Strong monolithic and composite MoSi2 materials by nanostructure design

被引:0
|
作者
Niihara, Koichi [1 ]
Suzuki, Yoshikazu [1 ]
机构
[1] The Inst. of Sci. and Indust. Res., Osaka Univ., 8-1 Mihogaoka, Ibaraki, Osaka 567-0047, Japan
来源
Materials Science and Engineering A | 1999年 / 261卷 / 1-2期
基金
日本学术振兴会;
关键词
D O I
暂无
中图分类号
学科分类号
摘要
The nanocomposite concept is briefly reviewed at first, and the approach to fabricating strong and tough MoSi2-based materials through the nanocomposite technology is demonstrated. Strong MoSi2-based nanocomposites such as MoSi2/SiC and MoSi2/Mo(Si,Al)2/SiC were developed by conventional powder metallurgical techniques. Effects of grain boundary and interface structure on mechanical properties were investigated for these composites. In the MoSi2/SiC nanocomposites, both MoSi2 matrix and siliceous grain boundary phases were simultaneously controlled, nano-sized SiC particles (50-200 nm) were dispersed into both MoSi2 matrix grains and glassy SiO2 located at triple junctions. High-resolution TEM observation revealed that the intragranular SiC particles directly bonded to MoSi2 without any impurity phases, resulting in toughening by the thermal expansion mismatch between MoSi2 and SiC. The intergranular SiC particles played important roles to inhibit the grain growth of MoSi2 matrix, and they concurrently toughened the glassy SiO2. For Al-alloyed systems, α-Al2O3 was dispersed in the compacts instead of glassy SiO2. The matrices became di-phasic, that is, mixture of tetragonal MoSi2 and hexagonal Mo(Si,Al)2. SiC dispersion in the Mo-Si-Al alloys effectively improved their mechanical properties. By means of such material designs, all composites showed very high strength (more than 1 GPa by the three-point bending test). In particular, MoSi2/Mo(Si,Al)2/SiC composites possessed the improved high-temperature strength of about 1 GPa at 1100°C. © 1999 Elsevier Science S.A.
引用
收藏
页码:6 / 15
相关论文
共 50 条
  • [41] ABRASIVE WEAR BEHAVIOR OF MOSI2/SIC AND MOSI2/ZRO2 COMPOSITES
    ALMAN, DE
    HAWK, JA
    PETROVIC, JJ
    SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (11): : 1765 - 1770
  • [42] Improvement of MoSi2 oxidation resistance via boron addition: Fabrication of MoB/MoSi2 composite by mechanical alloying and subsequent reactive sintering
    Taleghani, P. R.
    Bakhshi, S. R.
    Erfanmanesh, M.
    Borhani, G. H.
    Vafaei, R.
    POWDER TECHNOLOGY, 2014, 254 : 241 - 247
  • [43] Indentation testing of MOSi2
    Henzel, M
    Zimovcák, P
    Dusza, J
    Juhász, A
    Lendvai, J
    FRACTOGRAPHY OF ADVANCED CERAMICS II, 2005, 290 : 288 - 291
  • [44] On the oxidation behaviour of MoSi2
    Liu, YQ
    Shao, G
    Tsakiropoulos, P
    INTERMETALLICS, 2001, 9 (02) : 125 - 136
  • [45] FRACTURE MODES IN MOSI2
    WADE, RK
    PETROVIC, JJ
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1992, 75 (06) : 1682 - 1684
  • [46] ON THE SLIP SYSTEMS IN MOSI2
    MALOY, SA
    HEUER, AH
    LEWANDOWSKI, JJ
    MITCHELL, TE
    ACTA METALLURGICA ET MATERIALIA, 1992, 40 (11): : 3159 - 3165
  • [47] Preparation and microstructure of WSi2/MoSi2 composite heat element
    Ai, YL
    Cheng, YG
    Yang, YQ
    Kang, MK
    Liu, CH
    RARE METAL MATERIALS AND ENGINEERING, 2005, 34 (06) : 962 - 965
  • [48] Dense SiCf/MoSi2 composite via liquid silicon infiltration
    Huang, Minzhong
    Wang, Qi
    Li, Siwei
    Chen, Lifu
    Xiao, Hongrui
    Su, Xiaohui
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2019, 102 (10) : 5716 - 5724
  • [49] Fabrication and characterization of SiCw/MoSi2 composite from COSHSed powder
    Jianguang Xu
    Baolin Zhang
    Guojian Jiang
    Wenlan Li
    Hanrui Zhuang
    Journal of Materials Science, 2007, 42 : 5795 - 5798
  • [50] Fabrication and characterization SiCw/MOSi2 composite from COSHSed powder
    Xu, Jianguang
    Zhang, Baolin
    Jiang, Guojian
    Li, Wenlan
    Zhuang, Hanrui
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (14) : 5795 - 5798