The present work pertains to the study of electroless Ni-P and Ni-P-Si3N4 composite coatings. The deposits are obtained from a proprietary high phosphorus electroless nickel plating bath, comprising nickel sulphate, sodium hypophosphite, complexing agents and stabilizers. The maximum weight percent of Si3N4 incorporated in the electroless deposits is obtained at a concentration of 10 g/l in the bath. The electroless Ni-P deposits have 0%, 2.01%, 5.81% and 8.10% of Si3N4, respectively, obtained from baths containing 0, 2, 5 and 10 g/l of Si3N4, are characterized by optical microscopy, XRD and TEM. Hardness is found to increase with the incorporation of Si3N4 at all heat treatment temperatures studied. Also hardness increases with an increase in weight percent of Si3N4 incorporated in the deposit. The analyses of the composite coatings by XRD and TEM reveal that the inclusion of Si3N4 particles does not change the amorphous nature of the Ni-P matrix.
引用
收藏
页码:84 / 86
相关论文
共 50 条
  • [31] Electroless deposition of Ni-P composite coatings containing kaolin nanoparticles
    Srinivasan, K. N.
    Thangavelu, P. R.
    TRANSACTIONS OF THE INSTITUTE OF METAL FINISHING, 2012, 90 (02): : 105 - 112
  • [32] The Preparation, Characterization, and Influence of Multiple Electroless Nickel-Phosphorus (Ni-P) Composite Coatings on Poplar Veneer
    Pan, Yanfei
    Wang, Xin
    Huang, Jintian
    BIORESOURCES, 2016, 11 (01): : 724 - 735
  • [33] Wear resistance of electroless deposited Ni-P and Ni-P/SiC composite coatings on low alloy cast iron
    Wu, YC
    Li, GH
    Zhang, L
    SURFACE ENGINEERING, 2000, 16 (06) : 506 - 510
  • [34] A study on the wear resistance of electroless Ni-P/Diamond composite coatings
    Reddy, VVN
    Ramamoorthy, B
    Nair, PK
    WEAR, 2000, 239 (01) : 111 - 116
  • [35] Surface free energies of electroless Ni-P based composite coatings
    Zhao, Q
    Liu, Y
    Abel, EW
    APPLIED SURFACE SCIENCE, 2005, 240 (1-4) : 441 - 451
  • [36] Structure and phase transformation behaviour of electroless Ni-P composite coatings
    Balaraju, JN
    Narayanan, TSNS
    Seshadri, SK
    MATERIALS RESEARCH BULLETIN, 2006, 41 (04) : 847 - 860
  • [37] Fabrication and wear properties of electroless Ni-P/cenosphere composite coatings
    Shenzhen Key Laboratory of Special Functional Materials, Shenzhen University, Shenzhen 518060, China
    Shenzhen Daxue Xuebao (Ligong Ban), 2008, 2 (195-199):
  • [38] Preparation and properties of Ni-Co-P/nano-sized Si3N4 electroless composite coatings
    Hu, Jia
    Fang, Liang
    Zhong, Pei-Wen
    Tang, An-Qiong
    Yin, Bo
    Li, Yun
    SURFACE AND INTERFACE ANALYSIS, 2012, 44 (04) : 450 - 455
  • [39] Corrosion properties of the Ni-P/Si3N4 composite layers produced by electroless plating on the aluminum
    Trzaska, Maria
    Kucharska, Beata
    OCHRONA PRZED KOROZJA, 2009, 52 (11): : 558 - 560
  • [40] Effect of surfactants on the behavior of the Ni-P bath and on the formation of electroless Ni-P-TiC composite coatings
    Czagany, M.
    Baumli, P.
    SURFACE & COATINGS TECHNOLOGY, 2019, 361 : 42 - 49