Wettability and bonding strength between copper base alloys and sintered Al2O3 compacts

被引:0
|
作者
Yokota, Masaru
Fujii, Takahiro
Nagai, Hiroshi
Shoji, Keiichiro
机构
关键词
Copper and Alloys--Wetting - Copper Tin Alloys--Wetting - Copper Tin Titanium Alloys--Wetting - Copper Titanium Alloys--Wetting - Tin Titanium Alloys--Wetting;
D O I
暂无
中图分类号
学科分类号
摘要
Studies on the wettability and bonding of Cu-Sn-Ti (pure metals except for Ti, binary alloys and a ternary alloy) against sintered Al2O3 compacts were carried out. Wettability of Cu, Sn pure metals, Cu-10%Sn and Cu-5%Ti binary alloys in vacuum (1.3×10-2, 4.0×10-3 Pa) were unsatisfactory. Cu-10%Sn-5%Ti was comparatively wettable, where a reaction layer corresponding to Ti3Al containing slight Cu and Sn was formed in the interface between the brazing alloy and sintered Al2O3 compact. Sn-5%Ti binary alloy against sintered Al2O3 showed fair wettability, but did not form any reaction layer. Bonding strength of sintered Al2O3 compacts brazed with Cu, Sn pure metals and Cu-10%Sn or Cu-5%Ti had a tendency to decrease with increasing the degree of vacuum (or with decreasing oxygen partial pressure) of the bonding atmosphere. Bonding strength of sintered Al2O3 compacts brazed with Sn-5%Ti and Cu-10%Sn-5%Ti alloys were comparatively high and had a tendency to increase with a higher bonding temperature.
引用
收藏
页码:543 / 547
相关论文
共 50 条
  • [22] Mathematical Simulation of the Wettability of Al2O3 Substrate through Different Aluminum Alloys
    Rocha-Rangel, Enrique
    Rodriguez-Garcia, Jose A.
    Castillo-Robles, Jose A.
    Armendariz Mireles, Eddie N.
    Calles-Arriaga, Carlos A.
    JOURNAL OF COMPOSITES SCIENCE, 2021, 5 (06):
  • [23] THE BONDING STRENGTH FOR FE/(FE-FEO)/AL2O3 SYSTEMS
    SAKATA, K
    OHKOSHI, T
    NII, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1986, 50 (07) : 654 - 658
  • [24] Microstructural changes in sintered Al2O3 by acid treatment of compacts produced by slip casting in gypsum molds
    Hotta, Y
    CERAMICS INTERNATIONAL, 2002, 28 (06) : 593 - 599
  • [25] A new method for preparation of direct bonding copper substrate on Al2O3
    He, Hong
    Fu, Renli
    Wang, Deliu
    Song, Xiufeng
    Jing, Min
    MATERIALS LETTERS, 2007, 61 (19-20) : 4131 - 4133
  • [26] Bond strength and microstructure investigation on Al2O3/Al/Al2O3 joints
    Ksiazek, M
    Sobczak, N
    Mikulowski, B
    Radziwilli, W
    Winiarski, B
    SURFACE AND INTERFACE ANALYSIS, 2004, 36 (08) : 673 - 676
  • [27] Improvement of wettability of Al2O3 by molten aluminum
    Cailiao Gongcheng/Journal of Materials Engineering, 2000, (04): : 11 - 13
  • [28] PROTECTIVE AL2O3 SCALE FORMATION ON NBAL3-BASE ALLOYS
    DOYCHAK, J
    HEBSUR, MG
    OXIDATION OF METALS, 1991, 36 (1-2): : 113 - 141
  • [29] ACOUSTIC-EMISSION AND MICROCRACKING IN SAPPHIRE, SINTERED AL2O3, AL/AL2O3 COMPOSITE, AND ALUMINUM
    BREVAL, E
    SRIKANTH, V
    SUBBARAO, EC
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1995, 78 (09) : 2541 - 2544
  • [30] Microstructure evolution and bonding strength of the Al2O3/Al2O3 interface brazed via Ni-Ti intermetallic phases
    Lu, Yao
    Zhu, Meixiong
    Zhang, Qi
    Hu, Tao
    Wang, Juan
    Zheng, Kaihong
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2020, 40 (04) : 1496 - 1504