SOLIDIFICATION AND SEGREGATION OF LARGE KILLED STEEL INGOTS.

被引:0
|
作者
Hirahara, Hiroaki
Hashio, Moriki
Marukawa, Katsukiyo
Shiroishi, Hiroaki
机构
关键词
STEELMAKING - Rare Earth Additions;
D O I
10.2355/tetsutohagane1955.62.13_1641
中图分类号
学科分类号
摘要
The results of the investigation show that the solidification pattern in large flat steel ingots is proportional to the square root of time after teeming in the first stage solidification and proportional to the square of time with the formation impurity precipitates. Skimming of the liquid steel in the mold makes the inverse V segregation disappear in the top surface of the ingot, but it remains in the ingot bottom. Further, the inverse V segregation lines become thin and shift to the inner parts of the ingot. Formation of inverse V segregation is closely related to solidification velocity. The critical solidification velocity becomes small by skimming. By RE metal addition to the liquid steel in the ladle, the inverse V segreg lines in sulfur prints become the white segregation, and occurrence of large inclusions is insignificant.
引用
收藏
页码:1641 / 1652
相关论文
共 50 条
  • [41] CHEMICAL HETEROGENEITY OF LARGE SEMI-KILLED STEEL INGOTS
    KAZACHKOV, EA
    REVTOV, NI
    STEEL IN THE USSR, 1980, 10 (01): : 19 - 20
  • [42] COMPUTER CALCULATION OF PROCESS OF SOLIDIFICATION OF LARGE STEEL INGOTS
    KAZACHKO.EA
    MAKUROV, SL
    PARAFEIN.EP
    STEEL IN THE USSR, 1974, 4 (05): : 368 - 370
  • [43] INFLUENCE OF MOULD DESIGN ON THE SOLIDIFICATION AND SOUNDNESS OF HEAVY FORGING INGOTS.
    Tashiro, Koichi
    Watanabe, Shiro
    Kitagawa, Ikujiro
    Tamura, Itaru
    Tetsu-To-Hagane/Journal of the Iron and Steel Institute of Japan, 1981, 67 (01): : 103 - 112
  • [44] THERMAL ANALYSIS OF SOLIDIFICATION AND SHRINKAGE CAVITY FORMATION IN CYLINDRICAL INGOTS.
    Putilov, N.T.
    Romanov, A.A.
    Ryabov, V.V.
    Kochegarov, V.G.
    Krylova, M.V.
    Kats, S.S.
    Zagudailov, Yu.V.
    Oblasov, G.A.
    Russian metallurgy. Metally, 1987, (03) : 71 - 74
  • [45] PRODUCTION OF HIGH INTEGRITY LARGE FORGING INGOTS.
    Sigachev, A.A.
    Davidenko, N.I.
    Chalenko, R.P.
    Kulik, N.N.
    Gnedash, A.V.
    1600, (17):
  • [46] OXYGEN AND SULFUR SEGREGATION IN COMMERCIAL KILLED INGOTS
    WOJCIK, WM
    KOWAL, RF
    TRANSACTIONS OF THE METALLURGICAL SOCIETY OF AIME, 1965, 233 (10): : 1867 - &
  • [47] SOLIDIFICATION AND SEGREGATION IN HEAVY FORGING INGOTS
    MAIDORN, C
    BLIND, D
    NUCLEAR ENGINEERING AND DESIGN, 1985, 84 (02) : 285 - 296
  • [48] Control of Directional Solidification of Aluminum-Copper Alloy Ingots.
    Garcia, Amauri
    De Campos, Carlos Alfredo Baptista
    De Campos Filho, Mauricio Prates
    Metalurgia, ABM (Associacao Brasileira de Metais), 1977, 33 (235): : 323 - 326
  • [49] INFLUENCE OF NATURAL-CONVECTION ON SOLIDIFICATION IN BROAD-BASE KILLED STEEL INGOTS
    NEDOPEKIN, FV
    PETRENKO, SS
    POLYAKOV, VF
    MINEVICH, VY
    RUSSIAN METALLURGY, 1985, (05): : 61 - 66
  • [50] PROGRESS OF TEMPERATURE IN KILLED STEEL INGOTS DURING SOLIDIFICATION COOLING AND REHEATING IN PIT FURNACE
    MULLER, K
    HAMMERSC.P
    FUNKE, P
    STAHL UND EISEN, 1969, 89 (08): : 404 - &