, traditional linear pressurization technique leads to a rapid surge of liquid metal inlet velocity at the regions where the mold cavity cross-section enlarges. This rapid increasement of liquid metal inlet velocity causes serious entrapment of gas and oxide films, and results in various casting defects such as the bifilm defects. These defects detrimentally deteriorate mechanical properties of the castings. To address this issue, an innovative nonlinear pressurization strategy timely matching to the casting structure was proposed. The pressurization rate decreases at sections where the cross-section widens, but it gradually increases as the liquid metal level rises. By this way, the inlet velocity remains below a critical threshold to prevent the entrapment of gas and oxide films. Comparative analyses involving numerical simulations and casting verification illustrate that the nonlinear pressurization technique, compared to the linear pressurization, effectively diminishes both the size and number of bifilm defects. Furthermore, the nonlinear pressurization method enhances the casting yield strength by 10%, tensile strength by 14%, and elongation by 10%. Examination through scanning electron microscopy highlights that the bifilm defects arising from the linear pressurization process result in the reduction of the castings' mechanical properties. These observations underscore the efficacy of nonlinear pressurization in enhancing the quality and reliability of gigantic castings, as exemplified by a 5.4-ton extra-large sized C95800 copper alloy propeller hub with complex structures in the current study.
引用
收藏
页码:717 / 726
页数:10
相关论文
共 50 条
  • [11] LOW-PRESSURE CASTING FOR ALLOY V-8 BLOCK
    不详
    AUTOMOTIVE ENGINEERING, 1978, 86 (04): : 18 - 19
  • [12] Effect of process parameters on density of magnesium alloy parts by low-pressure expendable pattern casting
    李继强
    樊自田
    董选普
    TransactionsofNonferrousMetalsSocietyofChina, 2007, (S1) : 358 - 362
  • [13] Low-pressure die casting of magnesium alloy AM50: Response to process parameters
    Fu, Penghuai
    Luo, Alan A.
    Jiang, Haiyan
    Peng, Liming
    Yu, Yandong
    Zhai, Chunquan
    Sachdev, Anil K.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2008, 205 (1-3) : 224 - 234
  • [14] Effect of process parameters on density of magnesium alloy parts by low-pressure expendable pattern casting
    Li Ji-qiang
    Fan Zi-tian
    Dong Xuan-pu
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2007, 17 : S358 - S362
  • [15] Low-pressure permanent mold casting of copper-base alloys
    Fasoyinu, FA
    Morin, G
    Cousineau, D
    Sadayappan, M
    Sahoo, M
    TRANSACTIONS OF THE AMERICAN FOUNDRYMEN'S SOCIETY, VOL 105, 1998, 105 : 333 - 342
  • [16] EFFECT OF COOLING PROCESS ON POROSITY IN THE ALUMINUM ALLOY AUTOMOTIVE WHEEL DURING LOW-PRESSURE DIE CASTING
    Sui, Dashan
    Cui, Zhenshan
    Wang, Rong
    Hao, Shengfei
    Han, Qingyou
    INTERNATIONAL JOURNAL OF METALCASTING, 2016, 10 (01) : 32 - 42
  • [17] A new vacuum-assisted low-pressure investment casting process for K446 alloy
    Ma, Lan-bo
    Cheng, Wen-jin
    Guo, Xin-li
    Fan, Bing-zheng
    Guan, Yang
    Li, Yi-peng
    Jin, Lei
    Shui, Guo-yan
    Jiang, Yi-zhong
    Sun, Xun
    CHINA FOUNDRY, 2024, 21 (06) : 702 - 708
  • [18] A new vacuum-assisted low-pressure investment casting process for K446 alloy
    Lanbo Ma
    Wenjin Cheng
    Xinli Guo
    Bingzheng Fan
    Yang Guan
    Yipeng Li
    Lei Jin
    Guoyan Shui
    Yizhong Jiang
    Xun Sun
    China Foundry, 2024, 21 (06) : 702 - 708
  • [19] Effect of Cooling Process on Porosity in the Aluminum Alloy Automotive Wheel During Low-Pressure Die Casting
    Dashan Sui
    Zhenshan Cui
    Rong Wang
    Shengfei Hao
    Qingyou Han
    International Journal of Metalcasting, 2016, 10 : 32 - 42
  • [20] A new vacuum-assisted low-pressure investment casting process for K446 alloy
    Ma, Lan-Bo
    Cheng, Wen-Jin
    Guo, Xin-Li
    Fan, Bing-Zheng
    Guan, Yang
    Li, Yi-Peng
    Jin, Lei
    Shui, Guo-Yan
    Jiang, Yi-Zhong
    Sun, Xun
    China Foundry, 21 (06): : 702 - 708