共 50 条
- [31] Special misorientations and textural heredity in the commercial alloy Fe-3% Si The Physics of Metals and Metallography, 2014, 115 : 775 - 785
- [32] Influence of shear bands on recrystallization texture in Fe-3%Si alloy RECRYSTALLIZATION AND GRAIN GROWTH, VOLS 1 AND 2, 2001, : 1197 - 1202
- [33] THE MECHANISM OF HYDROGEN INDUCED CLEAVAGE IN FE-3 PCT SI ALLOY METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (05): : 1335 - 1343
- [36] Special misorientations and textural heredity in the commercial alloy Fe-3% Si PHYSICS OF METALS AND METALLOGRAPHY, 2014, 115 (08): : 775 - 785
- [37] STRUCTURAL CHANGES DURING ROLLING OF FE-3 PERCENT SI ALLOY RUSSIAN METALLURGY-METALLY-USSR, 1969, (04): : 63 - &
- [38] Study of Ferrite Grain Growth in Fe plus 3% Si Alloy. Izvestiya Vysshikh Uchebnykh Zavedenij. Chernaya Metallurgiya, 1980, (08): : 79 - 83
- [39] Inhibitor precipitation of Fe-3%Si strip by thin slab casting and rolling Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2010, 31 (10): : 21 - 25