Microcracking and the Strength of Quartz-containing Clay Ceramics.

被引:0
|
作者
Storch, Werner [1 ]
Ruf, Heinz [1 ]
Scholze, Horst [1 ]
机构
[1] Fraunhofer-Inst fuer, Silicatforschung, Weurzburg, West, Ger, Fraunhofer-Inst fuer Silicatforschung, Weurzburg, West Ger
来源
CFI Ceramic Forum International | 1984年 / 61卷 / 07期
关键词
D O I
暂无
中图分类号
学科分类号
摘要
CERAMIC PRODUCTS
引用
收藏
页码:335 / 342
相关论文
共 50 条
  • [21] Mechanochemical Synthesis of Composite Magnetic Materials on the Basis of Quartz-Containing Systems
    Mofa, N. N.
    Mansurov, Z. A.
    EURASIAN CHEMICO-TECHNOLOGICAL JOURNAL, 2010, 12 (01) : 55 - 62
  • [22] Biaxial flexural strength of bovine dentin and castable ceramics.
    Takahashi, H
    Nishimura, F
    Inoue, T
    Iwasaki, N
    Kitazaki, H
    Nakano, F
    Tonami, F
    Yan, M
    JOURNAL OF DENTAL RESEARCH, 2001, 80 (04) : 1382 - 1382
  • [23] MODEL FOR EVALUATING STRENGTH AND FRACTURE TOUGHNESS OF STRUCTURAL CERAMICS.
    Nakakado, Kimiaki
    Takahashi, Ichiro
    Miyata, Hiroshi
    Zairyo/Journal of the Society of Materials Science, Japan, 1986, 35 (388) : 48 - 53
  • [24] Effect of surface treatments on the flexural strength of dental ceramics.
    Kim, CW
    Chung, SH
    Lim, BS
    JOURNAL OF DENTAL RESEARCH, 1996, 75 : 380 - 380
  • [25] Cyclic fatigue strength of CAD/CAM machinable ceramics.
    Nakazato, T
    Takahashi, H
    Nishimura, F
    Kurosaki, N
    JOURNAL OF DENTAL RESEARCH, 2000, 79 : 183 - 183
  • [26] ESTIMATING METHOD OF MATERIAL STRENGTH PROPERTIES AND RELIABILITY FOR CERAMICS.
    Okabe, Nagatoshi
    Ito, Hiroshige
    Hirata, Hideyuki
    Muramatsu, Masamitsu
    Zairyo/Journal of the Society of Materials Science, Japan, 1987, 36 (408) : 1012 - 1017
  • [27] Shearbond strength of cements to zirconia and lithium disilicate ceramics.
    Piwowarczyk, A
    Berge, HX
    Lauer, HC
    Sorensen, JA
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : A401 - A401
  • [28] Strength degradation from contact damage in dental ceramics.
    Peterson, IM
    Jung, YG
    Lawn, BR
    Pajares, A
    JOURNAL OF DENTAL RESEARCH, 1998, 77 : 681 - 681
  • [29] TRANSFORMATION TOUGHENING IN ZrO2-CONTAINING CERAMICS.
    Heuer, A.H.
    1600, (70):
  • [30] Adhesive bond strength between resin cements and high-strength ceramics.
    Edelhoff, D
    Marx, R
    Abuzayeba, M
    Yildifim, M
    Spiekermann, H
    Sorensen, JA
    JOURNAL OF DENTAL RESEARCH, 2000, 79 : 618 - 618