KINETICS OF THE REDUCTION OF FeO IN CaO-SiO2 SLAG WITH SOLID CARBON.

被引:0
|
作者
Sasaki, Yasushi
Soma, Tanekazu
机构
关键词
D O I
10.2355/tetsutohagane1955.64.3_376
中图分类号
TF [冶金工业]; TG14 [金属材料];
学科分类号
0806 ;
摘要
The testing temperature ranged from 1400 degree C to 1600 degree C and basicity (CaO/SiO//2) from 0. 5 to 2. 0. The reduction rate is independent of the FeO concentration in the range of reduction of 30% to 80%. Reduction takes place in the form of indirect reduction in which CO as reductant is consumed and regenerated by solid carbon. The controlling step is gasification. CaO increases the reduction rate.
引用
收藏
页码:376 / 384
相关论文
共 50 条
  • [21] Rate of 2CaO•SiO2 Dissolution into Molten CaO-FeO-SiO2 Slag Saturated with Solid Iron
    Kobayashi, Yoshinao
    Sadamoto, Takahide
    ISIJ INTERNATIONAL, 2017, 57 (10) : 1703 - 1709
  • [22] REDUCTION OF SiO2 BY SOLID CARBON. (RATE OF THE FORMATION OF SiO AND SiC).
    Kawauchi, Kazuteru
    Maeda, Masafumi
    Kaneko, Masao
    Sasabe, Minoru
    Transactions of the Iron and Steel Institute of Japan, 1986, 27 (03)
  • [23] NITROGEN TRANSFER BETWEEN CaO-SiO2 BINARY SLAG AND CARBON SATURATED IRON.
    Kimura, Hiroshi
    Shimoo, Toshio
    Nakamura, Hideki
    Kawai, Masao
    Nippon Kinzoku Gakkaishi/Journal of the Japan Institute of Metals, 1976, 40 (05): : 451 - 457
  • [24] Kinetics of Electrically Enhanced Boron Removal From Silicon Using CaO-SiO2 and CaO-SiO2-Al2O3 Slag
    A. D. P. Putera
    M. S. Islam
    K. L. Avarmaa
    H. T. B. M. Petrus
    G. A. Brooks
    M. A. Rhamdhani
    Metallurgical and Materials Transactions B, 2023, 54 : 1228 - 1244
  • [25] Kinetics of Electrically Enhanced Boron Removal From Silicon Using CaO-SiO2 and CaO-SiO2-Al2O3 Slag
    Putera, A. D. P.
    Islam, M. S.
    Avarmaa, K. L.
    Petrus, H. T. B. M.
    Brooks, G. A.
    Rhamdhani, M. A.
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2023, 54 (03): : 1228 - 1244
  • [26] A study of the reduction rate of FeO in slag by solid carbon
    D. J. Min
    J. W. Han
    W. S. Chung
    Metallurgical and Materials Transactions B, 1999, 30 : 215 - 221
  • [27] Surface kinetics of nitrogen dissolution and its correlation to the slag structure in the CaO-SiO2, CaO-Al2O3, and CaO-SiO2-Al2O3 slag system
    Han, Seung-Min
    Park, Jin-Gyun
    Sohn, Il
    JOURNAL OF NON-CRYSTALLINE SOLIDS, 2011, 357 (15) : 2868 - 2875
  • [28] A study of the reduction rate of FeO in slag by solid carbon
    Min, DJ
    Han, JW
    Chung, WS
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 1999, 30 (02): : 215 - 221
  • [29] RATE OF FEO REDUCTION FROM A CAO-SIO2-AL2O3 SLAG BY CARBON-SATURATED IRON
    DELVE, FD
    PHILBROOK, WO
    KIRKBRIDE, LD
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1956, 206 (10): : 1403 - 1404
  • [30] RATE OF FEO REDUCTION FROM A CAO-SIO2-AL2O3 SLAG BY CARBON-SATURATED IRON
    PHILBROOK, WO
    KIRKBRIDE, LD
    TRANSACTIONS OF THE AMERICAN INSTITUTE OF MINING AND METALLURGICAL ENGINEERS, 1956, 206 (03): : 351 - 356