Investigation of Al2O3/Cr3C2 composites prepared by pressureless sintering (Part 2)

被引:0
|
作者
Natl Cheng-Kung Univ, Tainan, Taiwan [1 ]
机构
来源
Mater Chem Phys | / 3卷 / 211-215期
关键词
D O I
暂无
中图分类号
学科分类号
摘要
引用
收藏
相关论文
共 50 条
  • [11] PREPARATION OF AL2O3/NI COMPOSITES BY PRESSURELESS SINTERING IN H-2
    TUAN, WH
    LIN, MC
    WU, HH
    CERAMICS INTERNATIONAL, 1995, 21 (04) : 221 - 225
  • [12] The influence of oxidation on crack resistance in injection moulded Cr3C2/Al2O3 composites
    Jeng, CA
    Huang, JL
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2003, 23 (09) : 1477 - 1484
  • [13] Fabrication and Microstructure of the Fe3Al/Al2O3 Composites by Pressureless Sintering
    Jiang, Tao
    Pan, Kewei
    TESTING AND EVALUATION OF INORGANIC MATERIALS I, 2011, 177 : 411 - 414
  • [14] Wet erosion damage of Cr3C2/Al2O3 composite
    Jeng, CA
    Huang, JL
    JOURNAL OF MATERIALS RESEARCH, 2003, 18 (05) : 1162 - 1167
  • [15] ELECTRODISCHARGE-MACHINING OF AL2O3/CR3C2 COMPOSITE
    SHU, KM
    FU, CT
    LIU, DM
    JOURNAL OF MATERIALS SCIENCE LETTERS, 1994, 13 (15) : 1146 - 1148
  • [16] Ultrasonic evaluation of thermally shocked Cr3C2/Al2O3
    Wu, SJ
    Jeng, CA
    Huang, JL
    2002 IEEE ULTRASONICS SYMPOSIUM PROCEEDINGS, VOLS 1 AND 2, 2002, : 873 - 876
  • [17] Wet erosion damage of Cr3C2/Al2O3 composite
    Ching-An Jeng
    Jow-Lay Huang
    Journal of Materials Research, 2003, 18 : 1162 - 1167
  • [18] Influence of VC and Cr3C2 as grain growth inhibitors on WC-Al2O3 composites prepared by hot press sintering
    Dong, Weiwei
    Zhu, Shigen
    Wang, Ying
    Bai, Tao
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2014, 45 : 223 - 229
  • [19] Pressureless sintering of Al2O3/Ni nanocomposites
    Chen, RZ
    Tuan, WH
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1999, 19 (04) : 463 - 468
  • [20] Pressureless sintering of Al2O3/TiC nanocomposites
    Ueda, Hisao
    Tsuji, Hidekazu
    Takenouchi, Takeyoshi
    Nakahira, Atsushi
    Niihara, Kouichi
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 1994, 41 (10): : 1226 - 1231