Growth of Ti3SiC2 thin films by elemental target magnetron sputtering

被引:0
|
作者
Emmerlich, Jens [1 ]
Högberg, Hans [1 ]
Sasvári, Szilvia [1 ]
Persson, Per O. Å. [1 ]
Hultman, Lars [1 ]
Palmquist, Jens-Petter [2 ]
Jansson, Ulf [2 ]
Molina-Aldareguia, Jon M. [3 ]
Czigány, Zsolt [4 ]
机构
[1] Department of Physics, Linköping University, Thin Film Physics Division, SE-581 83 Linköping, Sweden
[2] Department of Material Chemistry, Uppsala University, Ångstrom Laboratory, P. O. Box 538, SE-751 21 Uppsala, Sweden
[3] CEIT, P. Manuel Lardizabal 15, 20018 San Sebastian, Spain
[4] Res. Inst. Tech. Phys. and Mat. Sci., P.O. Box 49, H-1525 Budapest, Hungary
来源
| 1600年 / American Institute of Physics Inc.卷 / 96期
关键词
Chemical vapor deposition - Composition - Magnetron sputtering - Phase diagrams - Reaction kinetics - Substrates - Thermal effects - X ray diffraction analysis;
D O I
暂无
中图分类号
学科分类号
摘要
Epitaxial Ti3SiC2(0001) thin films have been deposited by dc magnetron sputtering from three elemental targets of Ti, C, and Si onto MgO(111) and Al2O3(0001) substrates at temperatures of 800-900°C. This process allows composition control to synthesize Mn+1AXn (MAX) phases (M: early transition metal; A: A-group element; X: C and/or N; n = 1-3) including Ti 4SiC3. Depositions on MgO(100) substrates yielding the Ti-Si-C MAX phases with (1015), as the preferred orientation. Samples grown at different substrate temperatures, studied by means of transmission electron microscopy and x-ray diffraction investigations, revealed the constraints of Ti3SiC2 nucleation due to kinetic limitations at substrate temperatures below 700°C. Instead, there is a competitive TiCx growth with Si segregation to form twin boundaries or Si substitutional incorporation in TiCx. Physical properties of the as-deposited single-crystal Ti3SiC2 films were determined. A low resistivity of 25 μ cm was measured. The Young's modulus, ascertained by nanoindentation, yielded a value of 343-370 GPa. For the mechanical deformation response of the material, probing with cube corner and BerkoVich indenters showed an initial high hardness of almost 30 GPa. With increased maximum indentation loads, the hardness was observed to decrease toward bulk values as the characteristic kink formation sets in with dislocation ordering and delamination at basal planes. © 2004 American Institute of Physics.
引用
收藏
相关论文
共 50 条
  • [21] Evaluation of properties of spark plasma sintered Ti3SiC2 and Ti3SiC2/SiC composites
    Islak, Bilge Yaman
    Ayas, Erhan
    CERAMICS INTERNATIONAL, 2019, 45 (09) : 12297 - 12306
  • [22] Monte Carlo Simulations of Elastic Scattering with Applications to DC and High Power Pulsed Magnetron Sputtering for Ti3SiC2
    Geiser, Juergen
    Blankenburg, Sven
    COMMUNICATIONS IN COMPUTATIONAL PHYSICS, 2012, 11 (05) : 1618 - 1642
  • [23] Joining of Ti3SiC2 by Magnetron Sputtering a Layer of Cu or Zr Followed by Heat Treating at Relatively Low Temperatures
    Li, Aijun
    Zhou, Yanchun
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2011, 94 (09) : 3072 - 3077
  • [24] Growth and Microstructure of Epitaxial Ti3SiC2 Contact Layers on SiC
    Tsukimoto, Susumu
    Ito, Kazuhiro
    Wang, Zhongchang
    Saito, Mitsuhiro
    Ikuhara, Yuichi
    Murakami, Masanori
    MATERIALS TRANSACTIONS, 2009, 50 (05) : 1071 - 1075
  • [25] Photoemission studies of Ti3SiC2 and nanocrystalline-TiC/amorphous-SiC nanocomposite thin films
    Eklund, P.
    Virojanadara, C.
    Emmerlich, J.
    Johansson, L. I.
    Hogberg, H.
    Hultman, L.
    PHYSICAL REVIEW B, 2006, 74 (04)
  • [26] Polymorphism of Ti3SiC2
    R. Yu
    Q. Zhan
    L. L. He
    Y. C. Zhou
    H. Q. Ye
    Journal of Materials Research, 2002, 17 : 948 - 950
  • [27] Preparation of Ti3SiC2
    P. V. Istomin
    A. V. Nadutkin
    Yu. I. Ryabkov
    B. A. Goldin
    Inorganic Materials, 2006, 42 : 250 - 255
  • [28] Polymorphism of Ti3SiC2
    Yu, R
    Zhan, Q
    He, LL
    Zhou, YC
    Ye, HQ
    JOURNAL OF MATERIALS RESEARCH, 2002, 17 (05) : 948 - 950
  • [29] Structure of Ti3SiC2
    Rawn, CJ
    Payzant, EA
    Hubbard, CR
    Barsoum, MW
    El-Raghy, T
    EUROPEAN POWDER DIFFRACTION, PTS 1 AND 2, 2000, 321-3 : 889 - 892
  • [30] Ti3SiC2 and ice
    Barsoum, MW
    Radovic, M
    Finkel, P
    El-Raghy, T
    APPLIED PHYSICS LETTERS, 2001, 79 (04) : 479 - 481